Alloy Digest (1993) 42 (10): Fe-101.
Published: 01 October 1993
... CARPENTER GLASS SEALING 52 alloy has a virtually constant rate of thermal expansion to 1050 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. Filing Code: FE-101. Producer or source: Carpenter. Producer or Source: Carpenter...
Journal Articles
Alloy Digest (1953) 2 (10): Fe-3.
Published: 01 October 1953
... KOVAR A is a cobalt, nickel, iron alloy recommended for sealing into hard glass. Has similar expansion curve as glass, makes firm bond between metal and glass, is easy to machine and form, and has high resistance to thermal shock. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1955) 4 (3): Fe-6.
Published: 01 March 1955
... RODAR is a cobalt, nickel, iron alloy recommended for sealing into hard glass. Has similar expansion curve as glass, makes firm bond between metal and glass, is easy to machine and form, and has high resistance to thermal shock. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1976) 25 (11): Ni-235.
Published: 01 November 1976
... METGLAS Alloy 2826 (Fe40Ni40P14B6) is a ferromagnetic, high permeability, nickel-iron metallic glass which, when appropriately annealed, yields a material similar to the higher nickel containing permalloys in magnetic properties. Alloy 2826 is a single phase, opaque metallic material with a glass...
Journal Articles
Alloy Digest (1980) 29 (4): Ni-262.
Published: 01 April 1980
... METGLAS MBF-20A is a general-purpose, nickel-base filler metal well suited for brazing stainless steels and heat-resisting nickel alloys. It is supplied as ductile, flexible metallic-glass foil that can be stamped or cut into precision preforms to fit complex joints; it acts as its own shim...
Journal Articles
Alloy Digest (1981) 30 (11): Ni-272.
Published: 01 November 1981
... METGLAS MBF-10A is a brazing foil in ductile, flexible metallic-glass form (a similar grade, MBF-10, is identical except that it has larger dimensional tolerances). This foil provides an alloy with high strength at both elevated and room temperatures. It can be used to join highly stressed...
Journal Articles
Alloy Digest (1981) 30 (12): Ni-273.
Published: 01 December 1981
... METGLAS MBF-30A is a brazing foil in ductile, flexible metallic-glass form (a similar grade, MBF-30, is identical except that it has larger dimensional tolerances). This foil provides an alloy with high strength at both elevated and room temperatures. It can be used to join highly stressed...
Journal Articles
Alloy Digest (1982) 31 (8): Ni-278.
Published: 01 August 1982
... METGLAS MBF-60A is a brazing foil in ductile, flexible metallic-glass form (a similar grade, MBF-60, is identical except that it has larger dimensional tolerances). It is an excellent choice of filler metal for large production runs of low-to-medium stressed assemblies. Its excellent flow...
Journal Articles
Alloy Digest (1983) 32 (1): Ni-282.
Published: 01 January 1983
... METGLAS MBF-15A is a brazing foil in ductile, flexible metallic-glass form (a similar grade, MBF-15, is identical except that it has larger dimensional tolerances). It provides high strength with good resistance against oxidation and corrosion at elevated temperatures. This alloy also withstands...
Journal Articles
Alloy Digest (1983) 32 (5): Ni-286.
Published: 01 May 1983
... METGLAS MBF-75A is a brazing foil in ductile, flexible metallic-glass form (a similar grade, MBF-75, is identical except that it has larger dimensional tolerances). It has excellent high-temperature strength and flows readily into narrow joints. Its high solidus temperature facilitates heat...
Journal Articles
Alloy Digest (1983) 32 (8): Ni-290.
Published: 01 August 1983
... METGLAS MBF-80A is a brazing foil in ductile, flexible metallic-glass form (a similar grade, MBF-80, is identical except that it has larger dimensional tolerances). It provides high-strength brazements at elevated temperatures and good moderate-temperature resistance to oxidation and corrosion...
Journal Articles
Alloy Digest (1984) 33 (4): Ni-296.
Published: 01 April 1984
... METGLAS MBF-35A is a brazing foil in ductile flexible metallic-glass form (a similar grade, MBF-35, is identical except that it has larger dimensional tolerances. It is a low-temperature filler metal foil designed for joining superalloys where the brazing operation should be done simultaneously...
Journal Articles
Alloy Digest (1984) 33 (6): Ni-298.
Published: 01 June 1984
... METGLAS MBF-90/MBF-90A is a brazing foil in ductile, flexible metallic-glass form (a similar grade, MBF-90, is identical except that is has larger dimensional tolerances. It is suitable for joining stainless steels and superalloys, including those containing aluminum and titanium. It provides high...
Journal Articles
Alloy Digest (1984) 33 (9): Ni-303.
Published: 01 September 1984
... METGLAS MBF-17A is a brazing foil in ductile, flexible metallic-glass form (A similar grade, MBF-17, is identical except that it has larger dimensional tolerances). It provides high strength at both elevated and room temperatures with moderate oxidation and corrosion resistance. An example...
Journal Articles
Alloy Digest (1984) 33 (12): Ni-306.
Published: 01 December 1984
... METGLAS MBF-65A is a brazing foil in ductile, flexible metallic-glass form (A similar grade, MBF-65 is identical except that it has larger dimensional tolerances). The chromium content (nominally 14%) provides superior resistance to corrosion and oxidation. This alloy is recommended for inert...
Journal Articles
Alloy Digest (1970) 19 (8): Fe-44.
Published: 01 August 1970
... UNISEAL 42 is a closely controlled thermal expansion iron alloy used for glass-to-metal and metal-to-ceramic seals. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, joining...
Journal Articles
Alloy Digest (1970) 19 (8): Ni-156.
Published: 01 August 1970
... UNISEAL 52 is a nickel-iron alloy produced for glass-to-metal seals with higher-than-normal thermal expansion glasses such as Types O120 and 9010. It is used in hermetically-sealed magnetic dry reed switches, compression seals, and ceramic seals where expansion is required to be almost linear...
Journal Articles
Alloy Digest (1970) 19 (11): Fe-45.
Published: 01 November 1970
... UNISEAL 29-17 is a controlled expansion iron-base alloy containing nickel and cobalt. It is widely used for glass-to-metal seals with borosilicate glasses commonly employed in electronic power tube envelopes. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1993) 42 (11): Fe-102.
Published: 01 November 1993
... CARPENTER GLASS SEALING 42 has wide-ranging applications in glass-to-metal and ceramic-to-metal sealing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, joining...
Journal Articles
Alloy Digest (1961) 10 (8): Fe-11.
Published: 01 August 1961
... THERLO, also known as D-H Alloy No. 373, is an iron-nickel-cobalt alloy ideally suited for sealing to glass. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining...