1-20 of 37 Search Results for

gaskets

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1970) 19 (1): Cu-210.
Published: 01 January 1970
... ALRONZE is a high strength, special aluminum bronze having excellent corrosion and stress-corrosion resistance. It is recommended for electrical contacts, springs, gaskets, cutlery, wear plates, etc. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1978) 27 (7): In-1.
Published: 01 July 1978
... INDALLOY No. 4 is the metallic element indium. It is a very versatile, malleable and soft metal; it is softer even than lead. Indium remains malleable at temperatures approaching absolute zero; therefore, it is an excellent for a variety of applications including gaskets and seals. It is a useful...
Journal Articles
Alloy Digest (2015) 64 (11): SS-1232.
Published: 01 November 2015
... is an austenitic stainless steel for automotive head gaskets, exhaust manifold gaskets, various diaphragms, and various components needing fatigue resistance. Producer: Nippon Steel and Sumitomo Metal Chicago, IL 60611, USA Tel: (312) 751-0800 Fax: (312) 751-0345 In Japan: Chiyoda-ku, Tokyo 100-871, Japan Tel: +81...
Journal Articles
Alloy Digest (2015) 64 (2): SS-1201.
Published: 01 February 2015
..., and strip forms. Applications: Nonmagnetic spring, gaskets, electronic components, and other components where magnetism is not desired. Producer: Nippon Yakin Kogyo Co., Ltd. 1-5-8, Kyobashi, Chuo-ku, Tokyo 104-8365, Japan Tel: + 81 (3) 3273-4649 Fax: +81 (3) 3273-4642 www.nyk.co.jp ISSN: 002-614X SS-1201B...
Journal Articles
Alloy Digest (1957) 6 (11): SS-64.
Published: 01 November 1957
...- antes, electric ranges, manifolds, collector rings, heaters, gaskets, jet blankets, combustion liners, thermocouple coverings, petrochemical equipment. Manufacturer: The International Nickel Company, Inc. New York 5, New York ...
Journal Articles
Alloy Digest (1994) 43 (8): Ni-459.
Published: 01 August 1994
... deformation is acceptable. Those stresses may result in dimensional changes due to permanent strain and are not recommended for applications such as flanges of gasketed joints. DOI: 10.31399/asm.ad.ni0459 Copyright © ASM International® 1996 Specification Equivalents: ASTM B409 ASME SB409 General...
Journal Articles
Alloy Digest (1992) 41 (10): SS-535.
Published: 01 October 1992
... to permanent strain. These stress values are not recommended for the flanges of gasket joints or other applications where slight amounts of distortion can cause leakage or malfunction. Heat Treatments: Annealing is accomplished by heating to 1700- 1800°F for one-half hour per inch of section and water quenched...
Journal Articles
Alloy Digest (2011) 60 (7): SS-1096.
Published: 01 July 2011
... in coil). DOI: 10.31399/asm.ad.ss1096 Applications: Nonmagnetic spring, gaskets, electronic components, and other components where magnetism is not desired Producer: Nippon Yakin Kogyo Co., Ltd. San ei Bldg., 1 5 8, Kyobashi Chuo ku, Tokyo 104 8365 Japan Tel: + 81 (3) 3273 4649 Fax: +81 (3) 3273 4642 Web...
Journal Articles
Alloy Digest (1984) 33 (10): Cu-485.
Published: 01 October 1984
..., gaskets, gift hollow ware and lead frames. Manufacturers: Copper alloy mills. ...
Journal Articles
Alloy Digest (2020) 69 (11): TS-804.
Published: 01 November 2020
..., blanking of electrical sheet, cold forging, deep drawing, extruder screws, fine blanking, gasket stamping, granulator knives, powder pressing, slitting knives (paper and foil). Supplier Uddeholms AB (a voestalpine company) Uvedsvägen SE-683 33 Hagfors, Sweden Tel: +1 800 638 2520 (USA) Web...
