Skip Nav Destination
Close Modal
Search Results for
glass-to-metal seals
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 85 Search Results for
glass-to-metal seals
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (10): Fe-101.
Published: 01 October 1993
... Copyright © ASM International® 1996 1996 ASM International Carpenter Glass Sealing 52 chemical composition elasticity hardness physical properties tensile properties thermal expansion CARPENTER GLASS SEALING 52 Filing Code: Iron Alloy Fe-l 01 - DIGEST- OCTOBER 1993 DATA ON WORLD WIDE METALS...
Abstract
View article
PDF
CARPENTER GLASS SEALING 52 alloy has a virtually constant rate of thermal expansion to 1050 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. Filing Code: FE-101. Producer or source: Carpenter.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1999) 48 (1): Fe-119.
Published: 01 January 1999
... chemical composition elasticity hardness physical properties Sealvar tensile properties thermal properties SEALVAR® (Glass to Metal Sealing Alloy) SEALVAR is an iron-nickel-cobalt strip alloy primarily used for making hermetic seals with harder glasses and ceramics. It is distinguished by its high...
Abstract
View article
PDF
SEALVAR is an iron-nickel-cobalt strip alloy primarily used for making hermetic seals with harder glasses and ceramics. It is distinguished by its high purity, closely controlled chemistry and very low carbon level. The alloy meets specified ASTM F 15-78 (83) expansion coefficients. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. Filing Code: FE-119. Producer or source: AMETEK Specialty Metal Products.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1970) 19 (8): Fe-44.
Published: 01 August 1970
... UNISEAL 42 is a closely controlled thermal expansion iron alloy used for glass-to-metal and metal-to-ceramic seals. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, joining...
Abstract
View article
PDF
UNISEAL 42 is a closely controlled thermal expansion iron alloy used for glass-to-metal and metal-to-ceramic seals. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, joining, and surface treatment. Filing Code: Fe-44. Producer or source: Cyclops Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1970) 19 (8): Ni-156.
Published: 01 August 1970
... UNISEAL 52 is a nickel-iron alloy produced for glass-to-metal seals with higher-than-normal thermal expansion glasses such as Types O120 and 9010. It is used in hermetically-sealed magnetic dry reed switches, compression seals, and ceramic seals where expansion is required to be almost linear...
Abstract
View article
PDF
UNISEAL 52 is a nickel-iron alloy produced for glass-to-metal seals with higher-than-normal thermal expansion glasses such as Types O120 and 9010. It is used in hermetically-sealed magnetic dry reed switches, compression seals, and ceramic seals where expansion is required to be almost linear to 1000 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-156. Producer or source: Cyclops Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1970) 19 (11): Fe-45.
Published: 01 November 1970
... UNISEAL 29-17 is a controlled expansion iron-base alloy containing nickel and cobalt. It is widely used for glass-to-metal seals with borosilicate glasses commonly employed in electronic power tube envelopes. This datasheet provides information on composition, physical properties, hardness...
Abstract
View article
PDF
UNISEAL 29-17 is a controlled expansion iron-base alloy containing nickel and cobalt. It is widely used for glass-to-metal seals with borosilicate glasses commonly employed in electronic power tube envelopes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Fe-45. Producer or source: Cyclops Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1961) 10 (8): Fe-11.
Published: 01 August 1961
... glass-to-metal seals with the so-cakd hard giass. The alloy has a thermal expansion similar to that of hard giass aii the way from room temperature up to the annealing temperature of the glass. Therio has a high resistance to amalgamation with mercury and exceptional resistance co high thermal shock...
Abstract
View article
PDF
THERLO, also known as D-H Alloy No. 373, is an iron-nickel-cobalt alloy ideally suited for sealing to glass. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: Fe-11. Producer or source: Driver-Harris Company. Originally published July 1956, revised August 1961.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1953) 2 (10): Fe-3.
Published: 01 October 1953
... KOVAR A is a cobalt, nickel, iron alloy recommended for sealing into hard glass. Has similar expansion curve as glass, makes firm bond between metal and glass, is easy to machine and form, and has high resistance to thermal shock. This datasheet provides information on composition, physical...
