Skip Nav Destination
Close Modal
Search Results for
fittings
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 654
Search Results for fittings
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (1991) 40 (4): P-25.
Published: 01 April 1991
... MANGUM ABS FG960 is specifically designed for pipe fittings. MAGNUM ABS (acrylonitrile-butadiene-styrene) FG960 is a virgin, prime grade material, listed by the National Sanitation Foundation (NSF). It is available in black as a factory color mix product (natural resin with black color concentrate...
Abstract
View articletitled, FG960 PIPE <span class="search-highlight">FITTING</span> GRADE: Magnum ABS Specialty Resin
View
PDF
for article titled, FG960 PIPE <span class="search-highlight">FITTING</span> GRADE: Magnum ABS Specialty Resin
MANGUM ABS FG960 is specifically designed for pipe fittings. MAGNUM ABS (acrylonitrile-butadiene-styrene) FG960 is a virgin, prime grade material, listed by the National Sanitation Foundation (NSF). It is available in black as a factory color mix product (natural resin with black color concentrate), designated No. 2150-Black-7. MAGNUM ABS FG960 is specifically designed for injection molded pipe fittings for drain, waste and vent, and sewer and conduit uses which meet ASTMD-2661 DWV and F-628 DWV, D-2750 conduit and D-2751 sewer standards. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. Filing Code: P-25. Producer or source: The Dow Chemical Company, Dow Plastics.
Journal Articles
Alloy Digest (1979) 28 (8): Cu-378.
Published: 01 August 1979
...-pressure valve fittings, plumbing fixtures and general hardware fittings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining...
Abstract
View articletitled, COPPER ALLOY No. 845: Cast Semi Red Brass
View
PDF
for article titled, COPPER ALLOY No. 845: Cast Semi Red Brass
Copper Alloy No. 845 was formerly identified as 78-3-7-12 alloy or 78 Semi-Red Brass. It is a free-cutting copper-tin-lead-zinc alloy and is characterized by good casting properties, moderate strength and ductility, excellent machinability and good corrosion resistance. Among its many uses are low-pressure valve fittings, plumbing fixtures and general hardware fittings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-378. Producer or source: Copper alloy foundries.
Journal Articles
Alloy Digest (1995) 44 (3): SS-586.
Published: 01 March 1995
... PARALLOY CR39W is an austenitic heat resisting alloy with a combination of creep strength, carburization resistance and ductility. The alloy can be cast for fittings and centrifugally cast for tubing. Typical applications are within the petrochemical furnace arena. This datasheet provides...
Abstract
View articletitled, PARALLOY CR39W: Cast Heat Resistant Alloy
View
PDF
for article titled, PARALLOY CR39W: Cast Heat Resistant Alloy
PARALLOY CR39W is an austenitic heat resisting alloy with a combination of creep strength, carburization resistance and ductility. The alloy can be cast for fittings and centrifugally cast for tubing. Typical applications are within the petrochemical furnace arena. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance as well as casting. Filing Code: SS-586. Producer or source: Paralloy Ltd.
Journal Articles
Alloy Digest (1997) 46 (6): SS-409.
Published: 01 June 1997
... operations where longer tool life results in more productive machining time. Applications include shafts, valve bodies, valves, valve trim, and fittings. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness and creep. It also...
Abstract
View articletitled, PROJECT 70/PROJECT 7000 STAINLESS TYPE 303: Free-Machining Austenitic Stainless Steels
View
PDF
for article titled, PROJECT 70/PROJECT 7000 STAINLESS TYPE 303: Free-Machining Austenitic Stainless Steels
Project 70 stainless type 303 and Project 7000 stainless type 303 are free-machining stainless steels of the austenitic chromium-nickel type. They offer significantly improved machinability and longer tool life. These steels are suited particularly for automatic bar-machine and Swiss-type machine operations where longer tool life results in more productive machining time. Applications include shafts, valve bodies, valves, valve trim, and fittings. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness and creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-409. Producer or source: Carpenter. Originally published June 1982, revised June 1997.
Journal Articles
Alloy Digest (1997) 46 (7): SS-689.
Published: 01 July 1997
... UCI-190 (HP) material is a general-purpose alloy for use in steam-cracking tubes and fittings and reformer furnaces. HP alloy has carburization, oxidation, and creep resistance at temperatures up to 2000 F. The alloy is weldable by GTAW, GMAW, and SMAW using electrodes with composition matching...
