1-20 of 292 Search Results for

gear cases

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2005) 54 (12): SA-553.
Published: 01 December 2005
... Ferrium C69 is a case/core steel with a case hardness of 69 HRC and a core hardness of 50 HRC. It is used in racing applications, where rolling contact fatigue is an issue, and will be undergoing testing by the National Aeronautics and Space Administration (NASA) for aerospace gear applications...
Journal Articles
Alloy Digest (1967) 16 (2): Al-163.
Published: 01 February 1967
... Aluminum A357 is a high strength, pressure tight sand and permanent mold aluminum casting alloy. It is age-hardenable. It is recommended for cast gear cases, cylinder heads, transmission cases and strong structural castings. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1986) 35 (12): Al-274.
Published: 01 December 1986
... cases, gear cases, oil pans, airframe fittings and instrument housings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion...
Journal Articles
Alloy Digest (1976) 25 (5): Al-223.
Published: 01 May 1976
... ALUMINUM 356.0 is an aluminum casting alloy that normally is used only when heat-treated (aged) strengths are required. It is recommended for high strength, pressure-tight castings, intricate shapes and good resistance to corrosion. Its many applications include gear cases, instrument housings...
Journal Articles
Alloy Digest (1985) 34 (1): SA-405.
Published: 01 January 1985
... UNS No. G46260 is a carburizing grade of alloy steel. Both the core and the carburized case have relatively good mechanical properties. This steel is used for producing case-hardened parts such as gears, pinions, chuck jaws and camshafts. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1968) 17 (4): SA-225.
Published: 01 April 1968
... for applications such as rocket motor cases and accessories, bolts and fasteners and aircraft structural components- particularly landing gear. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (1962) 11 (10): SA-136.
Published: 01 October 1962
... AISI 4422 is a carbon-molybdenum type carburizing steel designed as alternate for the AISI 8600 grades of steel for single quench practice. It is recommended for case hardened gears, pinions, shafts and the like. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1962) 11 (11): SA-137.
Published: 01 November 1962
... martensitic steel which is strengthened by precipitation hardening. It has excellent combination of strength and toughness particularly in the presence of notches and cracks. It is recom- mended for applications such as solid fuel rocket cases and aircraft landing gear. Composition: Physical Constants: Carbon...
Journal Articles
Alloy Digest (1963) 12 (9): SA-154.
Published: 01 September 1963
... ALMAR 25 is a maraging alloy steel having an excellent combination of strength and toughness particularly in the presence of notches or cracks. It is recommended for applications such as fuel rocket cases and aircraft landing gears. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1963) 12 (10): SA-156.
Published: 01 October 1963
... ALMAR 18 is a high-nickel martensitic steel which is strengthened by precipitation hardening. It has excellent combination of strength and toughness particularly in the presence of notches or cracks. It is recommended for applications such as solid fuel rocket cases and aircraft landing gears...
Journal Articles
Alloy Digest (1964) 13 (3): SA-161.
Published: 01 March 1964
... AISI 4023 is a low carbon, molybdenum case hardening steel, recommended for gears, pinions, camshafts, etc., where hard wear resistant surfaces and tough cores are desired. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1964) 13 (4): SA-162.
Published: 01 April 1964
... ALMAR 20 is a high nickel martensitic steel which is strengthened by precipitation hardening. It has excellent combination of strength and toughness particularly in the presence of notches and cracks. It is recommended for applications such as solid fuel rocket cases and aircraft landing gear...
Journal Articles
Alloy Digest (1965) 14 (7): SA-180.
Published: 01 July 1965
... AISI 8615 is a low-carbon, nickel-chromium-molybdenum alloy steel capable of producing high core strength and toughness. It is a case hardening steel recommended for heavy duty gears, cams, shafts, chains, fasteners, piston pins, etc. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1974) 23 (6): SA-306.
Published: 01 June 1974
... SAE 4427 is a 0.5% molybdenum steel designed for carburizing applications and it is also useful for general purposes. It is recommended for case-hardened gears, pinions, shafts and similar components. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1985) 34 (6): SA-409.
Published: 01 June 1985
... steel and is outstanding for- its uniformity of case and response to heat treatment, relative freedom from distortion during quenching, and excellent toughness at high hardness. The permissible compressive stress (Hertz) on case-hardened gears is 230.000 psi on the average. with maximum stress...
Journal Articles
Alloy Digest (1969) 18 (8): SA-242.
Published: 01 August 1969
... Republic RSM-300 alloy is an 18% nickel-cobalt-molybdenum age-hardening steel designed to develop up to 300,000 psi yield strength with good toughness. It is recommended for landing gears extrusion dies, rocket motor cases, high-strength bolts, etc. This datasheet provides information...
Journal Articles
Alloy Digest (1970) 19 (6): SA-253.
Published: 01 June 1970
... SAE 4626 is a carburizing alloy steel suitable for producing case-hardened parts, such as gears, pinions and camshafts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1955) 4 (10): CI-12.
Published: 01 October 1955
...: Applications: Machine tool castings, gears, sllafu, housings, pump bodies, valve bodies, steam cylinden, cylinder hers, casings, cylinder heads, governor frames. Manufachwer: Foundries under conttact with Meehanite Metal Corporation New Rocheile, New York ...
Journal Articles
Alloy Digest (1990) 39 (10): SA-450.
Published: 01 October 1990
... CBS-1000M VIM-VAR is a carburizing bearing and gear steel designed for service up to 800 F(427 C). It is produced by vacuum induction melting followed by vacuum arc remelting to provide optimum strength, ductility, fatigue life and fracture toughness. The hardened case properties match those of M...
Journal Articles
Alloy Digest (2005) 54 (11): SA-551.
Published: 01 November 2005
... Ferrium C61 is a case/core alloy with ultrahigh strength and excellent fracture toughness. It is used in gears and a number of automotive racing applications. This datasheet provides information on tensile properties. It also includes information on forming and heat treating. Filing Code: SA-551...