1-20 of 1197 Search Results for

gas industry

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2011) 60 (4): Ni-689.
Published: 01 April 2011
...-base powder that is used primarily for the local repair and hard facing of glass- forming molds and in the manufacture of down-hole stabilizers in the oil and gas industry. It is typically deposited as a machinable, nonmagnetic spray-fuse (SF) or powder weld deposited overlay. It is similar to Deloro...
Journal Articles
Alloy Digest (2014) 63 (4): Ni-666.
Published: 01 April 2014
... MR0175 / ISO 15156-3 up to NACE level VI. Properties of alloy 945 are defined in the Special Metals Corporation internal specification, HA 119, Rev. 0. Alloy 945 is available as round bar, forging stock, and tubing. Applications: Alloy 945 is especially suited for applications in the oil and gas industry...
Journal Articles
Alloy Digest (2006) 55 (2): SA-554.
Published: 01 February 2006
... Superelso 500HR, also known as SE 500HR, is a high yield strength, quenched-and-tempered alloy for wet H2S service in the oil and gas industry. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on corrosion resistance as well as...
Journal Articles
Alloy Digest (1988) 37 (4): Ni-330.
Published: 01 April 1988
..., flue gas desulfurization systems and the pulp and paper industries. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and...
Journal Articles
Alloy Digest (1993) 42 (12): SS-558.
Published: 01 December 1993
...-shore technology and in the gas and oil industry. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat...
Journal Articles
Alloy Digest (1987) 36 (1): SS-481.
Published: 01 January 1987
... and 317L stainless steels. Its many uses include marine scrubbers, desalination equipment, sulfuric acid production, wet phosphoric acid production, mild sour gas wells, urea production and pulp and paper industry. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1957) 6 (12): Ni-38.
Published: 01 December 1957
... INCOLOY 901 is a nickel-base alloy having creep and rupture strength at 1000 to 1400 F. It is recommended for use in aircraft and industrial gas turbine components. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also...
Journal Articles
Alloy Digest (1990) 39 (7): Cer-4.
Published: 01 July 1990
... SILICON NITRIDE SN-220 has found its niche in industrial applications in engine and gas turbine components. It has excellent high-temperature strength and thermal shock resistance. This datasheet provides information on composition, physical properties, elasticity, and bend strength as well as...
Journal Articles
Alloy Digest (1978) 27 (8): Cu-358.
Published: 01 August 1978
... liquid or gas pressures. Its many uses in- clude bearings, fittings and valves. *BUNTING is a registered Composition: copper* Tm Lead zinc Iron Antilnony Nickel* trademark of NL Industries, Inc. Nominal 88 10 z Range 86.0-89.0 9.&l 1.0 0.30 max. l&3.0 0.20 max. 0.20 max. 1.0 max. 0.05 max. Physical...
Journal Articles
Alloy Digest (1978) 27 (9): CS-74.
Published: 01 September 1978
... UNIFLUX 70 is a continuous flux-cored welding electrode (wire) for welding in carbon dioxide shielding gas in the flat groove and horizontal fillet positions. It is used widely in shipbuilding and other fabricating industries to weld carbon steel and provides around 82,000 psi tensile strength and...
Journal Articles
Alloy Digest (1979) 28 (2): Cu-367.
Published: 01 February 1979
..., steam castings, bushings, nuts, bearings, gears and piston rings. Also castings subject to gas or liquid pressures as in pumps, valves and fittings. Manufacturer: NL Bearings/NL Industries, Inc. Toledo, Ohio 43601. ...
Journal Articles
Alloy Digest (1979) 28 (7): SA-362.
Published: 01 July 1979
... UNIFLUX 90 is a continuous flux-cored welding electrode (wire) for welding in carbon dioxide shielding gas in the flat groove and horizontal fillet positions. It was developed to weld high-strength low-alloy steels, but it can be used successfully to weld other low-alloy steels and carbon steels...
Journal Articles
Alloy Digest (1980) 29 (6): Ti-77.
Published: 01 June 1980
... Division, Colt Industries Copyright © ASM International® 1996 1996 ASM International air-frame forgings bend strength chemical composition corrosion-resistant alloys creep properties CRUCIBLE C-120AV elasticity fatigue properties fracture toughness gas-turbine compressors heat...
Journal Articles
Alloy Digest (1985) 34 (7): Ni-317.
Published: 01 July 1985
... temperatures. It can be hot upset, forged, deep drawn, impact extruded and welded. Applications include highly corrosive environments in agrichemical, petrochemical, pulp and paper, oil and gas, marine and other chemical process industries. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1975) 24 (4): SS-309.
Published: 01 April 1975
... Steel Division, Colt Industries. Producer or Source: Crucible Stainless Steel Division, Colt Industries Copyright © ASM International® 1996 1996 ASM International automotive emission control systems chemical composition corrosion-resistant alloys CRUTEMP 25 elasticity gas turbines...
Journal Articles
Alloy Digest (1976) 25 (6): Ni-229.
Published: 01 June 1976
... NIMAG 133 is a wrought form of commercially pure nickel. It has good mechanical properties and excellent resistance to many corrosive environments. It has useful magnetic and magnetostrictive properties, high electrical and thermal conductivities, low gas content and low vapor pressure. Among its...
Journal Articles
Alloy Digest (1967) 16 (11): Co-54.
Published: 01 November 1967
... MAR-M Alloy 509 is a vacuum melted, cobalt-base alloy having high strength, low creep rates, and resistance to oxidation and thermal shock. It is recommended for aircraft and industrial gas turbine applications. This datasheet provides information on composition, physical properties, hardness, and...
Journal Articles
Alloy Digest (2002) 51 (6): SS-786.
Published: 01 June 2002
... 304, 316, and 317L stainless steels. Its many uses include marine scrubbers, desalination equipment, sulfuric acid production, wet phosphoric acid production, mild sour gas wells, urea production, and applications in the pulp and paper industry. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1994) 43 (8): SS-571.
Published: 01 August 1994
... SUMITOMO DP8 is a duplex stainless steel. Duplex stainless steels are designed to be economical and reliable for material applications in the production of oil and gas to resist the environments there of carbon dioxide, hydrogen sulfide and chlorides. This family of alloys is also resistant to...
Journal Articles
Alloy Digest (1995) 44 (5): Co-97.
Published: 01 May 1995
... BIODUR CCM PLUS ALLOY is a high carbon version of BioDur Carpenter CCM Alloy (Alloy Digest Co-96, March 1995), produced by vacuum induction melting, followed by inert gas atomization and hot isostatic pressure. Applications are in the orthopedic industry. This datasheet provides information on...