Alloy Digest (1995) 44 (3): SS-587.
Published: 01 March 1995
... the semiconductor market to maintain gas purity. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on heat treating, machining, and joining. Filing Code: SS-587. Producer or source: Carpenter Technology Corporation. Producer...
Journal Articles
Alloy Digest (1992) 41 (9): Ni-412.
Published: 01 September 1992
... INCONEL FILLER METAL 52 is a high chromium filler metal for gas-metal-arc and gas-tungsten-arc welding of Inconel Alloy 690 (See Alloy Digest Ni-266, March 1981). Higher chromium is beneficial in resisting stress-corrosion cracking in high purity water for pressurized water reactors...
Journal Articles
Alloy Digest (2006) 55 (8): SS-970.
Published: 01 August 2006
... Allvac Ultra-High Purity 316L stainless steel was developed for the semiconductor industry to minimize microcontamination from defects and impurities on electropolished surfaces. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also...
Journal Articles
Alloy Digest (1972) 21 (12): Ni-183.
Published: 01 December 1972
... BLENDALLOY 22-1000 is a high-purity nickel for use where low base hardness, high, ductility, and a low work-hardening rate combined with product purity, corrosion resistance, heat dissipation, electrical conductivity and formability considerations are required. This datasheet provides information...
Journal Articles
Alloy Digest (1984) 33 (8): Ni-301.
Published: 01 August 1984
... NICKEL 290 is a high-purity grade of nickel made by a powder-metallurgy process. Its high purity makes it useful for electronic applications such as components of hydrogen thyratrons and for battery applications. The low annealing temperature of Nickel 290 makes it superior to other forms...
Journal Articles
Alloy Digest (1998) 47 (3): In-3.
Published: 01 March 1998
.... High purity indium is used in electronic device technology. crystal growth in epitaxial processes, and the production of single crystal I&V compound semiconductors. Chemical Composition: ~-P==paW(ppbh) 6N 6Ns 6Nswa 7N B Al w Si S Fe Ni ch zm Ga E cd sn n Pb Bi MO ca Toral-ilD- Cl00 60 Cl00 Cl0 ND 40...
Journal Articles
Alloy Digest (2011) 60 (2): Ni-686.
Published: 01 February 2011
... HPM 270 Nickel is a high purity nickel free from nonmetallic inclusions. Its good ductility easily permits significant cold reduction without annealing. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1969) 18 (3): Ni-143.
Published: 01 March 1969
... Nickel 270 is a high purity nickel exceptionally free from non-metallic inclusions. Its low hardness and good ductility permit heavy cold deformation without reannealing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (2017) 66 (4): Ti-159.
Published: 01 April 2017
... ATI 6-4 ELI, also known as Grade 23, is a higher purity grade of ATI Ti-6Al-4V for use in surgical and medical applications. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1959) 8 (7): Al-80.
Published: 01 July 1959
... ALUMINUM 357 is a highly purity aluminum casting alloy which develops high tensile and yield strengths with good ductility after heat treatment. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on corrosion resistance as well...
Journal Articles
Alloy Digest (1998) 47 (12): Re-2.
Published: 01 December 1998
... has been done. Strip and wire as thin as 2 mils are possible. Welding. Rhenium can be welded soldered, or brazed by con- ventional means. Welds made by inert-gas or electron beam methuds ate extremely ductile and can be formed further at room temperamre. Products Available: Ribbon. Uses of rhenium...
Journal Articles
Alloy Digest (2023) 72 (6): Ti-193.
Published: 01 June 2023
... Elgiloy CP Titanium Grade 1 / Ti 25 is an unalloyed commercially pure titanium. It has the highest purity, lowest strength, and best ductility and formability of the four ASTM unalloyed titanium grades. This grade can be used in the temperature range -184 to 540 °C (-300 to 1000 °F...
Journal Articles
Alloy Digest (2008) 57 (5): Al-413.
Published: 01 May 2008
... Kaiser aluminum alloy 2124 is a high-purity version of 2024 with tighter controls on the iron and silicon for an increase in strength and toughness. It is primarily used as plate in the aircraft industry. This data sheet applies to sheet, coil, and plate in the T851 temper. This datasheet provides...
Journal Articles
Alloy Digest (2008) 57 (6): Al-414.
Published: 01 June 2008
... Kaiser Aluminum alloy 7175/7475 is a high-purity version of 7075 and is heavily used by the aircraft and ordinance industries because of its superior strength. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1953) 2 (9): Mg-7.
Published: 01 September 1953
... DOWMETAL FS and FS-1 are wrought magesium-base alloys that do not respond to age-hardening heat treatment for increased hardness and strength. They are general purpose extrusion alloys. DOWMETAL FS-1 is the controlled purity grade. Extrusions are supplied in both FS and FS-1. Sheet and plate...
Journal Articles
Alloy Digest (1988) 37 (5): Mg-73.
Published: 01 May 1988
... AZ91D and AZ91E alloys are magnesium-aluminum-zinc-manganese alloys of closely controlled purity. Ingot is available for use in the production of improved corrosion resistant sand, permanent-mold and die castings. AZ91D is used for die casting and AZ91E for sand and permanent-mold castings...
Journal Articles
Alloy Digest (1972) 21 (12): SS-285.
Published: 01 December 1972
...-Brite 26-1 suggest good blanking, piercing, press-brake forming, spinning, roll forming, and embossing characteristics. E-BRITE 26-l is a chromiummolybdenum ferritic stainless steel that is produced by electron-beam melting. It is a high-purity material with very low gas content and, as a result...
Journal Articles
Alloy Digest (1980) 29 (1): Al-161.
Published: 01 January 1980
... ALUMINUM 5252 is a high-purity aluminum-magnesium alloy of moderate strength, good fabricating characteristics and excellent resistance to corrosion. It is highly resistant to denting and is used widely as trim in the automotive industry and for a wide variety of other industrial products...
Journal Articles
Alloy Digest (1973) 22 (12): Cu-273.
Published: 01 December 1973
... AMAX-LP is an oxygen-free low phosphorus copper produced from a high purity oxygen-free copper. It has a minimum electrical conductivity of 90% IACS and is used in applications such as refrigerator tubing and components where a material having a somewhat lower electrical conductivity than...
Journal Articles
Alloy Digest (1973) 22 (11): Cu-272.
Published: 01 November 1973
... AMAX-XLP is an oxygen-free low-phosphorus copper identical in electrical conductivity to that specified for deoxidized low-phosphorus (DLP) copper, but with a lower phosphorus range than that required in DLP copper. AMAX-XLP is produced from high-purity oxygen-free copper; this results...