Alloy Digest (1986) 35 (8): SS-473.
Published: 01 August 1986
... INCOLOY Alloy DS is a wrought, austenitic nickel-chromium-iron alloy with high resistance to heat and oxidation. Its many applications include furnace parts, woven-wire conveyor belts for continuous furnaces, radiant heat tubes and gas-turbine components. This datasheet provides information...
Journal Articles
Alloy Digest (2002) 51 (5): SS-853.
Published: 01 May 2002
... and improves weldability. Typical uses include furnace parts, heating elements, aircraft and jet engine parts, heat exchangers, carburizing-annealing boxes, sulfite liquor handling equipment, kiln liners, boiler baffles, refinery and chemical processing equipment, and auto exhaust parts. This datasheet...
Journal Articles
Alloy Digest (1998) 47 (9): SS-729.
Published: 01 September 1998
... and 816 C (800 and 1500 F). This grade is nonmagnetic in the annealed condition but is slightly magnetic when cold worked. Among its many applications are aircraft engine exhaust manifolds, furnace parts, and fasteners. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1969) 18 (2): SS-221.
Published: 01 February 1969
... Type HH is an iron-chromium-nickel casting alloy having high heat, oxidation and corrosion resistance. It is recommended for furnace parts, salt pots, grate bars, belt conveyors and other parts operating up to 21008 F in intermittent service. It may be supplied in partially ferritic Type I...
Journal Articles
Alloy Digest (1983) 32 (5): SS-426.
Published: 01 May 1983
... worked. Among its many applications are aircraft-engine exhaust manifolds, furnace parts and expansion joints. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information...
Journal Articles
Alloy Digest (2006) 55 (11): SS-980.
Published: 01 November 2006
... Kubota alloy HH II is a heat-resistant fully austenitic stainless steel casting for multiple furnace parts. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance...
Journal Articles
Alloy Digest (1958) 7 (1): SS-67.
Published: 01 January 1958
... NIMONIC DS is a wrought, austenitic nickel-chromium-iron alloy having high oxidation and heat resistance. It is recommended for furnace parts and gas turbine components. This datasheet provides information on composition, physical properties, and elasticity as well as creep. It also includes...
Journal Articles
Alloy Digest (1968) 17 (2): SS-205.
Published: 01 February 1968
... COPPER Alloy 31 is an iron-chromium-molybdenum casting alloy having good resistance to oxidation at temperatures up to about 1200 F. It is recommended for furnace parts and oil refinery equipment. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1969) 18 (8): SS-229.
Published: 01 August 1969
... Firth Vickers F.I. 20 is a non-hardenable, ferritic high-chromium steel recommended for furnace parts, heat treating equipment, zinc die casting machine nozzles and other high temperature applications up to approximately 750 C. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1984) 33 (3): SS-441.
Published: 01 March 1984
... and structures can be fabricated easily and it can be machined readily. It can be welded easily and gives strong, ductile welds. Some of its many applications are annealing boxes, boiler baffles, dryers, furnace parts, heat exchangers and oil-refining equipment. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2010) 59 (12): Ni-684.
Published: 01 December 2010
... in various parts for heat treatment furnaces, diesel vehicle glow plugs and the like. Product Forms Available: Plate, sheet and strip forms, coil is available. Applications: Muffle furnaces, baskets and other furnace parts, industrial heat treatment furnace parts, special glass melting, furnace parts...
Journal Articles
Alloy Digest (1965) 14 (6): TS-165.
Published: 01 June 1965
... HALGRAPH is an electric furnace melted, oil hardening, graphitic tool steel with excellent non-deforming properties. It is free-machining and has a high resistance to wear. It is non-deforming type steel suitable for use as tools, dies, gauges and parts requiring maximum hardness and freedom from...
Journal Articles
Alloy Digest (2019) 68 (3): SS-1304.
Published: 01 March 2019
... Manaurite 900 is a high-temperature casting alloy developed for parts outside the direct furnace. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: SS-1304. Producer or source: Manoir Industries, Manoir Pîtres. Producer or Source...
Journal Articles
Alloy Digest (1956) 5 (5): SA-42.
Published: 01 May 1956
... HY-TEN M is a triple alloy electric furnace steel recommended for parts requiring great hardness, density of structure, resistance to wear, and high strength combined with toughness. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (1968) 17 (11): Fe-36.
Published: 01 November 1968
... Silicon Core Iron is a low carbon silicon electric furnace melted iron recommended for direct current and alternating current magnetic applications in solenoids, armatures and other flux carrying parts operating at high saturations. It is furnished in five grades: A, A-FM, B, B-FM, and C...
Journal Articles
Alloy Digest (1982) 31 (1): Bi-27.
Published: 01 January 1982
... characteristics make it of great use in industry for such applications as sprinkler and fire safety devices, support for bending pipe and tubing, anchoring aircraft parts for machining, and seals for annealing and nitriding furnaces. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1982) 31 (11): Sn-12.
Published: 01 November 1982
..., it can be recovered readily an recycled into new uses any number of times. Among its many uses are fusible mandrels for electroforming, low-temperature solder, holding parts for machining, dies for a wax patterns for investments casting and liquid scals for furnaces. This datasheet provides information...
Journal Articles
Alloy Digest (1983) 32 (10): Bi-32.
Published: 01 October 1983
...-shrinkage characteristics make it of great use in industry for such applications as sprinkler and fire safety devices, support for bending pipe and tubing, anchoring aircraft parts for machining, and seals for annealing and nitriding furnaces. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1985) 34 (7): TS-444.
Published: 01 July 1985
... CARPENTER BARTO is a cold-melt, grain-controlled, electric-furnace chromium-nickel tool steel. It was developed for applications requiring extreme toughness. Barto's extreme toughness is developed at the expense of some wear resistance; however, it will harden to Rockwell C 55/56. Typical...
Journal Articles
Alloy Digest (2012) 61 (10): SS-1127.
Published: 01 October 2012
... environments where resistance to thermal cycling, oxidation, and carburization is required while maintaining strength. Applications include furnace containers for annealing fixtures, furnace parts, heat treating baskets, furnace fans, and petrochemical furnace parts. Producer: Electralloy, a G.O Carlson, Inc...