1-20 of 41 Search Results for

heater elements

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1975) 24 (8): Ni-220.
Published: 01 August 1975
... TECHALLOY A (80-20) is a nickel-chromium electrical resistance alloy for operating temperatures up to 2150 F. It is non-magnetic, highly corrosion resistance, and has a lower temperature coefficient of resistance than other alloys for heater elements. This datasheet provides information...
Journal Articles
Alloy Digest (2003) 52 (11): SS-893.
Published: 01 November 2003
... Aluchrom Y is an oxidation-resistant ferritic stainless steel alloyed with aluminum. Applications include heating elements in high-temperature furnaces, radiant heaters, quartz heaters, and toasters. This datasheet provides information on composition, physical properties, elasticity, and tensile...
Journal Articles
Alloy Digest (2005) 54 (2): SS-917.
Published: 01 February 2005
... Incoloy Alloy 832 is designed for sheathed heater applications. It is reasonably priced and contains sufficient alloying elements to develop a good surface oxide. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1971) 20 (2): Ni-162.
Published: 01 February 1971
... TOPHET H is a heating-element alloy specifically designed for use in duct heaters and clothes dryers where hot strength and long life are of most importance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (2021) 70 (8): Cu-923.
Published: 01 August 2021
... for equalization of the tem- Consumer Downspouts, flashing, gutters, roofing. perature. Do not finish below 750 °C (1380 °F). Electrical Industrial Condenser sheets, heater units. Heat Treatment Marine Air conditioners, refrigerators. Annealing temperature Stress relieving temperature Heater elements, wire...
Journal Articles
Alloy Digest (1993) 42 (10): Cu-589.
Published: 01 October 1993
... (6.4 mm) deposit 32 (221 Mpa) 14 (97 MPa) 30 60 Applications: Electrical connectors, heater elements, electrode holders, bus bars, crucibles, high-conductivity parts, welding AMPCO 97. Producer: AMPCO Metal, Inc. Milwaukee, WI 53201 4 14-645-3750 DOI: 10.31399/asm.ad.cu0589 Copyright © ASM...
Journal Articles
Alloy Digest (1988) 37 (11): Fe-87.
Published: 01 November 1988
... such as toasters with weIl supported heater elements, applications where available space is a factor and its high resistivity is advantageous. UsualIy used in medium-to-heavy wire sizes. ...
Journal Articles
Alloy Digest (1993) 42 (9): Cu-587.
Published: 01 September 1993
...). Applications: Billet molds, conductor rolls, heater elements, copper sculp- tures, steel mill: electrode holders, bus bars, copper connec- tors. Producer: AMPCO Metal, Inc. Milwaukee, WI 53201 414-645-3750 Table 1 - TYPICAL MECHANICAL PROPERTIES (Nominal all-weld metal Values) Tensile strength, ksi 29 (200 MPa...
Journal Articles
Alloy Digest (1980) 29 (8): Cu-400.
Published: 01 August 1980
..., hydraulic and gas lines, air conditioners, chemical and industrial heat exchangers, refrigerators, radiant-heating lines, sugar house refinery lines and heaters and calandria pans, brewery tubs and kettles, brewery lines, pulp and paper lines and tanks, instrument piping, heater elements. wire connectors...
Journal Articles
Alloy Digest (2009) 58 (8): SS-1039.
Published: 01 August 2009
... applications for Nikrothal 30 are solid hot plates, open coil heaters in HVAC systems, night-storage heaters, convection heaters, heavy-duty rheostats, and fan heaters. Nikrothal 30 is also used in heating cables and rope heaters in defrosting and deicing elements, electric blankets and pads, car seats...
Journal Articles
Alloy Digest (2009) 58 (7): SS-1038.
Published: 01 July 2009
... of such impurities from the heaters is reduced. Another consequence is even better oxidation properties compared with Kanthal APM. Heating elements of the alloy have shown longer oxidation life, lower resistance changes, and better form stability than any FeCrAl wire tested. DATA ON WORLDWIDE METALS AND ALLOYS...
Journal Articles
Alloy Digest (1976) 25 (4): Fe-57.
Published: 01 April 1976
...) imperceptible change throughout service life, and lowest cost per hot ohm for heating elements. Also, it is good for industrial heating furnace elements operating in protective atmospheres up to 1750-1800oF. Forms Available: Wire, rod, flat wire and strip. Applications: Heating elements for heaters. appliances...
Journal Articles
Alloy Digest (1992) 41 (8): Ni-408.
Published: 01 August 1992
... CRONIX 80 EXTRA and CRONIX 70 EXTRA are non-magnetic austenitic alloys for resistance heating elements. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. Filing Code: Ni-408. Producer or source: VDM Technologies Corporation. Producer...
Journal Articles
Alloy Digest (2010) 59 (5): Ta-13.
Published: 01 May 2010
... Composition: Element ppm (max) Carbon 50 Oxygen 100 Nitrogen 50 Hydrogen 10 Niobium 0.1 % (1000) Titanium 40 Nickel 50 Molybdenum 200 Silicon 25 Tungsten 2.0 3.5 wt. % Iron bal PGM(b) 1000 2000 Mass fraction in % [cg/g]; ppm [ g/g]) (a) and (c). (a) Contact producer for testing methods. (b) Platinum group...
Journal Articles
Alloy Digest (1976) 25 (8): Ni-232.
Published: 01 August 1976
.... It has good resistance to high-temperature cor- rosion and oxidation. It is paramagnetic. Forms Available: Wire, rod, strip. flat wire and castings. Applications: Heat-resistant elements for heating devices such as toasters. percolators, waffle irons. heater pads, flat irons, ironing machines, hair...
Journal Articles
Alloy Digest (1992) 41 (9): SS-534.
Published: 01 September 1992
... resistivity and operating temperature and the longest ser- vice life with excellent oxide formation. Aluchrom 1 has excellent oxidation and dielectric strength. It is used ad- ditionally with vertical quartz tube heaters. Aluchrom S has high resistivity and low specific gravity. It is also used in flat irons...
Journal Articles
Alloy Digest (1980) 29 (7): Bi-18.
Published: 01 July 1980
... Elements: Indalloy No. 255 is used as fusible elements in auto- matic safety devices such as safety plugs on pressure cookers, water tank heaters and electric radiators, and safety relief valves for large diesel engines. General Characteristics: Indalloy No. 255 is a 55.5% bismuth44.5% lead alloy...
Journal Articles
Alloy Digest (2002) 51 (5): Al-377.
Published: 01 May 2002
... Alcotec Weld Wire 5554 is a non-heat-treatable filler wire with moderate high-strength capabilities. The principal alloying elements are magnesium, manganese, chromium, and titanium. This datasheet provides information on composition, physical properties, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1986) 35 (5): Bi-39.
Published: 01 May 1986
... Elements: Bismuth-45Pb alloy is used as fusible elements in automatic safety devices such as safety plugs on pressure cookers. water tank heaters and electric radiators. and safety relief \,alves for large diesel engines. Foundry Aids: Bismuth-45Pb allo!, is used for proof casting cavities. molds. dies...
Journal Articles
Alloy Digest (1981) 30 (7): Bi-25.
Published: 01 July 1981
... as it freezes. It can be recovered easily and recycled into new uses any number of times. Among its many uses are (1) Anchoring metal parts in glass, (2) Filler for large diameter tubes for bending, (3) Proof casting forging dies, (4) Fusable elements is safely plugs and (5) Mechanical dentistry. This datasheet...