Alloy Digest (1992) 41 (1): Cer-9.
Published: 01 January 1992
..., AN-291 (Alumina [alundum] kiln furniture) Statistical process control production of these materials assures high quality, high consistency products. Chemical Characterization: The seven material types listed above are alumina (alundum) ceramics bonded with mullite (3AJO,*SiO,) PROPERTIES Table 1...
Journal Articles
Alloy Digest (1992) 41 (4): Cer-11.
Published: 01 April 1992
... ADVANCER NITRIDE BONDED SILICON CARBIDE has exceptional high-temperature strength. Its oxidation resistance assures long life. It is a low-mass ceramic that is ideally suited to kiln furniture. This datasheet provides information on composition, physical properties, elasticity, and shear strength...
Journal Articles
Alloy Digest (1977) 26 (4): Cu-331.
Published: 01 April 1977
... Copper Alloy No. 976 is a cast leaded nickel bronze containing 20% nickel; it is known as Nickel Silver (20% Nickel) and its trade name is Dairy Bronze. It has a pleasing silvery color and high resistance to corrosion by milk and many other materials. Among its many uses are furniture and ship...
Journal Articles
Alloy Digest (1980) 29 (10): Cu-405.
Published: 01 October 1980
... of light-duty applications such as andirons, furniture hardware, valves and ship trimmings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength. It also includes information on corrosion resistance as well as casting...
Journal Articles
Alloy Digest (2019) 68 (1): SA-835.
Published: 01 January 2019
..., MHZ steels by the producer have proven their value, among other factors, in the automotive industry in body-in- white components, particularly for crash-relevant structural parts such as members and pillars, as well as in industrial applications such as furniture hardware and window fittings. The high...
Journal Articles
Alloy Digest (2019) 68 (2): SA-837.
Published: 01 February 2019
..., MHZ steels by the producer have proven their value, among other things, in the automotive industry in body-in- white components, particularly for crash-relevant structural parts such as members and pillars, as well as in industrial applications such as furniture hardware and window fittings. The high...
Journal Articles
Alloy Digest (2018) 67 (11): sa-828.
Published: 01 November 2018
... such as furniture hardware and window fittings. The high strength properties result from precipitation hardening, thanks to finely-dispersed carbonitrides and a fine-grained microstructure. Even very small amounts of the elements titanium and/or niobium in the region of 0.01% result in a significant increase...
Journal Articles
Alloy Digest (2018) 67 (12): sa-831.
Published: 01 December 2018
... applications such as furniture hardware and window fittings. The high strength properties result from precipitation hardening thanks to finely-dispersed carbonitrides and a fine-grained microstructure. Even very small amounts of the elements titanium and/or niobium in the region of 0.01% result...
Journal Articles
Alloy Digest (1991) 40 (3): P-24.
Published: 01 March 1991
... or from parts stored in a seated container. Applications: Tote bins, chip carriers, PC board racks, conveyor parts, hospital equipment, ordnance handling and computer room furniture. Producer: Akzo Engineering Plastics, Inc. P.O. Box 3333 Evansville, Indiana 47732. ...
Journal Articles
Alloy Digest (1962) 11 (1): Al-110.
Published: 01 January 1962
... mold, shell, plaster investment. Also ingots. ornamental grilles, brackets, ball joints, valve handles, furniture parts, clamps. Manufacturer: Federated Metals Division American Smelting & Refining Co. New York 5, New York ...
Journal Articles
Alloy Digest (1963) 12 (8): Al-128.
Published: 01 August 1963
..., street light standards, brackets, road vehicle structural members, appli- ance [rim, pipes, portable bridges, window frames, tubular furniture, aircraft hangar doors, ladders, scaffold cubing, ski poles. Manufacturer: Aluminum Company of Canada, Ltd. Man [real, Canada .Aluminium Ltd. Sales, Inc...
Journal Articles
Alloy Digest (2003) 52 (11): Al-386.
Published: 01 November 2003
....) The alloy is available in the T651 and T8 tempers. Applications: Applications include heavy-duty structures requiring good corro- sion resistance, marine applications, truck parts, railroad cars, furniture, and pipelines. Producer: Tennalum A Division of Kaiser Aluminum Jackson, TX 38301 (800) USE-2011 (731...
Journal Articles
Alloy Digest (1999) 48 (6): SS-749.
Published: 01 June 1999
... of ductility. Products Available: This alloy is available in ingots, slabs, hot bands, sheet, and strip. Typical Applications: J&L 405 is used in burial caskets, plumbing hardware, appliance components, furniture trim, fins for heater tubes, transformer and capacitor cases, dry fertilizer spreaders, exhaust...
Journal Articles
Alloy Digest (2018) 67 (3): SS-1282.
Published: 01 March 2018
... Ferrotherm 4828 is a standard steel grade used for the fabrication of furnace furniture and other high temperature components. Compared with Ferrotherm 4878 and 4713, Ferrotherm 4828 exhibits superior resistance to scaling. Due to its high tensile strength at elevated temperatures, compared with other grades...
Journal Articles
Alloy Digest (1957) 6 (1): Mg-30.
Published: 01 January 1957
... and hollow shapes. Appllcatlons: Light alloy parts, truck bodie3, d0Ck boards, typewriter platens, framing for a&raft cowling and windows, in- terior paneling, furniture, flooring, oil tanks, instru- ment housings, structural members. Manufacturer: Whitelight Magnesium Division White Metal Rolling...
Journal Articles
Alloy Digest (1990) 39 (4): Al-303.
Published: 01 April 1990
... forming of 6061 alloy are given in Table 3. Heavy-duty structmes requiring good corrosion resistance, truck and marine, railroad cars, furniture, pipelines. Producers: Aluminum alloy mills. ...
Journal Articles
Alloy Digest (2022) 71 (5): Al-487.
Published: 01 May 2022
... Forms Sand castings; gravity die castings; high pressure die castings. Applications Electrical conductors; food industry; mechanical engineering; optics/furniture; chemical industry. Supplier Aluminium Rheinfelden Alloys GmbH Bukheinstrasse 2 79618 Rheinfelden, Germany Tel: +49 7623 93375 Web...
Journal Articles
Alloy Digest (1991) 40 (10): Al-320.
Published: 01 October 1991
... by all commonly used welding methods or by brazing. Forms Available: Joining: AA 6063 has good weldability (gas, arc and resistance methods) and brazeability. Drawn or extruded tube, pipe, extruded wire, rod, bar and shapes. Applications: Corrosion Resistance: Ripe railing, furniture, architectural...
Journal Articles
Alloy Digest (2022) 71 (7): Al-488.
Published: 01 July 2022
... for ratings of corrosion resistance and fabrication characteristics. Product Forms Flat products; angles; channels; hollow circular and square sections. Applications The ready extrudability of Atlas 6063 enables thin walled and intricate hollow shapes to be produced. Typical applications include furniture...
Journal Articles
Alloy Digest (2002) 51 (8): Al-380.
Published: 01 August 2002
... to 6061 and 6013 to 6013. In the recreation industry 4043 is used in bicycle and sport wheel chairs for strength, fatigue resistance, and anodizing welding 6013 to 6013, and also in lawn furniture for weld cosmetics and strength welding 6063 to 6063. The alloy is used in containers for chem- ical storage...