Alloy Digest (1984) 33 (3): SS-442.
Published: 01 March 1984
... of phosphoric acid; down-hole tubulars in deep, sour gas wells; piping and heat-exchanger tubes in sulfuric acid service and seawater cooled heat exchangers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1959) 8 (9): Cu-81.
Published: 01 September 1959
... Revere No. 508 is a highly ductile, malleable and corrosion resistant copper-nickel alloy suitable for condenser and heat exchanger tubes and many engineering applications such as salt water piping aboard ship, many components of salt water and fresh water stills, feed water heater tubes...
Journal Articles
Alloy Digest (1982) 31 (12): Cu-449.
Published: 01 December 1982
.... Its strength and other mechanical properties are similar to the older copper-nickel alloys (90-10 and 70-30). Alloy C72200 is used primarily for condenser and heat-exchanger tubing using seawater and for salt-water piping. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1983) 32 (6): Cu-459.
Published: 01 June 1983
..., where velocities are higher than normal, and where impingement is more severe than normal. Typical uses are condenser and heat-exchanger tubes, distiller tubes and ferrules. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1985) 34 (6): Cu-497.
Published: 01 June 1985
... to corrosion. It is used widely for condenser, evaporator and heat-exchanger tubes and associated applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat...
Journal Articles
Alloy Digest (1970) 19 (3): Cu-213.
Published: 01 March 1970
... AMBRALOY-687 is an aluminum brass alloy containing arsenic as an inhibitor to dezincification. It is recommended for condenser and heat exchanger tubes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1961) 10 (12): Cu-111.
Published: 01 December 1961
... Bridgeport Alloy 77 is a modified copper-zinc brass having improved resistance to bio-fouling, dezincification, and other forms of copper attack. It is recommended for condenser and heat exchanger tubes for marine use. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1965) 14 (12): Ni-108.
Published: 01 December 1965
... Sanicro 71 is a nickel-base alloy having good resistance to stress-corrosion, oxidation and creep at elevated temperatures. It is recommended for nuclear power reactor heat exchanger tubes, aircraft turbojet engines and for equipment in the textile, plastic, and chemical industries. This datasheet...
Journal Articles
Alloy Digest (1981) 30 (10): Cu-424.
Published: 01 October 1981
... with higher zinc contents. Typical uses are plumbing pipe and condenser and heat-exchanger tubes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating...
Journal Articles
Alloy Digest (1981) 30 (9): Cu-422.
Published: 01 September 1981
... alkaline. It also prossesses good resistance to corrosion by waters containing sulfides. It has moderate strength and good ductility. For a long time, this alloy has been considered a standard for condenser and heat-exchanger tubes. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1994) 43 (11): Cu-599.
Published: 01 November 1994
... addition of inhibitor is made to minimize the alloy’s susceptibility to dezincification and stress corrosion. They are used for condenser, evaporator and heat-exchanger tubes and associated applications. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1983) 32 (12): SS-437.
Published: 01 December 1983
... and weldability are good. The uses of ES-2205 include heat exchangers, tubes and other components and equipment that must resist chloride-containing media, inorganic acids and organic acids. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1981) 30 (6): Cu-418.
Published: 01 June 1981
... its many uses are architectural applications, trim, hot forgings, condenser plates and heat exchanger tubes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (1987) 36 (7): Cu-526.
Published: 01 July 1987
... to minimize the alloy's susceptibility to dezincification and stress corrosion. It is used widely for condenser, evaporator and heat-exchanger tubes and associated applications. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1969) 18 (6): Cu-200.
Published: 01 June 1969
... Cupro Nickel, 30%-716 is a high strength copper-nickel-iron alloy for heat exchanger tubes in power plant feed water heaters, and also for oil refinery service. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1963) 12 (9): Cu-133.
Published: 01 September 1963
... Cupro Nickel, 30%-707 is a high strength copper-nickel-iron alloy for heat exchanger tubes in power plant feedwater heaters. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (1974) 23 (7): SS-298.
Published: 01 July 1974
... CARPENTER STAINLESS No. 7-Mo is a two-phase alloy consisting of a ferritic matrix with pools of austenite. It has high resistance to stress-corrosion cracking and pitting, and good general corrosion resistance in many environments. Its principal use is for tubing and pipe in heat exchangers...
Journal Articles
Alloy Digest (2005) 54 (8): SA-550.
Published: 01 August 2005
...) is effective for a reduction in sulfuric acid dew-point corrosion and developed S-TEN1 as a 0.3% Cu-0.1% Sb alloy of steel plates and tubes. S-TEN1 tubes have been widely used as air preheater tubes and heat-exchanger tubes. Recently, the need for sulfuric acid dew-point corrosion-resistant steels has spread...
Journal Articles
Alloy Digest (1971) 20 (5): Cu-232.
Published: 01 May 1971
... and bent readily. Tubes in the annealed and half-hard condition can be rolled into tube sheets without difficulty. problems. As condenser and heat exchanger tubes, it is used for maximum resistance to sea water of high and low velocity. It is the preferred condenser and salt-water tube material for vessels...
Journal Articles
Alloy Digest (2007) 56 (10): SS-999.
Published: 01 October 2007
... 250 °C (482 °F) for prolonged periods, the microstructure changes, which results in a reduction in impact strength. This does not necessarily affect the behavior of the material at the operating temperature. For example, heat-exchanger tubes can be used at higher temperatures without any problems...