Journal Articles
Alloy Digest (1984) 33 (11): SS-454.
Published: 01 November 1984
... of hydrocarbons in refinery or petrochemical services, superheater and reheater tubin8g, nuclear reactor steam generators, heat-treating equipment and food processing. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (1975) 24 (10): SS-317.
Published: 01 October 1975
... processing, petroleum refining and food processing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on corrosion resistance as well as forming, heat treating...
Journal Articles
Alloy Digest (1964) 13 (11): Al-141.
Published: 01 November 1964
... Aluminum 214 is a non-heat treatable alloy containing 4% magnesium and characterized by excellent corrosion resistance and excellent weldability. It is recommended for marine applications and food processing equipment. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1966) 15 (5): SS-181.
Published: 01 May 1966
... Illium-PD is an austenitic-ferritic stainless steel casting alloy developed to meet the commercial need for a hardenable, high strength, corrosion resistant alloy free of copper content. It is recommended for equipment for the food processing, chemical, pharmaceutical and platic industry equipment...
Journal Articles
Alloy Digest (2019) 68 (6): Cu-890.
Published: 01 June 2019
..., and relays; in food processing, hospital and medical equipment; and in ferrules. This datasheet provides information on composition and physical properties. Filing Code: Cu-890. Producer or source: Olin Brass. Producer or Source: Olin Brass Copyright ┬ę ASM International┬« 2019 2019 ASM International...
Journal Articles
Alloy Digest (1996) 45 (8): SS-651.
Published: 01 August 1996
... Remainit 4318, similar to type 301LN, is in the family of lowest-alloyed austenitic stainless steels. This type has the highest rate of work hardening. Typical applications include the transportation industry and conveyor belts for food processing. This datasheet provides information...
Journal Articles
Alloy Digest (1982) 31 (2): Al-236.
Published: 01 February 1982
... ALUMINUM 514.0 is a non-heat-treatable alloy containing nominally 4% magnesium. It has relatively low strength and hardness. It is characterized by excellent weldability and excellent resistance to corrosion. Aluminum 514.0 is recommended for food-processing equipment and marine applications...
Journal Articles
Alloy Digest (1982) 31 (7): SS-412.
Published: 01 July 1982
... corrosion resistance is quite good but inferior to lower strength grades produced for corrosion-resistance applications. JS17Cr-4Ni is used widely for critical applications in the aerospace, chemical, food processing and other industries. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1983) 32 (6): Ni-287.
Published: 01 June 1983
.... Its many applications include aircraft/aerospace components, equipment for chemical and food processing and parts for heat-treating equipment. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion...
Journal Articles
Alloy Digest (2002) 51 (10): SS-865.
Published: 01 October 2002
... valuable property is high creep strength at elevated temperatures. The alloy has extensive use in marine exterior trim, chemical- and food-process equipment, pharmaceutical and textile-finishing equipment, and in the pulp and paper industry. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2010) 59 (12): Co-120.
Published: 01 December 2010
..., and instrument parts in medical, chemical, food processing and marine environments. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: CO-120. Producer or source: Hamilton Precision Metals...
Journal Articles
Alloy Digest (1998) 47 (7): SS-723.
Published: 01 July 1998
... is conveyor belts in the food processing industry. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as heat treating. Filing Code: SS-723. Producer or source: Allegheny...
Journal Articles
Alloy Digest (2000) 49 (11): SS-807.
Published: 01 November 2000
... Carpenter Stainless Type 416BQ is a modification of Type 416 to achieve a minimum hardness of 40 HRC when bright hardened, while retaining nearly the machinability of Type 416. Typical applications are cutters in food processing. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1985) 34 (1): Ni-309.
Published: 01 January 1985
... Nickel Alloy 600 is a nickel-base alloy intended for use in a wide range of applications from cryogenic to temperatures above 2000 F, where high-temperature properties and resistance to oxidation or corrosion are desired. This alloy has been used in nuclear, petroleum, chemical, food-processing...
Journal Articles
Alloy Digest (1987) 36 (4): Al-280.
Published: 01 April 1987
... UNS No. A05140 is a casting alloy that cannot be hardened nor strengthened by heat treatment. It has relatively low strength and hardness. It is characterized by excellent weldability and excellent resistance to corrosion. UNS No. A05140 is recommended for food-processing equipment and marine...
Journal Articles
Alloy Digest (1971) 20 (3): SS-252.
Published: 01 March 1971
... ARMCO 22-13-5 provides an unusually good combination of corrosion resistance and strength for an austenitic stainless steel. It is nonmagnetic even after severe cold work. Common applications are in the petrochemical, chemical, pulp and paper, textile, food processing, and marine industries...
Journal Articles
Alloy Digest (1961) 10 (9): Al-107.
Published: 01 September 1961
... APEX 400 is a 4% magnesium type aluminum casting alloy having high corrosion resistance. It is not heat treatable. It is recommended for marine applications and food processing equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Journal Articles
Alloy Digest (1969) 18 (3): SS-222.
Published: 01 March 1969
... AISI No. 635 is a transformation and a precipitation hardening stainless steel providing a combination of a high degree of corrosion resistance with high strength and hardness. It is recommended for valves, bearings, and chemical and food processing equipment. This datasheet provides information...
Journal Articles
Alloy Digest (1969) 18 (6): SS-225.
Published: 01 June 1969
... Duraloy CB 30 is a cast chromium steel having good corrosion resistance. It cannot be hardened by heat treatment. It is recommended for food processing and oil services at high temperatures, valve bodies, impellers and heat treating equipment. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1987) 36 (8): SS-488.
Published: 01 August 1987
... at elevated temperatures. Type 316 is suitable for a wide range of applications in chemical and petroleum processing, power plants, pollution-control equipment, pulp and paper plants and food and pharmaceutical processing. This datasheet provides information on composition, physical properties, hardness...