Published: 01 March 1992
... ULTEM 4001 is an unreinforced polyetherimide resin with an internal lubricant. It is wear resistant and it has a reduced coefficient of friction. See also ULTEM 4000 (Alloy Digest CP-21, March 1992) for reinforced resin properties. ULTEM 4001 is available in opaque colors only. This datasheet...
Journal Articles
Alloy Digest (1992) 41 (3): Cp-21.
Published: 01 March 1992
... ULTEM 4000 is a reinforced polyetherimide resin with an internal lubricant. It is wear resistant and has a reduced coefficient of friction. See also ULTEM 4001 for unreinforced resin properties (Filing code P-33, 3/92). This datasheet provides information on physical properties, hardness, tensile...
Journal Articles
Alloy Digest (2003) 52 (10): Al-385.
Published: 01 October 2003
... Kaiser Aluminum alloy 4026 has high strength and good wear resistance, as well as galling resistance. It was developed for sliding friction resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1956) 5 (7): Sn-2.
Published: 01 July 1956
... FEDRATED NO. 3 is a tin-base bearing alloy recommended for moderate to high speeds and loads. It has low frictional resistance, low wear, good running-in properties, good emergency behavior upon failing of lubrication, and lower coefficient of expension than the lead-base alloys. This datasheet...
Journal Articles
Alloy Digest (2022) 71 (2): Cu-929.
Published: 01 February 2022
... formability, high strength and good corrosion resistance, which makes it ideal for use as springs. It also has a low coefficient of friction against steel. This makes it a popular choice for wear resistant guide strips and similar bearing applications involving boundary lubrication conditions. The alloy has...
Journal Articles
Alloy Digest (2013) 62 (6): Cu-819.
Published: 01 June 2013
... ToughMet 2 CX is a Cu-9Ni-6Sn alloy that combines low coefficient of friction with wear resistance. ToughMet alloys are a line of spinodal hardened Cu-Ni antigalling alloys for bearings capable of performing with a variety of shafting materials and lubricants. The alloys combine a high lubricity...
Journal Articles
Alloy Digest (1976) 25 (4): Zn-27.
Published: 01 April 1976
... MICROZINC Alloy 100 is a zinc-lead-cadmium alloy having good ductility with adequate strength, good resistance to corrosion, and a low coefficient of sliding friction. It is solderable and non-magnetic. Processing differences give three commercial products or classes designated= 101, 102 and 103...
Journal Articles
Alloy Digest (1976) 25 (6): Mo-12.
Published: 01 June 1976
... METCO 505 is a high-molybdenum powder designed to produce plasma flame spray coatings for use as hard bearing surfaces with low coefficient of friction and for resisting wear by abrasive grains or hard surfaces. Its coatings have excellent non-scuffing properties and are compatible with many...
Journal Articles
Alloy Digest (1976) 25 (11): Zn-29.
Published: 01 November 1976
... MICROZINC Alloy 190 is a zinc-copper alloy with good atmospheric corrosion resistance and a low coefficient of sliding friction to eliminate galling in service. It has maximum strength commensurate with good ductility and drawability. Processing differences give two commercial products or classes...
Journal Articles
Alloy Digest (1977) 26 (10): Al-229.
Published: 01 October 1977
... anti-scuffing properties, low friction and high resistance to wear under conditions of boundary and thin-film lubrication, it is used extensively for large rolling mill bearings. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fatigue...
Journal Articles
Alloy Digest (1979) 28 (5): Cu-373.
Published: 01 May 1979
... BUNTING Alloy 937 is a cast bushing and bearing bronze. It is one of the most satisfactory materials to use where shaft alignments or shaft wear is a problem. It has a good load capacity and excellent anti-friction characteristics. Its many uses include pressure-tight castings, corrosion-resistant...
Journal Articles
Alloy Digest (1979) 28 (7): Cu-377.
Published: 01 July 1979
... friction and resists wear. Among its many applications are chemical hardware, bearings and springs. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating...
Journal Articles
Alloy Digest (1982) 31 (9): Al-240.
Published: 01 September 1982
...-scuffing characteristics, low friction and high resistance to wear under conditions of boundary and thin-film lubrication. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information...
Journal Articles
Alloy Digest (1970) 19 (9): Al-199.
Published: 01 September 1970
... ALUMINUM 392.0 is a hypereutectic aluminum-silicon alloy developed for die castings which require high resistance to wear and abrasion. Applications include variable speed pulleys, automotive clutch friction rings, cylinder liners, sheaves, and brake drums. This datasheet provides information...
Journal Articles
Alloy Digest (1970) 19 (12): Cu-223.
Published: 01 December 1970
... CDA ALLOY 544 is a leaded phosphor bronze with good resistance to corrosion and good machinability. It has strength equivalent to mild steel, good bearing and friction characteristics, good electrical conductivity, and is nonmagnetic. It is used for bearings, cams, gears, valves, meter and camera...
Journal Articles
Alloy Digest (1965) 14 (3): Cu-149.
Published: 01 March 1965
... Revere Alloy 411 is a bearing bronze alloy having good formability, low coefficient of friction, corrosion resistance, and freedom from stress-cracking. (It was formerly known as Revere No. 325.) This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1998) 47 (9): Ni-545.
Published: 01 September 1998
... Colmonoy 98 is a nickel-base alloy with high corrosion resistance, particularly to sodium hydroxide, salt water, and sulfuric acid. It also has a low coefficient to friction to reduce metal-to-metal adhesive wear loss. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1973) 22 (4): Sn-3.
Published: 01 April 1973
... Tin Babbit comprises a family of essentially tin-antimony-copper alloys used to minimize friction in moving parts of machines. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness...
Journal Articles
Alloy Digest (1973) 22 (7): Pb-10.
Published: 01 July 1973
.... Producer or Source: White metal bearing alloy producers Copyright © ASM International® 1996 1996 ASM International castability chemical composition compressive strength corrosion-resistant alloys elasticity fatigue strength friction hardness heat treatability lead alloys lead babbit...
Journal Articles
Alloy Digest (1973) 22 (8): Cu-269.
Published: 01 August 1973
... BUNTING Alloy 72 is a cast bushing and bearing bronze with excellent load capacity and anti-friction qualities. It is used in a wide variety of industrial and automotive equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...