Alloy Digest (1963) 12 (3): Al-123.
Published: 01 March 1963
... NORAL 162 is an age-hardenable aluminum casting alloy. It has low thermal expansion, good high temperature strength and bearing (frictional) properties. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive, shear...
Journal Articles
Alloy Digest (1956) 5 (8): Pb-3.
Published: 01 August 1956
... FEDERATED No. 8 is a lead-base bearing alloy recommended for moderate to high speeds and moderate loads. It has very good frictional properties, reasonably good corrosion resistance and low price. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (1973) 22 (4): Sn-3.
Published: 01 April 1973
... Tin Babbit comprises a family of essentially tin-antimony-copper alloys used to minimize friction in moving parts of machines. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness...
Journal Articles
Alloy Digest (1970) 19 (12): Cu-223.
Published: 01 December 1970
.... Producer or source: Anaconda American Brass Company. Producer or Source: Anaconda American Brass Company Copyright © ASM International® 1996 1996 ASM International bearing strength chemical composition corrosion-resistant alloys elasticity fracture toughness friction properties hardness...
Journal Articles
Alloy Digest (1973) 22 (7): Pb-10.
Published: 01 July 1973
... Lead Babbit comprises a family of alloys used to cut down on friction in moving parts of machines. Alloys 7, 8 and 13 are essentially lead-antimony-tin alloys. Alloy 15 is an arsenical (about 1% arsenic) lead-base alloy. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1998) 47 (9): Ni-545.
Published: 01 September 1998
... Colmonoy 98 is a nickel-base alloy with high corrosion resistance, particularly to sodium hydroxide, salt water, and sulfuric acid. It also has a low coefficient to friction to reduce metal-to-metal adhesive wear loss. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1976) 25 (12): Cu-324.
Published: 01 December 1976
..., psi Coefficient of friction - dry 0.324 93 11 x 10-6 11 x 10-6 8.7 x 10-6 23.4 10.4 10-12 x 106 33 x 106 0.14 PROPERTIES Table 1 ROOM-TEMPERATURE MECHANICAL PROPERTIES - Castings Tensile Properties Tensile strength, psi 24000 Yield strength (0.2% permanent set), psi 14000 Elongation (2 in % 12...
Journal Articles
Alloy Digest (1972) 21 (9): Cu-258.
Published: 01 September 1972
... possessing unusually good frictional properties. It will not, even under extreme conditions, melt like a babbit or freeze on the shaft like a bronze. Microexamination shows that the lead is in fine, globular form and uniformly distributed. Also, there is no lead between the copper-tin grain boundaries...
Journal Articles
Alloy Digest (1958) 7 (7): Pb-5.
Published: 01 July 1958
.... This all09 is stronger and more suitable for higher speeds, higher loads, and higher operating temperatures than the lead-antimony alloys. It is cheap, easy to cast, has good frictional properties, and is successfull used for machinery generally where speeds and stresses are moderate. Under more servere...
Journal Articles
Alloy Digest (1956) 5 (8): SS-46.
Published: 01 August 1956
.... and in intermittent service to 1400 deg. F. Enduto FC is a hardenable type of free-machining chrom- ium stainless steel. It has low frictional properties which tend to reduce scratching, galling, or seizing in service. Endure FC is intended for use where machining is of prime importance. It does not provide...
Journal Articles
Alloy Digest (1973) 22 (7): Pb-11.
Published: 01 July 1973
... severe, such as in rolling-mill bearings and other heavy equipment. G Babbit has excellent anti-frictional properties, in keeping with that of the other Lead Babbit alloys. G Babbit is durable and wears remarkably well. It tends to minimize shock loads and deaden noise; it can be provided readily...
Journal Articles
Alloy Digest (2016) 65 (2): Cu-847.
Published: 01 February 2016
... hardness level. These attributes, combined with high anti- friction properties and excellent wear resistance, provide very good bearing properties under high loading. The alloy can be summarized as follows: Excellent mechanical strength Proof strength 90% of UTS Very high wear resistance Good...
Journal Articles
Alloy Digest (1957) 6 (11): Pb-4.
Published: 01 November 1957
... to cast, has good frictional properties, and is successfulIy used for mach- inery generally where speeds and stresses are moderate. Under more severe service conditions, the tin-base babbirts are more frequently used. Casting and cooling conditions affect the microsrruc- ture, fracture, and mechanical...
Journal Articles
Alloy Digest (1965) 14 (6): SS-170.
Published: 01 June 1965
... machine operations. The low frictional properties of the metal minimize scratching and galling in service. Threaded sections work freely without seizing and disassemble easily because of the absence of corrosion in the threads. Project 70 is not usually recommended for vessels containing gases or liquids...
Journal Articles
Alloy Digest (2015) 64 (12): Cu-845.
Published: 01 December 2015
... offers a high hardness level and excellent wear resistance, anti-friction properties, and very good bearing properties, especially under high loading against hardened steels. This alloy is a high copper alloy with small additions of nickel and silicon that COLSIBRO® (Age-Hardened Copper-Nickel-Silicon...
Journal Articles
Alloy Digest (1977) 26 (3): Cu-328.
Published: 01 March 1977
... high hardness and strength. Its low lead content (0.5O%max) gives it relatively low anti-friction properties and makes it somewhat difficult to machine; however, it can be machined successfully with proper care and technique. It can be welded successfully and has generally good resistance to corrosion...
Journal Articles
Alloy Digest (1956) 5 (7): Sn-2.
Published: 01 July 1956
... FEDRATED NO. 3 is a tin-base bearing alloy recommended for moderate to high speeds and loads. It has low frictional resistance, low wear, good running-in properties, good emergency behavior upon failing of lubrication, and lower coefficient of expension than the lead-base alloys. This datasheet...
Journal Articles
Alloy Digest (1957) 6 (7): Al-53.
Published: 01 July 1957
...-scuffing properties, low friction and high wear resistance under conditions of boundary and thin-film lubrication make it particularly suitable. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive and shear strength as well as fatigue...
Journal Articles
Alloy Digest (1976) 25 (6): Mo-12.
Published: 01 June 1976
... METCO 505 is a high-molybdenum powder designed to produce plasma flame spray coatings for use as hard bearing surfaces with low coefficient of friction and for resisting wear by abrasive grains or hard surfaces. Its coatings have excellent non-scuffing properties and are compatible with many...
Journal Articles
Alloy Digest (1977) 26 (10): Al-229.
Published: 01 October 1977
... anti-scuffing properties, low friction and high resistance to wear under conditions of boundary and thin-film lubrication, it is used extensively for large rolling mill bearings. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fatigue...