Journal Articles
Alloy Digest (1990) 39 (11): Cu-554.
Published: 01 November 1990
.... Resistance butt welding is satisfactory; spot and seam methods not recommended. Forms Available: Strip, sheet, plate, rod, wire and shapes. Applications: Architectural; Building fronts, downspouts, flashing, gut- ters, roofing, screening, spouting. Automotive; Gaskets, radiators. Electrical; bus bars...
Journal Articles
Alloy Digest (2022) 71 (5): Cu-931.
Published: 01 May 2022
.... Product Forms Bar; rod; profiles. Applications Category Architecture Automotive Builder s hardware Electrical Industrial Applications Downspouts, flashing, roofing, gutters, building fronts, skylight frames, kitchen counter tops. Gaskets, radiators. Ball floats, butts, rivets, nails, cotter pines...
Journal Articles
Alloy Digest (1964) 13 (10): Cu-146.
Published: 01 October 1964
... this temperature is very slow. Forms Available: Sheet and strip. Applications: Electrical and electronic components, hollow ware, coffee pots, gaskets, springs, diaphrams. Manufacturer: Olin Mathieson Chemical Corp. Metals Division East Alton, Illinois New Haven, Connecticut ...
Journal Articles
Alloy Digest (1989) 38 (5): Ti-92.
Published: 01 May 1989
... used to con- trol biofouling. A possible limiting factor can be corrosion in metal-to-metal crevices or metal-to-gasket interfaces, depending on chloride environment, temperature and PH. Resistance improves as temperature and pH increase. Titanium is resistant o erosion and cavitation in sea water...
Journal Articles
Alloy Digest (1995) 44 (3): TS-536.
Published: 01 March 1995
...; fine blanking; blank- ing of electrical shees gasket stamping: deep drawing: cold forging; slitting knives (paper and foil); powder pressing; granular knives; exuuder screw, etc. Producer: UDDEHOLM Corporation Rolling Meadows, IL 60008 708-577-2220 ...
Journal Articles
Alloy Digest (1991) 40 (10): Cp-18.
Published: 01 October 1991
... valve seats, washers, gaskets, compressor seals and pump parts. Producer: Du Pant. Wilmington, Delaware 19898 ...
Journal Articles
Alloy Digest (1976) 25 (7): Cu-314.
Published: 01 July 1976
... by the processes normally used for copper alloys. Forms Available: Strip and sheet. Applications: Components for electrical and electronic applications, such as springs, contacts, connectors, terminals, fuse clips, transistor bases, lead frames, plug contacts, clamps, fastenings and gaskets. Also diaphragms...
Journal Articles
Alloy Digest (2021) 70 (4): Cu-919.
Published: 01 April 2021
... weather stripping. Electrical J/(kg K) 20 °C 25.5 Consumer Ball point pens; chain links; compacts; conductivity (cal/(g °C)) (68 °F) (44)(a)(b) costume jewelry; gaskets; housing for lipstick Electrical compacts; lipstick cases. m Hardware circular-mil/ Industrial Cable wrap. Ordnance ft) Doorknobs; hinges...
Journal Articles
Alloy Digest (2020) 69 (4): Ti-165.
Published: 01 April 2020
.... Donachie, Jr., Titanium: A Technical Guide, 2nd Edition, ASM International, 2000. Product Forms Coil: foil, ribbon, strip Wire: flat, profile, round, square Finishes See Table 3. Applications Aircraft skin, aircraft structural honeycomb, bellows, deep drawing applications, gaskets, heat exchanger parts...
Journal Articles
Alloy Digest (1971) 20 (5): Cu-233.
Published: 01 May 1971
... produced from strip. Applications: Electrical components such as springs, contacts, connectors, terminals, cable tape, fuse clips, plug contacts, clamps, transistor bases, fastenings, -gaskets, chaphra&, hdlow ware, giftware, flexible hose, architectural aoolications. lead frames, integrated circuit frames...