Journal Articles
Alloy Digest (1983) 32 (9): SA-394.
Published: 01 September 1983
... LESCALLOY UT-19 VAC-ARC is a premium quality carburizing steel with high hardenability. It is produced by vacuum are remelting (VAR) to provide a preferred ingot solidification and superior microcleanliness. It is used for aircraft gears, pinions and other carburized parts that require a high...
Journal Articles
Alloy Digest (1971) 20 (9): SA-268.
Published: 01 September 1971
... The 5 Ni-025 Mo Steel is a carburizing steel designed for heavy-duty service. It possesses materially higher hardenability in both case and core than any other commercially available carburizing steel free from the processing difficulties associated with the formation of massive chromium carbides...
Journal Articles
Alloy Digest (1988) 37 (6): SS-496.
Published: 01 June 1988
... or source: Allegheny Ludlum Corporation. Producer or Source: Allegheny Ludlum Corporation Copyright © ASM International® 1996 1996 ASM International AL 15-7 PRECIPITATION HARDENING ALLOY chemical composition corrosion-resistant alloys elasticity hardness heat treatability high-temperature...
Journal Articles
Alloy Digest (1988) 37 (8): SS-497.
Published: 01 August 1988
... Allegheny Ludlum AL 17-4 Precipitation Hardening Alloy is a chromium-nickel-copper stainless steel. It maintains high strength to about 600 F (316 C) and it exhibits a moderate level of corrosion resistance. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1992) 41 (5): SS-528.
Published: 01 May 1992
... AL 17-7 alloy, a precipitation hardening stainless steel, has moderate corrosion resistant characteristics and develops high strenth in the precipitation hardened condition. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (2020) 69 (10): SA-865.
Published: 01 October 2020
... Lucefin Group 20MnCr5 and 20MnCrS5 are low-carbon, 1.2Mn-1.1Cr, alloy case-hardening steels that are used in the carburized or carbonitrided, and subsequently quench hardened and tempered, condition. These steels are, in general, used for large casehardened parts requiring high wear resistance...
Journal Articles
Alloy Digest (2020) 69 (12): SA-866.
Published: 01 December 2020
... Lucefin Group 20NiCrMo2-2 and 20NiCrMoS2-2 are low-carbon, Ni-Cr-Mo, alloy case-hardening steels that are used in the carburized or carbonitrided, and subsequently quench hardened and tempered, condition. These steels are, in general, used for medium-size case-hardened parts requiring high fatigue...
Journal Articles
Alloy Digest (2021) 70 (11): SA-877.
Published: 01 November 2021
... Lucefin 50CrMo4 is a medium-carbon, chromium-molybdenum direct hardening alloy steel that is also suitable for flame hardening, induction hardening, and nitriding. This steel is a medium hardenability steel in the 0.45 to 0.50 mean carbon content classification. In general, it is used for medium...
Journal Articles
Alloy Digest (2021) 70 (12): SA-878.
Published: 01 December 2021
... Aubert and Duval CNS (35NiCr6) is a medium-carbon, nickel-chromium, direct hardening alloy steel. It is a medium hardenability steel in the 0.30 to 0.37 mean carbon content classification. This steel is frequently used for water-quenched parts of moderate section size and for oil-quenched parts...
Journal Articles
Alloy Digest (1972) 21 (1): Ni-167.
Published: 01 January 1972
... mandrels physical properties Pyrotool 7 tensile properties workability PYROTOOL 7 Filing Code: Ni-167 Nickel Alloy JANUARY 1972 - DATA ON WORLD WIDE METALS AND ALLOYS Pvblirbd by Engineering Alloys Dim Inc. Upper Momlair, New Jersey PY ROTOOL* 7 (Austenitic Precipitation-Hardenable Nickel-Base Alloy...
Journal Articles
Alloy Digest (1972) 21 (2): SS-268.
Published: 01 February 1972
... CARPENTER C-XB is a hardenable high-carbon high-silicon high-chromium stainless steel offering good high-temperature strength and corrosion resistance to combustion products of automotive gas engines. It is also available in aircraft quality. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1972) 21 (3): Ni-170.
Published: 01 March 1972
... PYROTOOL EX is an austenitic precipitation-hardenable nickel-base alloy with high strength in the range 1000 to 1500 F. When aged it produces a hardness of Rockwell C 40-44. Applications include high-temperature tooling, extrusion dies and dummy blocks. This datasheet provides information...
Journal Articles
Alloy Digest (1972) 21 (4): SS-271.
Published: 01 April 1972
... PYROTOOL 15 is a low-carbon martensitic precipitation-hardenable (maraging) heat-resistant steel designed to possess high strength from room temperature to 1050 F. Uses include tooling applications. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1972) 21 (5): SS-273.
Published: 01 May 1972
... Montclair. New Jersey EMPIRE ISO450* (Martensitic Age-Hardenable Cast Stainless Steel) EMPIRE IS0450 is a cast stainless steel with excellent corrosion resistance. A simple, single-step aging treatmcnl dcvclop, high strength with good ductility and toughness. *EMPIRE and IS0 are registered trademarks...
Journal Articles
Alloy Digest (1972) 21 (9): SA-279.
Published: 01 September 1972
... AISI 8645 is a triple-alloy steel of the oil-hardening type. Its good hardenability and strength make it suitable for axles, shafts and a wide variety of other engineering uses. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1972) 21 (8): Cu-257.
Published: 01 August 1972
... 1820 Pvbhbd by Engineering Alloys Dh XIX. Upper Montclair. New Jersey (Age-Hardenable Chromium-Copper Alloy) MUELLER ALLOY 1820 (formerly MBCo 902) is a chromium-copper alloy with high electrical conductivity, high mechan- ical strength, and superior creep, fatigue and wear properties. It is used...
Journal Articles
Alloy Digest (1972) 21 (10): SA-281.
Published: 01 October 1972
... STROLOY 503-A is a through-hardening steel developed for bearing races. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-281. Producer or source...
Journal Articles
Alloy Digest (1972) 21 (11): Cu-261.
Published: 01 November 1972
... PD-135 is an oxygen-free, age-hardenable copper containing chromium and cadmium. It has excellent mechanical properties and high electrical and thermal conductivities. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1973) 22 (1): Al-205.
Published: 01 January 1973
... ALUMINUM 6061 is a wrought precipitation-hardenable aluminum alloy having excellent resistance to corrosion and good mechanical properties. (This alloy is covered under its old designation, ALUMINUM 61S, in Alloy Digest Al-3, November 1952.) This datasheet provides information on composition...
Journal Articles
Alloy Digest (1973) 22 (2): SA-285.
Published: 01 February 1973
... AISI 4145 is a through-hardening, medium-carbon chromium-molybdenum steel recommended for heavy-duty service. It is suitable for a wide variety of engineering uses. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...