Abstract
View article
PDF
KOVAR A is a cobalt, nickel, iron alloy recommended for sealing into hard glass. Has similar expansion curve as glass, makes firm bond between metal and glass, is easy to machine and form, and has high resistance to thermal shock. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: Fe-3. Producer or source: Carborundum Company, Refractories Division.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1955) 4 (3): Fe-6.
Published: 01 March 1955
... RODAR is a cobalt, nickel, iron alloy recommended for sealing into hard glass. Has similar expansion curve as glass, makes firm bond between metal and glass, is easy to machine and form, and has high resistance to thermal shock. This datasheet provides information on composition, physical...
Abstract
View article
PDF
RODAR is a cobalt, nickel, iron alloy recommended for sealing into hard glass. Has similar expansion curve as glass, makes firm bond between metal and glass, is easy to machine and form, and has high resistance to thermal shock. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: Fe-6. Producer or source: Wilbur B. Driver Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (5): Fe-136.
Published: 01 May 2005
... Carpenter Glass Sealing 27 is a ductile chromium-iron alloy that has been used for strong glass-to-metal seals in electronic and vacuum tubes, and incandescent and fluorescent lamps. It exhibits no phase transformation up to 1150 deg C (2100 deg F). This datasheet provides information...
Abstract
View article
PDF
Carpenter Glass Sealing 27 is a ductile chromium-iron alloy that has been used for strong glass-to-metal seals in electronic and vacuum tubes, and incandescent and fluorescent lamps. It exhibits no phase transformation up to 1150 deg C (2100 deg F). This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance. Filing Code: FE-136. Producer or source: Carpenter Technology Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (12): Fe-60.
Published: 01 December 1979
... properties that are ideal for usage in glass-to-metal seals. Typical applications are transmitting tubes, relays and electronic power tube envelopes. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature...
Abstract
View article
PDF
TECHALLOY GLASSEAL 29-17 is an iron-nickel-cobalt alloy with a thermal expansion rate that is unlike most metals and closely matches the thermal expansion characteristics of borosilicate glass, PYREX glass, and other similar low-expansion materials. It assures precisely controlled expansion properties that are ideal for usage in glass-to-metal seals. Typical applications are transmitting tubes, relays and electronic power tube envelopes. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Fe-60. Producer or source: Techalloy Company Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1976) 25 (4): Ni-226.
Published: 01 April 1976
... ALLOY 52 is a controlled-expansion alloy developed for glass-to-metal seals for some of the soft glasses and some ceramics. Its rate of expansion is almost constant up to approximately 1050 F (565 C). This datasheet provides information on composition, physical properties, hardness, elasticity...
Abstract
View article
PDF
ALLOY 52 is a controlled-expansion alloy developed for glass-to-metal seals for some of the soft glasses and some ceramics. Its rate of expansion is almost constant up to approximately 1050 F (565 C). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-226. Producer or source: Magnetics Specialty Metals Division.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (5): Ni-260.
Published: 01 May 1979
... TECHALLOY GLASSEAL 52 is a nickel-iron alloy produced for glass-to-metal seals with higher than normal thermal-expansion glasses such as Types 0120 and 9010, and certain ceramics. It has relatively good mechanical properties: a tensile strength of 80,000 psi and an elongation of 35%. It is used...
Abstract
View article
PDF
TECHALLOY GLASSEAL 52 is a nickel-iron alloy produced for glass-to-metal seals with higher than normal thermal-expansion glasses such as Types 0120 and 9010, and certain ceramics. It has relatively good mechanical properties: a tensile strength of 80,000 psi and an elongation of 35%. It is used in a number of applications where expansion is required to be almost linear to 1000 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-260. Producer or source: Techalloy Company Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1982) 31 (6): Ni-276.
Published: 01 June 1982
... The 50 Nickel-Iron Alloy is recommended for glass-to-metal seals. It is used with such glasses as Types 0120 and 9010 that have higher than normal thermal expansion and with certain ceramics. It is used in a number of applications where expansion must be almost linear to 1000 F. The 50 Nickel-Iron...
