Alloy Digest (1997) 46 (11): Ni-530.
Published: 01 November 1997
... UCI-371 is a furnace tube alloy that can provide either a higher operating temperature with better furnace yield or a longer life than either HK 40 or HP-steel alloys. This alloy, with higher nickel content than the two noted above, permits higher concentrations of both chromium and silicon, which...
Journal Articles
Alloy Digest (2001) 50 (3): Ni-562.
Published: 01 March 2001
... UCI-471 is an improved version of the HP classification of furnace tube alloys with better oxidation and creep resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes information on high temperature...
Journal Articles
Alloy Digest (2001) 50 (5): Ni-566.
Published: 01 May 2001
... UCI-472 is an improved version of the well-known HP classification of furnace-tube alloys with improved carburization and oxidation resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes information...
Journal Articles
Alloy Digest (1977) 26 (11): SS-228.
Published: 01 November 1977
... tubes and refining furnace tubes. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-228...
Journal Articles
Alloy Digest (1997) 46 (9): SS-696.
Published: 01 September 1997
... UCI-270 is a cast, cobalt and tungsten stabilized, nickel-chromium-iron alloy having unequaled performance in high-temperature applications to 2300 F (1260 C). Among its many uses are components for heat-treating furnaces, cement kilns, petrochemical furnace tubes, and refining furnace tubes...
Journal Articles
Alloy Digest (1997) 46 (5): SS-682.
Published: 01 May 1997
... replacement applications for furnace tubing. This datasheet provides information on composition and physical properties as well as creep. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-682. Producer or source: Ultra-Cast Inc...
Journal Articles
Alloy Digest (1992) 41 (6): SS-530.
Published: 01 June 1992
... SANDVIK SANICRO 31HT is an austenitic iron-nickel-chromium alloy characterized by very good resistance to oxidation with good mechanical properties at elevated temperatures. It is recommended for resistance element sheathing, pyrometer tubes, airheaters, equipment for heat treating, furnace tubes...
Journal Articles
Alloy Digest (1965) 14 (9): SS-172.
Published: 01 September 1965
... SANDVIK SANICRO 31 is an iron-nickel-chromium alloy having good resistance to corrosion and oxidation and good mechanical properties at elevated temperatures. It is recommended for electrical sheathing, pyrometer tubes, equipment for heat treating and furnace tubes and other equipment...
Journal Articles
Alloy Digest (1996) 45 (9): SS-654.
Published: 01 September 1996
... Wiscalloy 25-35Nb is a high-temperature cast heat-resistant stainless steel with good creep-rupture properties. The alloy is centrifugally cast and is often used as petrochemical furnace tubing. This datasheet provides information on composition, physical properties, and tensile properties as well...
Journal Articles
Alloy Digest (1996) 45 (11): SS-656.
Published: 01 November 1996
... Wiscalloy 25-35NB MA is a high-temperature cast heat-resistant microalloyed stainless steel with good creep-rupture properties. The alloy is centrifugally cast and is often used as petrochemical furnace tubing. This datasheet provides information on composition, physical properties, and tensile...
Journal Articles
Alloy Digest (1993) 42 (6): SS-545.
Published: 01 June 1993
... Märker G4848 is a cast austenitic stainless steel for use up to 1050 C (1922 F). Typical uses include petrochemical ethylene furnace tubes and steam metal reformers. This datasheet provides information on composition and physical properties. It also includes information on casting and joining...
Journal Articles
Alloy Digest (1996) 45 (5): Ni-512.
Published: 01 May 1996
... Märker G 4857W is a cast alloy for petrochemical applications such as furnace tubes. It compares favorably to the HP Modified grades. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on joining. Filing Code: Ni-512...
Journal Articles
Alloy Digest (2001) 50 (1): SS-812.
Published: 01 January 2001
... Sandvik 7RE10 is a 25Cr/20Ni oxidation-resistant alloy with good carburization and oxidation resistance. It is typically used as furnace tubing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (1999) 48 (8): SS-755.
Published: 01 August 1999
... KHR35C Hi Si is similar to Kubota alloy KHR35C but with added silicon levels to improve carburization resistance. The typical application is ethylene furnace tubing. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (1999) 48 (12): SS-770.
Published: 01 December 1999
... UCI-198 is best described as an HP alloy modified with niobium and with microalloying by titanium and rare-earth elements. The alloy was developed to produce increased creep resistance in furnace tube applications. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1986) 35 (8): SS-473.
Published: 01 August 1986
... INCOLOY Alloy DS is a wrought, austenitic nickel-chromium-iron alloy with high resistance to heat and oxidation. Its many applications include furnace parts, woven-wire conveyor belts for continuous furnaces, radiant heat tubes and gas-turbine components. This datasheet provides information...
Journal Articles
Alloy Digest (1995) 44 (3): SS-586.
Published: 01 March 1995
... PARALLOY CR39W is an austenitic heat resisting alloy with a combination of creep strength, carburization resistance and ductility. The alloy can be cast for fittings and centrifugally cast for tubing. Typical applications are within the petrochemical furnace arena. This datasheet provides...
Journal Articles
Alloy Digest (1996) 45 (2): SS-635.
Published: 01 February 1996
... Märker G-4857M is a 25Cr-37Ni-Mo alloy with good creep rupture strength and good resistance to carburization. and oxidation. The alloy is used as tubes and castings for reformer and pyrolysis furnaces. It can be used to 1100 deg C (2000 deg F) in air or combustion gases. This datasheet provides...
Journal Articles
Alloy Digest (1996) 45 (3): SS-634.
Published: 01 March 1996
... 1996 1996 ASM International chemical composition creep properties elasticity furnace components joinability oxidation resistance physical properties RA 353 MA alloy radiant tubes thermal properties UNS S35315 - DIGEST - DATA ON WORLD WIDE METALS AND ALLOYS Put&hedby:ASh4lntemati0...
Journal Articles
Alloy Digest (1978) 27 (12): Bi-10.
Published: 01 December 1978
...-shrinking patterns, proof-casting, sealing heat-treating furnaces and bending large tubes (diameter greater than 13/4 inches). This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, and machining...