1-20 of 57 Search Results for

fuse clips

Sort by
Journal Articles
Alloy Digest (2018) 67 (11): cu-881.
Published: 01 November 2018
... Alloy CuSn3Zn9 (UNS C42500) is a bronze alloy. Typical uses include electrical devices, switching elements, connectors and terminals, fuse clips, pen clips, and weather stripping. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend...
Journal Articles
Alloy Digest (1968) 17 (11): Cu-193.
Published: 01 November 1968
... BRIMCO Bronze is a copper-tin-zinc alloy recommended as a substitute for phosphor bronze for cost saving in fuse clips, springs and electrical components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1999) 48 (8): Cu-638.
Published: 01 August 1999
... WRM alloy 5058 is a phosphor-bronze alloy with a good combination of electrical conductivity, tensile strength, and stress-relaxation resistance. Typical applications include lead frames, contact springs, and fuse clips. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1979) 28 (12): Cu-385.
Published: 01 December 1979
... ANACONDA Alloy (E) 505 is a low-tin phosphor bronze with excellent resistance to corrosion, excellent ductility and good resistance to fatigue. It has good thermal and electrical conductivity. Its uses include flexible metal hose, electrical contacts, fuse clips and fasteners. This datasheet...
Journal Articles
Alloy Digest (1980) 29 (5): Cu-394.
Published: 01 May 1980
... by high elastic and fatigue strengths, excellent resistance to wear and high resistance to general corrosion. Its many uses include springs, fuse clips, switch parts, pump parts and welding equipment. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1981) 30 (5): Cu-417.
Published: 01 May 1981
...-relaxation characteristics, good bend performance and excellent corrosion resistance. Among its typical uses are electrical connectors, fuse clips and relay springs. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also...
Journal Articles
Alloy Digest (1984) 33 (8): Cu-482.
Published: 01 August 1984
... Copper Alloy No. C42200 is brass with an addition of tin (nominally 1.1%). It can be machined, formed and joined successfully. It has good resistance to corrosion. Typical uses include terminals, fuse clips, contact springs and electrical connectors. This datasheet provides information...
Journal Articles
Alloy Digest (1984) 33 (10): Cu-485.
Published: 01 October 1984
... lines, cable wrap, eyelets, flexible hose and fuse clips. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu...
Journal Articles
Alloy Digest (1988) 37 (8): Cu-539.
Published: 01 August 1988
... UNS C42500 is a copper-zinc-tin alloy suitable for electrical switches and springs, fuse and pen clips, and weather stripping. It can be cold worked readily by conventional processes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1963) 12 (12): Cu-136.
Published: 01 December 1963
... Characteristics: Riverside No. 105 is of outstanding importance because of its relatively high electrical con- ductivity. Cold rolled to good spring strengths, in strip form, it is particularly adaptable co fuse clips, movable and fixed contacts, and for similar parts of electrical equipment. It is highly...
Journal Articles
Alloy Digest (1971) 20 (1): Cu-225.
Published: 01 January 1971
...: Electrical contacts, springs, fuse clips, heat exchangers, condensers, sash chain. .41loy 300: Electrical contacts. springs. retention devices, heat exchangers, fuse clips, switch and relay components. Manufacturer: Bridgeport Rolling Mills Company Bridgeport, Connecticut 06601 ...
Journal Articles
Alloy Digest (1983) 32 (9): Cu-463.
Published: 01 September 1983
... Copper Alloy No. C43000 is a copper-zinc-tin alloy of moderate strength and ductility. It can be hot worked readily. It has excellent cold-working characteristics and can be fabricated by the conventional cold-working processes. It is used for fuse and pen clips, weather stripping, electrical...
Journal Articles
Alloy Digest (1974) 23 (6): Cu-280.
Published: 01 June 1974
... COPPER Alloy No. 425 is a copper-zinc-tin alloy suitable for electrical switches and springs, fuse and pen clips, and weather stripping. It can be cold worked readily by convectional processes. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1990) 39 (10): Cu-555.
Published: 01 October 1990
... wire (drawn), rolled or drawn bar, sheet, plate, rod, wire and tube. Applications: Cunentandsignalcarryingsprings,leadfrarnes,mechanical springs, diaphragms, switch blades, contacts, connectors, terminals, fuse clips, bellows, die casting plunger tips, sleevebearings,toolingtomoldplastics...
Journal Articles
Alloy Digest (2004) 53 (9): Cu-723.
Published: 01 September 2004
..., connectors, fuse clips, pen clips, and weather strip- ping. Producer: Wieland Metals, Inc. Wheeling, IL 60090 (847) 537-3990 (847) 537-4085 (fax) In Germany: Wieland-Werke AG D-89070 Ulm Germany +49-0731-944-0 +49-0731-944-2772 (fax) e-mail: info@wieland.de www.wieland.com ISSN: 002-614X Cu-723B Fig. 3...
Journal Articles
Alloy Digest (2009) 58 (1): Cu-764.
Published: 01 January 2009
... (H00 through H10). Applications: Typical applications are electrical contacts, springs, and switches. Terminals, connectors, fuse clips, pen clips, weatherstrip, and thermostat element cups are additional uses. Producer: Luvata Sales, (USA), Inc. Bloomingdale, IL 60108 Tel: 630-980-8400 Fax: 630-980...
Journal Articles
Alloy Digest (1999) 48 (10): Cu-634.
Published: 01 October 1999
...: flexible hose, eyelets, circuit breaker components, fuse clips, welded condenser tubes, terminals, lead frames, connec- tors, and contact springs. Forms Available: Alloy C19400 is available in sheet and strip form. For most al- loys and tempers, the gage range is from 0.003 to 0.165 in. Widths produced...
Journal Articles
Alloy Digest (2010) 59 (6): Cu-783.
Published: 01 June 2010
... contacts, switches, connectors, chemical hardware, textile machinery plants, fuse clips, lock washers, sleeve bushing, perforated sheets, friction springs, wear guides, sprinklers. Producer: Luvata Sales, (USA), Inc. Bloomingdale, IL 60108 Tel: 630-980-8400 Fax: 630-980-8891 www.luvata.com ISSN: 002-614X...
Journal Articles
Alloy Digest (1966) 15 (1): Cu-160.
Published: 01 January 1966
..., springs, fuse clips, fasteners, wiring device components. Manufacturer: Bridgeport Rolling Mills Cornpan) Bridgeport, Connecricuc ...
Journal Articles
Alloy Digest (2018) 67 (5): Cu-871.
Published: 01 May 2018
... Applications Typical uses: Architectural: bridge bearing plates Hardware: beater bars, bellows, Bourdon tubing, clutch disks, cotter pins, diaphragms, fuse clips, fasteners, lock washers, sleeve bushing, springs, switch parts, truss wire, wire brushes Industrial: chemical hardware, perforated sheets...