Abstract
View articletitled, UCI-190: Heat-Resistant Cast Stainless Steel
View
PDF
for article titled, UCI-190: Heat-Resistant Cast Stainless Steel
UCI-190 (HP) material is a general-purpose alloy for use in steam-cracking tubes and fittings and reformer furnaces. HP alloy has carburization, oxidation, and creep resistance at temperatures up to 2000 F. The alloy is weldable by GTAW, GMAW, and SMAW using electrodes with composition matching the base metal (25Cr-35Ni) or NiCrCoMo-1 (AWS 5.11 and AWS 5.14). Preheat or post heat normally are not required. UCI-190 has been used for many years providing consistent and predictable results in high-temperature applications. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-689. Producer or source: Ultra-Cast Inc.
Journal Articles
Alloy Digest (1964) 13 (6): SS-156.
Published: 01 June 1964
... AISI No. 630 is a precipitation hardening stainless steel which is used in a variety of applications requiring strength combined with corrosion resistance. It is recommended for chemical process equipment, valve parts, aircraft fittings, pump shafts, etc. This datasheet provides information...
Abstract
View articletitled, AISI No. 630: Hardenable Stainless Steel
View
PDF
for article titled, AISI No. 630: Hardenable Stainless Steel
AISI No. 630 is a precipitation hardening stainless steel which is used in a variety of applications requiring strength combined with corrosion resistance. It is recommended for chemical process equipment, valve parts, aircraft fittings, pump shafts, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness, creep, and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-156. Producer or source: Various alloy steel mills (licensed).
Journal Articles
Alloy Digest (1965) 14 (8): Cu-154.
Published: 01 August 1965
... AUR-O-MET 145 is a silicon bronze die casting alloy having good castability and good weldability. It is suitable for gears, valve parts and marine fittings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Abstract
View articletitled, AUR-O-MET 145: Silicon Bronze
View
PDF
for article titled, AUR-O-MET 145: Silicon Bronze
AUR-O-MET 145 is a silicon bronze die casting alloy having good castability and good weldability. It is suitable for gears, valve parts and marine fittings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on heat treating and machining. Filing Code: Cu-154. Producer or source: Aurora Metal Company.
Journal Articles
Alloy Digest (2020) 69 (1): CI-65.
Published: 01 January 2020
... Dura-Bar G2 is a gray cast iron bar is used for continuous cast products. It is a good fit for a variety of applications due to its good machinability, wear resistance, and vibration damping properties. This datasheet provides information on composition, physical properties, hardness, elasticity...
Abstract
View articletitled, DURA-BAR G2: Gray Cast Iron
View
PDF
for article titled, DURA-BAR G2: Gray Cast Iron
Dura-Bar G2 is a gray cast iron bar is used for continuous cast products. It is a good fit for a variety of applications due to its good machinability, wear resistance, and vibration damping properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on machining. Filing Code: CI-65. Producer or source: Charter Dura-Bar, Inc.
Journal Articles
Alloy Digest (2020) 69 (2): CI-66.
Published: 01 February 2020
... Dura-Bar G2 is a gray cast iron bar is used for continuous cast products. It is a good fit for a variety of applications due to its good machinability, wear resistance, and vibration damping properties. This datasheet provides information on composition, physical properties, hardness, elasticity...
Abstract
View articletitled, MEEHANITE TYPE GM400: Low-Alloy Gray Cast Iron
View
PDF
for article titled, MEEHANITE TYPE GM400: Low-Alloy Gray Cast Iron
Dura-Bar G2 is a gray cast iron bar is used for continuous cast products. It is a good fit for a variety of applications due to its good machinability, wear resistance, and vibration damping properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on machining. Filing Code: CI-65. Producer or source: Charter Dura-Bar, Inc.
Journal Articles
Alloy Digest (1998) 47 (9): Al-353.
Published: 01 September 1998
... welding and very good brazing properties. Initial applications include fittings and connectors that are brazed and/or welded. This product is also available in cold-heading rod that has been used to cold-form connectors. This datasheet provides information on tensile properties. It also includes...
Abstract
View articletitled, ALCOA C238: Cold-Finished Wrought Alloy
View
PDF
for article titled, ALCOA C238: Cold-Finished Wrought Alloy
Alcoa C238 is a cold-finished aluminum wrought product developed for applications requiring postbrazing and welding strength. The alloy has good machinability and roll-threading characteristics. It has slightly lower corrosion resistance as compared to 6xxx series alloys. Alloy C238 has excellent welding and very good brazing properties. Initial applications include fittings and connectors that are brazed and/or welded. This product is also available in cold-heading rod that has been used to cold-form connectors. This datasheet provides information on tensile properties. It also includes information on corrosion resistance as well as machining and joining. Filing Code: AL-353. Producer or source: ALCOA Wire, Rod & Bar Division.