Abstract
View article
PDF
The 50 Nickel-Iron Alloy is recommended for glass-to-metal seals. It is used with such glasses as Types 0120 and 9010 that have higher than normal thermal expansion and with certain ceramics. It is used in a number of applications where expansion must be almost linear to 1000 F. The 50 Nickel-Iron Alloy has relatively good mechanical properties; in fact, at room temperature it has a tensile strength of 80,000 psi and an elongation of 35%. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-276. Producer or source: Mills that produce iron-nickel alloys.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1966) 15 (1): Fe-16.
Published: 01 January 1966
... NILO K has been developed specifically for the production of matched glass-to-metal seals when using hard, borosilicate glass. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating...
Abstract
View article
PDF
NILO K has been developed specifically for the production of matched glass-to-metal seals when using hard, borosilicate glass. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: Fe-16. Producer or source: Henry Wiggin & Company Ltd. Originally published August 1959, revised January 1966.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (1): Cu-903.
Published: 01 January 2020
... Olin Brass Alloy C10200 is an oxygen-free, high-conductivity copper. It is ideal for applications where extremely high electrical conductivity and resistance to hydrogen embrittlement are vital. Where glass-to-metal seals are required this material also provides the added advantage of developing...
Abstract
View article
PDF
Olin Brass Alloy C10200 is an oxygen-free, high-conductivity copper. It is ideal for applications where extremely high electrical conductivity and resistance to hydrogen embrittlement are vital. Where glass-to-metal seals are required this material also provides the added advantage of developing an adherent, nonscaling oxide at elevated temperatures. This datasheet provides information on composition and physical properties. It also includes information on corrosion resistance. Filing Code: Cu-903. Producer or source: Olin Brass GBC Metals, LLC.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (8): Ni-136.
Published: 01 August 1968
... BLENDALLOY 25-5200 is a 52% nickel-iron controlled expansion, glass-to-metal sealing alloy recommended for dry reed switches and mercury wetted relays. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Abstract
View article
PDF
BLENDALLOY 25-5200 is a 52% nickel-iron controlled expansion, glass-to-metal sealing alloy recommended for dry reed switches and mercury wetted relays. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-136. Producer or source: Magnetics Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (6): Fe-77.
Published: 01 June 1987
... NILO Alloy 42 is a binary nickel-iron alloy having a low and nominally constant expansion coefficient over the range 20-300 C (68-572 F). It is used for semiconductor lead frames, thermostats and glass-to-metal seals. This datasheet provides information on composition, physical properties...
Abstract
View article
PDF
NILO Alloy 42 is a binary nickel-iron alloy having a low and nominally constant expansion coefficient over the range 20-300 C (68-572 F). It is used for semiconductor lead frames, thermostats and glass-to-metal seals. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming and heat treating. Filing Code: Fe-77. Producer or source: Inco Alloys International Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (10): Fe-80.
Published: 01 October 1987
... NILO alloy 48 is a binary iron-nickel alloy used primarily for glass-to-metal seals. It is also used in thermostats up to 450 C (842 F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming, heat...
Abstract
View article
PDF
NILO alloy 48 is a binary iron-nickel alloy used primarily for glass-to-metal seals. It is also used in thermostats up to 450 C (842 F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Fe-80. Producer or source: Inco Alloys International Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (11): Fe-102.
Published: 01 November 1993
... CARPENTER GLASS SEALING 42 has wide-ranging applications in glass-to-metal and ceramic-to-metal sealing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, joining...
Abstract
View article
PDF
CARPENTER GLASS SEALING 42 has wide-ranging applications in glass-to-metal and ceramic-to-metal sealing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, joining, and surface treatment. Filing Code: FE-102. Producer or source: Carpenter.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (6): Fe-137.
Published: 01 June 2005
...) 276 (40) Elongation in 50 mm (2 in % 30 Hardness, HRB 80 Heat Treatment: To form a tight, dark green oxide film for glass-to-metal sealing, bubble hydrogen through water and into furnace held at 1038 1149 °C (1900 2100 °F). The temperature used for oxidiz- ing depends on the type of furnace, muffle...
Abstract
View article
PDF
Carpenter Glass Sealing 42-6 alloy has been used for sealing to Corning 0120 glass. A special thermal treatment develops a tightly adherent oxide beneficial to obtaining hermetic seals. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming and heat treating. Filing Code: FE-137. Producer or source: Carpenter Technology Corporation.