Alloy Digest (2005) 54 (9): TS-619.
Published: 01 September 2005
... 2005 DRM3 (Cold Forging Die Steel) Daido DRM3 is a high-speed tool steel with both high hardness and toughness for improved life in dies. The alloy has excellent hardenability. Fig. 1 Fatigue strength. DRM3 (65HRC) heated to 1100 °C (2010 °F), tempered twice 560 °C (1040 °F), air cooled. DRM3 (67HRC...
Journal Articles
Alloy Digest (2006) 55 (5): Ti-138.
Published: 01 May 2006
... Timetal 551 is an improved-strength version of Timetal 550 alloy that retains good forging characteristics. The alpha-beta alloy has a nominal composition of Ti-4Al-4Mo-4Sn-0.5 Si, and it is used in gas turbine engine parts. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1958) 7 (7): Al-67.
Published: 01 July 1958
... ALUMINUM 6151, formerly A51S Alloy, is an aluminum forging alloy combining good forgeability, strength, and resistance to corrosion. It responds to an age-hardening heat treatment. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1958) 7 (8): Al-68.
Published: 01 August 1958
... properties workability I 1 Filing Code: Al-68 0 NORAL 38s Aluminum Alloy mmmmw AUGUST 1958 DIGEST -DATA ON WORLD WIDE METALS AND ALLOYS Pdisbad br Engineering AUoys ljigess Inc. Upper Montclair, New Jersey NORAL 38s (Heat Treatable Aluminum Forging Alloy) Noral 3% is a high-silicon aluminum having...
Journal Articles
Alloy Digest (1959) 8 (4): Ni-52.
Published: 01 April 1959
... Unitemp M-252 is a high-strength nickel-base forging alloy recommended for heavy duty jet engine and gas turbine buckets. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep and fatigue. It also includes information...
Journal Articles
Alloy Digest (1960) 9 (1): Mg-44.
Published: 01 January 1960
... MAGNESIUM ALLOY-TA54A is a general purpose hammer-forging alloy having intermediate strength. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information...
Journal Articles
Alloy Digest (2013) 62 (4): Cu-817.
Published: 01 April 2013
... Mueller Alloy C37700 has excellent machining characteristics that make it useful for general forging applications. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, machining...
Journal Articles
Alloy Digest (2013) 62 (5): Cu-818.
Published: 01 May 2013
..., OH 44073-0002, 440-338-5151 [email protected] Fax 440-338-8542 www.asminternational.org Filing Code: Copper May 2013 Cu-818 Mueller Alloy C36500 has excellent machining characteristics. The alloy is often called Leaded Muntz Metal, uninhibited. MUELLER ALLOY C36500 (Forging...
Journal Articles
Alloy Digest (2014) 63 (5): Ti-154.
Published: 01 May 2014
... Timetal Grade 17 is a high-strength deep hardening forging alloy. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness and creep. It also includes information on forming and heat treating. Filing Code: Ti-154. Producer...
Journal Articles
Alloy Digest (2014) 63 (9): SA-708.
Published: 01 September 2014
... MX01 is a steel grade developed to achieve useful properties to minimize the cost of forging dies. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming. Filing Code: SA-708. Producer or source...
Journal Articles
Alloy Digest (1953) 2 (5): Al-7.
Published: 01 May 1953
... HIDUMINIUM RR56 is a heat-treatable aluminium-base alloy recommended for general purpose forgings. It enables production of material which is readily worked in the hot stage and gives high mechanical properties, both for structural use and for use at moderately elevated temperatures...
Journal Articles
Alloy Digest (1955) 4 (4): Al-25.
Published: 01 April 1955
... ALUMINUM 4032, formerly known as Aluminium 32S, is a forging alloy having comparatively low coefficient of expansion and good forgeability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well...
Journal Articles
Alloy Digest (1956) 5 (4): Mg-24.
Published: 01 April 1956
... MELTRON AZ855 is a magnesium forging alloy recommended for large forgings requiring high tensile strength, fatigue endurance and ductility, combined with good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1979) 28 (5): Al-130.
Published: 01 May 1979
... ALUMINUM 2018 is an age-hardenable aluminum forging alloy characterized by relatively high tensile and yield strengths along with fairly good ductility. It has good elevated-temperature properties. Its applications include engine pistons and engine cylinder heads. This datasheet provides...
Journal Articles
Alloy Digest (1978) 27 (8): Al-95.
Published: 01 August 1978
... ALUMINUM 2218 is an aluminum-copper-nickel-magnesium alloy (formerly designated B18S Alloy). It is a standard forging alloy and is recommended for elevated-temperature service. It is used for aircraft and jet engine components. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1980) 29 (10): Cu-404.
Published: 01 October 1980
... MUELLER Alloy 3771 (formerly MBCo. Alloy 211) is one of the most widely used and most easily forged of the copper-base forging alloys. It is most often used in multiple sequence hammer forging operations where a wide forging temperature range is desired. It is also a free-machining alloy. Typical...
Journal Articles
Alloy Digest (1967) 16 (11): Cu-182.
Published: 01 November 1967
... Mueller 3770 (formerly MBCo 200 Alloy) is a free-cutting, leaded brass recommended for forgings of all kinds. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining...
Journal Articles
Alloy Digest (1971) 20 (3): Al-201.
Published: 01 March 1971
... ALUMINUM 7049-T23 is a high-strength alloy having excellent resistance to stress-corrosion cracking. It was developed for use in die and hand forgings. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes...
Journal Articles
Alloy Digest (1971) 20 (11): Cu-245.
Published: 01 November 1971
... COPPER ALLOY No. 774 is a nickel silver press-forging alloy that has a forgeability rating of 85% of that of Forging Brass. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength. It also includes information on corrosion...
Journal Articles
Alloy Digest (1962) 11 (9): Ni-32.
Published: 01 September 1962
... ALLOY M252 is a high-strength nickel-base forging alloy recommended for heavy duty jet engine and gas turbine buckers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on forming...