Alloy Digest (1973) 22 (5): CI-40.
Published: 01 May 1973
... ALMANITE WSH is an austenitic nodular iron possessing superior tensile strength, toughness and ability to work harden under conditions of severe pounding impact. It is recommended for crusher liners, hammers, grinding balls, etc. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1957) 6 (4): Zn-4.
Published: 01 April 1957
... No. 2 DIE METAL is a zinc-base alloy recommended primarily for die castings and sand castings (stamping and drop-hammer dies). This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fracture toughness and fatigue...
Journal Articles
Alloy Digest (1967) 16 (10): CI-34.
Published: 01 October 1967
... Ni-Hard Type 4 is a wear-resistant martensitic white iron with improved resistance to fracture under repeated impact. It is recommended for jaw crushers, hammer mills, pulverizers and similar heavy duty wear resistant components. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1969) 18 (3): TS-216.
Published: 01 March 1969
... Dargraph is an oil-hardening, graphitic steel having excellent resistance to abrasive wear, galling, scuffing and scoring. It is recommended for drawing and forming dies, bushings, pneumatic hammers, wear plates, etc. This datasheet provides information on composition, hardness, and tensile...
Journal Articles
Alloy Digest (1960) 9 (1): Mg-44.
Published: 01 January 1960
... MAGNESIUM ALLOY-TA54A is a general purpose hammer-forging alloy having intermediate strength. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information...
Journal Articles
Alloy Digest (1979) 28 (4): Bi-11.
Published: 01 April 1979
...) anchoring inserts in wood, metal or plastics, (2) drop-hammer dies, (3) duplicate patterns in pottery and foundry, and (4) liquid metal bath for heat treating. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on casting...
Journal Articles
Alloy Digest (1979) 28 (12): TS-357.
Published: 01 December 1979
... be water quenched successfully with proper precautions. Its many uses include hammers, hand chisels, boiler punches, shear blades and pneumatic tools. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating...
Journal Articles
Alloy Digest (1980) 29 (10): Cu-404.
Published: 01 October 1980
... MUELLER Alloy 3771 (formerly MBCo. Alloy 211) is one of the most widely used and most easily forged of the copper-base forging alloys. It is most often used in multiple sequence hammer forging operations where a wide forging temperature range is desired. It is also a free-machining alloy. Typical...
Journal Articles
Alloy Digest (1975) 24 (1): TS-281.
Published: 01 January 1975
... for tools such as pins, punches, hammers and sledges. Black Diamond may be expected to give uniform and consistent results, although no definite limits of case depth or grain size are regularly guaranteed. This datasheet provides information on composition, physical properties, hardness, and elasticity...
Journal Articles
Alloy Digest (1982) 31 (6): TS-400.
Published: 01 June 1982
..., it is hardened by austenitizing and quenching in oil. Among the many uses of Mosil are hand chisels, hammers, rivet sets, concrete breakers and heavy-duty punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat...
Journal Articles
Alloy Digest (2000) 49 (3): TS-574.
Published: 01 March 2000
... Cuprodie is a die steel intended for use without water or oil-based lubricants. Some lubricity is provided by low-melting-point copper alloy in this grade. This alloy is suitable for hammers where operation without a lubricant/coolant results in low to moderate die operating temperatures...
Journal Articles
Alloy Digest (2000) 49 (4): TS-576.
Published: 01 April 2000
... Cuprodie 2 die steel is intended for use without water or oil-based lubricants. Some lubricity is provided by low-melting-point copper alloyed in this grade. The alloy is suitable for hammers where operation without a lubricant/coolant results in low to moderate die operating temperatures...
Journal Articles
Alloy Digest (2002) 51 (1): SS-843.
Published: 01 January 2002
... Colmonoy No. 1 is an abrasion-resistant alloy for high-impact applications such as dipper teeth, mill hammers, and catalyst valves. Colmonoy Special No. 1 is an abrasion-resistant iron-base alloy for use where impact is moderate such as ash plows, coal chutes, and dredge cutters. Both alloys can...
Journal Articles
Alloy Digest (2000) 49 (1): TS-570.
Published: 01 January 2000
... Finkl WF-XTRA has high wear resistance while retaining moderate fracture toughness. The alloy is recommended for larger die blocks. The optimum diameter for hardenability is 838 mm (33 in.). It is appropriate for use in high-production hammers where die temperatures may be above average...
Journal Articles
Alloy Digest (2018) 67 (9): TS-753.
Published: 01 September 2018
... YSS DM is a hot work stool steel with excellent toughness. Applications include hammer forging dies, aluminum forge dies, forging bolsters, and extrusion die backers. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming...
Journal Articles
Alloy Digest (1987) 36 (9): TS-480.
Published: 01 September 1987
..., bushings, mandrels, pneumatic hammers, stamps, taps, rotary slitting cutters and wear plates. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-480. Producer or source...
Journal Articles
Alloy Digest (1998) 47 (2): SA-493.
Published: 01 February 1998
... weakens the parts. Machinability: Fir&l FX-XTRA is furnished in the prehardened condition ready for sinking. In the case of special customer requirements. it can be supplied in the annealed state, such as FS. When specified, shanks of hammer dies up to 91-121 cm (36-48 in.) can be soft- ened approximately...
Journal Articles
Alloy Digest (2020) 69 (9): TS-799.
Published: 01 September 2020
... synthetic resin; molding dies; knurling tools; wire drawing dies; mandrels and dies for tube and rod drawing; mandrels for the cold pilger rolling of steel tubes; hammers; reducing dies for needle manufacture. Broaches; cutters for steel wool production; heavyduty woodworking tools. Press tools...
Journal Articles
Alloy Digest (2020) 69 (3): TS-788.
Published: 01 March 2020
..., mandrels and dies for tube and rod drawing, mandrels for the cold pilger rolling of steel tubes, hammers and reducing dies for needle manufacture. Fig. 2 influence of workpiece diameter on the core hardness and hardness penetration for Böhler K100. Harden- ing temperature, 950 °C (1740 °F); quenching...
Journal Articles
Alloy Digest (1994) 43 (9): TS-531.
Published: 01 September 1994
...) in diameter on air cooling from the austenitizing tem- perature. Silicon and nickel improve toughness. The com- plex chromium/vanadium carbides enhance the wear K sistance provided by the martensitic matrix. Applications: Solid cold heading dies, die inserts, heading hammers, coining dies, forming dies...