Journal Articles
Alloy Digest (1998) 47 (9): Al-352.
Published: 01 September 1998
...) are known for being small in size. Alloy 2011 is typically used in connectors and fittings, brake pistons, computer parts, knobs, and meter shafts. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fatigue. It also includes...
Abstract
View articletitled, KAISER ALUMINUM ALLOY 2011: Screw Machine Stock Alloy
View
PDF
for article titled, KAISER ALUMINUM ALLOY 2011: Screw Machine Stock Alloy
Kaiser Aluminum alloy 2011 is one of the most popular screw machine stock alloys available. Tennalum, a division of Kaiser Aluminum, produces alloy 2011 in the T3 temper as Microchip II, which offers excellent machinability and surface finish. The chips from Tennalum’s Microchip II (T3 temper only) are known for being small in size. Alloy 2011 is typically used in connectors and fittings, brake pistons, computer parts, knobs, and meter shafts. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: AL-352. Producer or source: Kaiser Aluminum Corporation.
Journal Articles
Alloy Digest (1999) 48 (9): Al-361.
Published: 01 September 1999
... Kaiser Aluminum alloy 6262 (Tennalum alloy 6262) is an Al-Mg-Si-Cu-Cr-Pb-Bi alloy with characteristic good machinability and corrosion resistance and a good acceptance of coatings (anodize response). It is typically used in automotive parts, fittings, building hardware, and valve components...
Abstract
View articletitled, KAISER ALUMINUM ALLOY 6262: Heat Treatable Wrought Aluminum Alloy
View
PDF
for article titled, KAISER ALUMINUM ALLOY 6262: Heat Treatable Wrought Aluminum Alloy
Kaiser Aluminum alloy 6262 (Tennalum alloy 6262) is an Al-Mg-Si-Cu-Cr-Pb-Bi alloy with characteristic good machinability and corrosion resistance and a good acceptance of coatings (anodize response). It is typically used in automotive parts, fittings, building hardware, and valve components. This datasheet provides information on composition, physical properties, tensile properties, and shear strength as well as fatigue. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: AL-361. Producer or source: Tennalum, A Division of Kaiser Aluminum.
Journal Articles
Alloy Digest (1999) 48 (10): Al-360.
Published: 01 October 1999
... Kaiser Aluminum alloy 6061 has excellent joining characteristics and good acceptance of coatings (anodizing response). It is used in applications where weldability and corrosion resistance are needed. The alloy is typically used in fittings, brake pistons, computer parts, couplings, and valves...
Abstract
View articletitled, KAISER ALUMINUM ALLOY 6061: Heat Treatable Wrought Aluminum Alloy
View
PDF
for article titled, KAISER ALUMINUM ALLOY 6061: Heat Treatable Wrought Aluminum Alloy
Kaiser Aluminum alloy 6061 has excellent joining characteristics and good acceptance of coatings (anodizing response). It is used in applications where weldability and corrosion resistance are needed. The alloy is typically used in fittings, brake pistons, computer parts, couplings, and valves. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: AL-360. Producer or source: Tennalum, A Division of Kaiser Aluminum. Originally published March 1999, corrected October 1999.
Journal Articles
Alloy Digest (2001) 50 (7): Ni-570.
Published: 01 July 2001
... KHR45A is a niobium-containing Ni-Cr-Fe alloy with very high temperature usage and high caburization resistance. It is typically used in pyrolysis tubes and fittings. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep...
Abstract
View articletitled, KUBOTA KHR45A: Heat Resistant Cast Alloy
View
PDF
for article titled, KUBOTA KHR45A: Heat Resistant Cast Alloy
KHR45A is a niobium-containing Ni-Cr-Fe alloy with very high temperature usage and high caburization resistance. It is typically used in pyrolysis tubes and fittings. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as joining. Filing Code: Ni-570. Producer or source: Kubota Metal Corporation.
Journal Articles
Alloy Digest (2001) 50 (8): Ni-571.
Published: 01 August 2001
... Kubota KHR45A LC is a modification of KHR45A (Alloy Digest Ni-570, July 2001) that changes either ductility or carburization resistance. The typical application is as outlet tubes and fittings in pyrolysis service. This datasheet provides information on composition, physical properties...
Abstract
View articletitled, KUBOTA KHR45A LC: Heat Resistant Alloy
View
PDF
for article titled, KUBOTA KHR45A LC: Heat Resistant Alloy
Kubota KHR45A LC is a modification of KHR45A (Alloy Digest Ni-570, July 2001) that changes either ductility or carburization resistance. The typical application is as outlet tubes and fittings in pyrolysis service. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance, and corrosion resistance. Filing Code: Ni-571. Producer or source: Kubota Metal Corporation.
