1-20 of 317 Search Results for

fine grain structure

Sort by
Journal Articles
Alloy Digest (2012) 61 (3): SA-645.
Published: 01 March 2012
... Dillimax 500 is a high-strength quenched and tempered, fine-grained structural steel with a minimum yield strength of 500 MPa (72 ksi). Plate is delivered in three qualities: basic, high toughness, and extra tough. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2012) 61 (4): SA-649.
Published: 01 April 2012
... Dillimax 550 is a high-strength quenched and tempered, fine-grained structural steel with a minimum yield strength of 550 MPa (80 ksi). Plate is delivered in three qualities: basic, high toughness, and extra tough. This datasheet provides information on composition, physical properties, tensile...
Journal Articles
Alloy Digest (2012) 61 (5): SA-652.
Published: 01 May 2012
... Dillimax 550 is a high-strength quenched and tempered, fine-grained structural steel with a minimum yield strength of 690 MPa (100 ksi). Plate is delivered in three qualities: basic, tough, and extra tough. This datasheet provides information on composition, physical properties, and tensile...
Journal Articles
Alloy Digest (2012) 61 (6): SA-653.
Published: 01 June 2012
... Dillimax 890 is a high-strength, quenched and tempered fine-grained structural steel with a minimum yield strength of 890 MPa (130 ksi). Plate is delivered in three qualities: basic, tough, and extra tough. This datasheet provides information on composition, physical properties, and tensile...
Journal Articles
Alloy Digest (2012) 61 (8): SA-659.
Published: 01 August 2012
... Dillimax 965 is a high-strength, quenched and tempered, fine-grained structural steel with minimum yield strength of 965 MPa (140 ksi). Plate is delivered in three qualities; basic, tough, and extra tough. This datasheet provides information on composition, physical properties, and tensile...
Journal Articles
Alloy Digest (2012) 61 (9): SA-663.
Published: 01 September 2012
... Dillimax 1100 is a high-strength, quenched and tempered, fine-grained structural steel with minimum yield strength of 1100 MPa (160 ksi). Its mechanical properties are achieved by water quenching followed by tempering. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2018) 67 (1): SA-808.
Published: 01 January 2018
... TBL is a wear-resistant special structural steel with boron as heavy plate that is normalized with thicknesses up to 100 mm (3.9 in.) made of fine-grained structural steel TBL. This datasheet provides information on composition and tensile properties. It also includes information on forming...
Journal Articles
Alloy Digest (2018) 67 (2): SA-811.
Published: 01 February 2018
... TBL Plus is a wear-resistant special structural steel with boron as heavy plate that is normalized with thicknesses up to 12 mm (in.) made of fine-grained structural steel. This datasheet provides information on composition and tensile properties. It also includes information on wear resistance...
Journal Articles
Alloy Digest (1960) 9 (8): TS-96.
Published: 01 August 1960
... KETOS is an oil-hardening non-deforming tool steel having deep hardening qualities with a fine grain structure. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as deformation. It also includes information on forming...
Journal Articles
Alloy Digest (1983) 32 (2): TS-411.
Published: 01 February 1983
... JESSOP TRUFORM is the general-purpose, oil-hardening, non-deforming alloy tool steel for applications where dimensional accuracy is required. It shows very low distortion in heat treating and very high safety (against cracking) in hardening. Truform has deep-hardening properties, a fine-grain...
Journal Articles
Alloy Digest (1973) 22 (6): TS-256.
Published: 01 June 1973
... CRUCIBLE VERSASTEEL is a type of tool steel with its composition carefully balanced to provide an unusual combination of fine grain structure, high secondary hardness and compressive yield strength, good toughness and exceptional wear resistance. Its resistance to tempering approaches that of high...
Journal Articles
Alloy Digest (1989) 38 (4): CI-58.
Published: 01 April 1989
... Ductile Iron grade 45-12 produced by continuous casting has consistent density and fine grain structure. It is the softest of the regular grades of ductile iron and it machines at high speeds with good surface finish. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2008) 57 (7): SA-581.
Published: 01 July 2008
... Domex 315 MC is a hot-rolled, high-strength low-alloy (HSLA) steel with a fine grain structure produced through thermomechanical rolling. It is used for cold-forming operations. The alloy meets or exceeds the requirements of S315MC in EN 10149-2. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2015) 64 (4): SA-724.
Published: 01 April 2015
... Diweten 460 is a fine-grained structural steel with improved atmospheric corrosion resistance. The alloy is thermomechanically rolled. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1967) 16 (1): TS-188.
Published: 01 January 1967
... VERSASTEEL is a tool steel designed to provide an unusual combination of fine grain structure, high secondary hardness, and compressive yield strength together with good toughness and high wear resistance. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1992) 41 (6): Cb-24.
Published: 01 June 1992
... KBI-1 is a columbium-base alloy with zirconium for higher mechanical properties than the pure metal, but developing easier fabrication with its fine grain structure. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (2015) 64 (1): SA-717.
Published: 01 January 2015
... DI-MC 460 is a weldable fine-grained thermomechanically rolled steel for structural design. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing...
Journal Articles
Alloy Digest (1990) 39 (7): CI-61.
Published: 01 July 1990
... machined. Its fine grained structure results in superior machined surface finish. The alloy may be chromium plated for even better surface finish and improved wear resistance. General Characteristics: DURA-BAR G 1A glass mold alloy is fesritic in structure and thus does not respond to heat treatment...
Journal Articles
Alloy Digest (2014) 63 (4): SA-699.
Published: 01 April 2014
... 0.025 Chromium 1.20 Molybdenum 0.30 Boron 0.005 Iron bal The steel is produced with a fine-grained structure. The nitrogen is absorbed to form nitrides. Mechanical Properties: Deliver condition Normalized Hardness at room temperature, HBW Plate thickness, 20 mm (0.787 in.) 270 Plate thickness, > 20...
Journal Articles
Alloy Digest (1976) 25 (12): TS-311.
Published: 01 December 1976
... hardness is 300 Brinell. It has excellent grindability when compared with other high-alloy high-speed grades, yet has excellent wear resistance, red hardness and toughness. Because of the fine grain structure and excellent carbide distribution, WKE4 can be ground to an exceptionally fine cutting edge...