1-20 of 236 Search Results for

fluidity

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2002) 51 (12): Al-383.
Published: 01 December 2002
... AlcoTec weld filler wire 4145 is a general-purpose high-silicon-containing wire for both welding and brazing. The alloy is often used instead of 2319 for welding higher-strength alloys because of its low melting temperature and high fluidity. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1965) 14 (11): Al-149.
Published: 01 November 1965
... Alcan 143 is a copper-silicon type aluminum die casting alloy having excellent fluidity, castability and improved machinability. It is recommended for pressure-tight castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (2021) 70 (11): CI-87.
Published: 01 November 2021
... above 5 mm (3/16 in.). It has excellent fluidity, no tendency towards hard edges and a uniformly fine structure with small proportions of ferrite and is, therefore, readily machinable. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also...
Journal Articles
Alloy Digest (1956) 5 (6): Zn-3.
Published: 01 June 1956
... DI-METAL 3 is a zinc-base alloy of high fluidity capable of producing fine detail in die castings. It is the most stable of the zinc die casting alloys, but on aging loses about 20% of its tensile strength with practically no impact drop. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1958) 7 (6): Al-66.
Published: 01 June 1958
... APEX 36 is a high silicon, aluminum die casting alloy having high fluidity, excellent castability and good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness...
Journal Articles
Alloy Digest (1977) 26 (5): Al-226.
Published: 01 May 1977
... FEDERATED F4110 is a general-purpose alloy for making intricate die castings. It is also used for thin-walled, complicated permanent-mold castings where maximum fluidity, pressure tightness and resistance to hot cracking are required. It has excellent castability and foundry characteristics, fair...
Journal Articles
Alloy Digest (1977) 26 (12): Al-231.
Published: 01 December 1977
... ALUMINUM 413.0 is normally classified as a die-casting alloy; however, it also can be used for sand and permanent-mold castings. Its high silicon content (12%) lowers its melting temperature and increases its fluidity, thus improving its castability. It is used for intricate thin-walled castings...
Journal Articles
Alloy Digest (2010) 59 (1): Cu-778.
Published: 01 January 2010
... forgeability. Fig. 1 Tensile and yield strength of Eco Brass DOI: 10.31399/asm.ad.cu0778 Castability: The melting temperature of Eco Brass is 130 °C (234 °F) lower than that of C83600, and the fluidity of Eco Brass is better that that of C83600. Eco Brass is also suitable as a casting alloy. Alloy Melting...
Journal Articles
Alloy Digest (2020) 69 (12): Al-471.
Published: 01 December 2020
... excellent fluidity and resists hot cracking and shrinkage formation. Extensive research and casting simulations have developed the parameters to minimize hot cracking and shrinkage. Castability is further improved by the use of micro-alloying additions and grain refining practices. Grain refinement...
Journal Articles
Alloy Digest (2001) 50 (3): Cu-662.
Published: 01 March 2001
.... The contraction range should be similar to that of leaded yellow brass (not measured). The ten- dency for porosity formation is lower than that of leaded yellow brass. The drossing tendency increases with bismuth content. The fluidity is slightly lower than that of leaded yellow brass in similar casting...
Journal Articles
Alloy Digest (1963) 12 (7): Al-127.
Published: 01 July 1963
... Characteri sti es: CS 2700 alloy was developed to fill a gap between Aluminum 43 and Aluminum 108. On one hand, Aluminum 43 with its low copper content has good corrosion resistance, fluidity, hor crack resistance and pressure rightness, but poor machinability; while Al&mu 10s and related alloys because...
Journal Articles
Alloy Digest (1977) 26 (9): Cu-340.
Published: 01 September 1977
... alIoy 4977 has excellent fluidity. It is one of the best alloys for investment casting and sand casting. It also can be cast in permanent molds, in plaster molds, by pressure methods and centrifugally. Molding and gating practice should follow procedures for manganese bronze and aluminum bronze because...
Journal Articles
Alloy Digest (1987) 36 (8): Cu-527.
Published: 01 August 1987
..., medium gassing, high fluidity, medium shrinkage and medium casting yield. The patternmaker s shrinkage is 3116inch/foot. The effect of section sizeon soundness and mechanical properties is medium. Joinability: The suitability of Copper Alloy No. C82600 is fair for being joined by soldering, brazing...
Journal Articles
Alloy Digest (1997) 46 (4): Cu-612.
Published: 01 April 1997
... of this alloy.) Oxyacetylene welding, carbon arc welding. and gas shielded arc Machinability: Machinability rating (free-cutting brass = 100): 81 Castability: Dressing: JAW Gassing: Medium Fluidity: Medium Shrinkage: Low Casting yield: High Embrittlemenr Not a problem Effect of section size on soundness...
Journal Articles
Alloy Digest (1997) 46 (6): Cu-614.
Published: 01 June 1997
...: Machinability rating (free.-cutting brass = 100): 66 Castability: . . . . l . . l 0 . . Dressing: Low Gassing: Medium Fluidity: High Shrinkage: Low Casting yield: High Embtittlemenc Not a problem Effect of section size on soundness and mechanical proper- ties: sqlall Pattemmakers shrinkage(ift):7~* Pressure...
Journal Articles
Alloy Digest (1997) 46 (2): Cu-610.
Published: 01 February 1997
...- dpoperdesmcuiagorexaedingIbcrypicavahlcslisIcdwhmpamdr2Lr755 (55-F) Oxyacetylene welding. carbon arc welding, gas shielded arc welding. and coated metal arc welding are not recommended Machinability: Machinability rating (free-cutting brass = 100): 80 Castability: 0 Dmssitlg:Low . Gassing: Medium . Fluidity: Medium l Shrinkage:Low l Casting yield: High l...
Journal Articles
Alloy Digest (1997) 46 (3): Cu-611.
Published: 01 March 1997
... . . . 29 . . . 12 Machinability: kdinabiiity rating (free-cutting brass = 100): 85 Castability: Dressing: Low Gassing: Medium Fluidity: Medium Shrinkage: Low Casting yield: High Embrittlement: Not a problem Effect of section size on soundness and mechanical proper- ties: Small Paaemmakers shrinkage (inEt...
Journal Articles
Alloy Digest (1997) 46 (5): Cu-613.
Published: 01 May 1997
... Weldability: Soldering: Excellent Brazing: Good Oxyacetylene welding, carbon arc welding, gas shielded arc welding, and coated metal arc welding are not recommended. Castability: 0 Drossing: Low l Gassing: Medium l Fluidity: Medium 0 Shrinkage: Low l Casting yield: High l Embrittlement: Not a problem l Effect...
Journal Articles
Alloy Digest (1987) 36 (6): Zn-41.
Published: 01 June 1987
... to where it was ready for full-scale commercial use. At that time it was named GALFAN. The work in the preceding paragraph showed the advantages of the superior fluidity and low melting temperature of the zino5% aluminum cutectic composition. It was learned that small additions of mischmetal (a naturally...
Journal Articles
Alloy Digest (1963) 12 (12): Cu-137.
Published: 01 December 1963
... pouring temperature to allow for the cooling that takes place during tapping, skimming and transport to the molds. Riser requirements are somewhat larger than that required for red brass, in fact about half way between red brass and manganese bronze or aluminum bronze. The fluidity of Tombasil...