Alloy Digest (1968) 17 (10): SA-232.
Published: 01 October 1968
... ISO-CAST 8 is a cast chromium-molybdenum steel recommended as a general purpose structural alloy of wide application with wide range of mechanical properties. It is used for aircraft and railroad car parts, machine tool and hammermill equipment, gears and shafts. This datasheet provides...