Alloy Digest (1985) 34 (5): Ni-314.
Published: 01 May 1985
... room and elevated temperatures. Its applications include heat treating furnace equipment, chemical equipment in various industries, and power plant equipment. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (1997) 46 (2): Ni-521.
Published: 01 February 1997
... room temperatures. Its application includes heat-treating furnace equipment, chemical equipment in various industries, and power plant equipment. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes information on...
Journal Articles
Alloy Digest (1967) 16 (2): CS-26.
Published: 01 February 1967
... USS CHAR-PAC is a heat treated carbon steel having exceptionally good notch toughness as well as high strength. It is recommended for pressure vessels, low temperature storage containers, earth moving equipment, offshore drilling rigs, etc. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2002) 51 (5): SS-853.
Published: 01 May 2002
... improves weldability. Typical uses include furnace parts, heating elements, aircraft and jet engine parts, heat exchangers, carburizing-annealing boxes, sulfite liquor handling equipment, kiln liners, boiler baffles, refinery and chemical processing equipment, and auto exhaust parts. This datasheet...
Journal Articles
Alloy Digest (1965) 14 (9): SS-172.
Published: 01 September 1965
... SANDVIK SANICRO 31 is an iron-nickel-chromium alloy having good resistance to corrosion and oxidation and good mechanical properties at elevated temperatures. It is recommended for electrical sheathing, pyrometer tubes, equipment for heat treating and furnace tubes and other equipment in the...
Journal Articles
Alloy Digest (1992) 41 (6): SS-530.
Published: 01 June 1992
... SANDVIK SANICRO 31HT is an austenitic iron-nickel-chromium alloy characterized by very good resistance to oxidation with good mechanical properties at elevated temperatures. It is recommended for resistance element sheathing, pyrometer tubes, airheaters, equipment for heat treating, furnace tubes...
Journal Articles
Alloy Digest (1984) 33 (8): SS-450.
Published: 01 August 1984
... 310S, a few typical uses include annealing boxes, chemical plant equipment, fire box sheets, furnace linings, heat exchangers, oil-refining equipment, kiln linings and tube hangers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as...
Journal Articles
Alloy Digest (1998) 47 (6): SS-719.
Published: 01 June 1998
... Allegheny Ludlum Type 310 is an austenitic chromium-nickel steel with high heat resisting properties. It is recommended for furnace equipment, heat treating boxes, burners, heat recovery systems, jet engine components, and heat exchangers. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1967) 16 (7): SS-197.
Published: 01 July 1967
... AISI TYPE 310 is an austenitic chromium-nickel steel with high heat resisting properties. It is recommended for furnace equipment, heat treating boxes, jet engine components and heat exchangers. This datasheet provides information on composition, physical properties, hardness, elasticity, and...
Journal Articles
Alloy Digest (1977) 26 (11): SS-228.
Published: 01 November 1977
... SUPERTHERM is a cast nickel-chromium-iron alloy stabilized with cobalt and tungsten. It is used worldwide in extremely high-temperature applications and has unexcelled performance to 2300 F (1260 C). Among its many uses are components for heat-treating furnaces, cement kilns, petrochemical furnace...
Journal Articles
Alloy Digest (1969) 18 (8): SS-229.
Published: 01 August 1969
... Firth Vickers F.I. 20 is a non-hardenable, ferritic high-chromium steel recommended for furnace parts, heat treating equipment, zinc die casting machine nozzles and other high temperature applications up to approximately 750 C. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1984) 33 (3): SS-441.
Published: 01 March 1984
... structures can be fabricated easily and it can be machined readily. It can be welded easily and gives strong, ductile welds. Some of its many applications are annealing boxes, boiler baffles, dryers, furnace parts, heat exchangers and oil-refining equipment. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1997) 46 (5): SS-682.
Published: 01 May 1997
... replacement applications for furnace tubing. This datasheet provides information on composition and physical properties as well as creep. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-682. Producer or source: Ultra-Cast Inc...
Journal Articles
Alloy Digest (1977) 26 (10): SS-345.
Published: 01 October 1977
... ALLOY 875 is an iron-chromium-aluminum electrical-resistance alloy with excellent resistance to oxidation at elevated temperatures. It was developed primarily for use as the heating element in industrial furnaces, kilns and other equipment where continuous operating temperatures up to 2350 F may...
Journal Articles
Alloy Digest (1979) 28 (9): SA-364.
Published: 01 September 1979
... CABOT ESR 4330 Mod is a modified 4330 alloy steel produced by electric-furnace, melting, vacuum degassing and electroslag remelting (ESR) by use of small-heat-size technology. Electroslag refining improves cleanliness and lowers the sulfur content to provide improved isotropy, ductility and...
Journal Articles
Alloy Digest (1980) 29 (4): SA-371.
Published: 01 April 1980
... CABOT ESR 4140 is a chromium-molybdenum alloy steel produced by electric-furnace melting, vacuum degassing and electroslag remelting by use of small-heat-size technology. Electroslag refining improves cleanliness and lowers the sulfur content to provide improved isotropy, ductility and toughness...
Journal Articles
Alloy Digest (1983) 32 (4): SA-388.
Published: 01 April 1983
... INGERSOLL-RAND OILFIELD PRODUCTS ESR 4330 MOD is a modified 4330 alloy steel produced by electric-furnace melting, vacuum degassing and electroslag remelting with the use of small-heat-size technology. Electroslag refining improves cleanliness and lowers the sulfur content to provide improved...
Journal Articles
Alloy Digest (1983) 32 (6): SA-391.
Published: 01 June 1983
... fatigue. It also includes information on low temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SA-391. Producer or source: Ingersoll-Rand Oilfield Products Company. Producer or Source: Ingersoll-Rand Oilfield...
Journal Articles
Alloy Digest (1965) 14 (7): SS-171.
Published: 01 July 1965
... well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-171. Producer or source: Stainless steel foundries. Producer or Source: Stainless steel foundries Copyright Ā© ASM InternationalĀ® 1996 1996...
Journal Articles
Alloy Digest (1967) 16 (1): Ni-120.
Published: 01 January 1967
... InternationalĀ® 1996 1996 ASM International chemical composition corrosion-resistant alloys creep properties elasticity furnace construction furnace equipment hardness heat treatability joinability machinability oxidation resistance physical properties RA-600 tensile properties workability...