Journal Articles
Alloy Digest (1987) 36 (4): Al-279.
Published: 01 April 1987
... properties. It has good castability, excellent machinability and high resistance to corrosion. TERNALLOY 7 has many uses including aircraft components, gears machinery parts, fittings, valves and ornamental products. This datasheet provides information on composition, physical properties, hardness...
Abstract
View articletitled, APEX TERNALLOY 7: Aluminum Foundry Alloy
View
PDF
for article titled, APEX TERNALLOY 7: Aluminum Foundry Alloy
APEX TERNALLOY 7 is one of a family of three APEX TERNALLOYS; see also APEX TERNALLOY 5 (Alloy Digest A1-273, revised March 1987) and APEX TERNALLOY 6 (Alloy Digest A1-277, February 1987). It can be hardened by aging at room temperature without a solution treatment and offers high mechanical properties. It has good castability, excellent machinability and high resistance to corrosion. TERNALLOY 7 has many uses including aircraft components, gears machinery parts, fittings, valves and ornamental products. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: Al-279. Producer or source: Apex International Alloys Inc..
Journal Articles
Alloy Digest (1987) 36 (12): Al-285.
Published: 01 December 1987
... UNS No. A02060 is an aluminum-mold casting alloy that responds to an age-hardening heat treatment. It is recommended for applications that require a combination of high tensile properties and good machinability. Among its many uses are fuel pump bodies, aircraft fittings and seat frames...
Abstract
View articletitled, UNS A02960: Permanent Mold Foundry Alloy
View
PDF
for article titled, UNS A02960: Permanent Mold Foundry Alloy
UNS No. A02060 is an aluminum-mold casting alloy that responds to an age-hardening heat treatment. It is recommended for applications that require a combination of high tensile properties and good machinability. Among its many uses are fuel pump bodies, aircraft fittings and seat frames for railway passenger cars. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on high temperature performance as well as casting, heat treating, machining, and joining. Filing Code: Al-285. Producer or source: Various aluminum companies.
Journal Articles
Alloy Digest (1974) 23 (6): Cu-279.
Published: 01 June 1974
... OM-METAL is a new, corrosion-resistant brass alloy. It has excellent resistance to dezincification which makes it highly suitable for water-system applications, decorative parts and marine fittings. This datasheet provides information on composition, physical properties, hardness, elasticity...
Abstract
View articletitled, OM-METAL: Dezincification Resistant Yellow Brass Alloy
View
PDF
for article titled, OM-METAL: Dezincification Resistant Yellow Brass Alloy
OM-METAL is a new, corrosion-resistant brass alloy. It has excellent resistance to dezincification which makes it highly suitable for water-system applications, decorative parts and marine fittings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, forming, heat treating, machining, and joining. Filing Code: Cu-279. Producer or source: American Smelting and Refining Company.
Journal Articles
Alloy Digest (1974) 23 (8): Al-58.
Published: 01 August 1974
... ALUMINUM 2017 is an age-hardenable wrought alloy of medium strength and ductility. Its service temperature is below 212 F. It is used for general engineering applications, such as transportation equipment, machine parts and fittings. This datasheet provides information on composition, physical...
Abstract
View articletitled, ALUMINUM 2017: Heat Treatable Wrought Aluminum Alloy
View
PDF
for article titled, ALUMINUM 2017: Heat Treatable Wrought Aluminum Alloy
ALUMINUM 2017 is an age-hardenable wrought alloy of medium strength and ductility. Its service temperature is below 212 F. It is used for general engineering applications, such as transportation equipment, machine parts and fittings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on low and high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: Al-58. Producer or source: Various aluminum companies. Originally published October 1957, revised August 1974.
Journal Articles
Alloy Digest (1975) 24 (1): Ni-214.
Published: 01 January 1975
... Nickel-Copper Alloys 410 and 411 are strong and ductile casting alloys; they are generally used in conjunction with wrought counterparts. They can be cast readily into fittings such as elbows, tees, return bends, flanges and similar components. This datasheet provides information on composition...
Abstract
View articletitled, NICKEL COPPER ALLOYS 410 and 411: Corrosion Resistant Casting Alloys
View
PDF
for article titled, NICKEL COPPER ALLOYS 410 and 411: Corrosion Resistant Casting Alloys
Nickel-Copper Alloys 410 and 411 are strong and ductile casting alloys; they are generally used in conjunction with wrought counterparts. They can be cast readily into fittings such as elbows, tees, return bends, flanges and similar components. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: Ni-214. Producer or source: Nickel alloy casting producers.
1