Alloy Digest (2019) 68 (6): Cu-890.
Published: 01 June 2019
..., and relays; in food processing, hospital and medical equipment; and in ferrules. This datasheet provides information on composition and physical properties. Filing Code: Cu-890. Producer or source: Olin Brass. Producer or Source: Olin Brass Copyright © ASM International® 2019 2019 ASM International...
Journal Articles
Alloy Digest (1983) 32 (6): Cu-459.
Published: 01 June 1983
..., where velocities are higher than normal, and where impingement is more severe than normal. Typical uses are condenser and heat-exchanger tubes, distiller tubes and ferrules. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1980) 29 (3): Cu-391.
Published: 01 March 1980
..., and in the chemical processing industries. In sheet form, it is used extensively in the manufacture of hot water tanks for domestic service. In small tube form, it is often fabricated into tips for welding torches, for distilIers tubes and for ferrules. Forms Available: Sheet, strip, plate, tube, rod and bar...
Journal Articles
Alloy Digest (1981) 30 (4): Fe-62.
Published: 01 April 1981
... the ferrule is glass sealed into the base of a lamp, and utilized to make electrical contact between the interior filament and the exterior connectors. Examples of this applica- tion include sealed beam headlamps and floodlamps. This application requires a gas-free seal which is achieved with A-L 42 through...
Journal Articles
Alloy Digest (1985) 34 (9): Cu-500.
Published: 01 September 1985
... 2 - TENSILE REQUIREMENTS FOR SEAMLESS CONDENSER TUBES AND FERRULE STOCK (ASTM Specification B I I I) Temper Annealed Tensile strength, min. psi (MPa) 38000 (260) Yield strength (0.5Vc extension min. psi (MPa) 12000 (85) *Under load. degree back rake. 7-10 degree side clearance and front clearance...
Journal Articles
Alloy Digest (1988) 37 (1): Cu-534.
Published: 01 January 1988
.... Applications: Coastal and sea-water condensers, condenser plates, distiller tubes, evaporator and heat-exchanger tubes, ferrules, and salt-water piping. Manufacturers: Into Alloys International, Inc. Huntington, West Virginia 25720. ...
Journal Articles
Alloy Digest (1991) 40 (2): Cu-557.
Published: 01 February 1991
... and heat-exchanger tubes, ferrules, salt water piping, off- shore drilling platform equipment. Producers: Copper and copper alloy mills. ...
Journal Articles
Alloy Digest (1969) 18 (10): Cu-207.
Published: 01 October 1969
.... Applications: Electronic and electrical components, ferrules, terminals, meter parts. Manufacturer: Connecticut Metals Corp. Hamden, Connecticut ...
Journal Articles
Alloy Digest (1964) 13 (5): Cu-141.
Published: 01 May 1964
... for marine and seaboard power plants and for conditions involving polluted water. It is popular for turbine driven seagoing vessels. Forms Available: Tube Applications: Tubes for condensers, evaporators, heat ex- changers and distillers. Ferrules. Steam Rower plant equipment, chemical and process equipment...
Journal Articles
Alloy Digest (1959) 8 (5): Cu-75.
Published: 01 May 1959
... polluted water. It is popular for turbine driven seagoing vessels. Forms Availabk: Tubes. Applleatlons: Tubes for condensers, evaporators, heat exchangers and distillers. Ferrules. Steam power plant equipment, chemical and process equipment. Marine applications. Manuf actwer: PracticaIIy aII brass mills. ...
Journal Articles
Alloy Digest (1959) 8 (7): Cu-77.
Published: 01 July 1959
... certain operating conditions compares favorably. Forms Available: Sheet, strip, plate, rod, bar, tube. Applications: Condenser tubes and plates, distiller tubes, tube sheets for condensers and heat exchangers, evaporator and heat-exchanger tubes, ferrules, salt water piping. The American Brass Co...
Journal Articles
Alloy Digest (1970) 19 (3): Cu-213.
Published: 01 March 1970
... aboard fast liners and any high-speed, turbinedriven vessels. Forms Available: Tubes Applications: Condenser, evaporator and heat exchanger tubes. Distiller tubes and ferrules. Marine and chemical processing equipment. Manufacturer: Anaconda American Brass Co. Waterbury, Connecticut ...
Journal Articles
Alloy Digest (1971) 20 (8): SS-257.
Published: 01 August 1971
.... It is primarily used as a fastener alloy. Forms Available: Bar, rod, wire. Applications: Fasteners, cold formed parts. ferrules, aircraft and missile components, chemical equipment. Manufacturer: UniversalCyclops Specialty Steel Division Cyclops Corporation Pittsburgh, Pa. 15228. ...
Journal Articles
Alloy Digest (1962) 11 (11): SS-138.
Published: 01 November 1962
..., such as Type 305, 16Cr-18 Ni, 12 Cr-15 Ni, and similar materials. Forms Available: Billets, hot and cold finished bars, hot rolled rods, and cold drawn wire. Applications: Cold formed parts, fasteners, ferrules. Air- craft and missile components, chemical equipment. Manufacturer: Armco Steel Corporation...
Journal Articles
Alloy Digest (1997) 46 (2): SS-671.
Published: 01 February 1997
... as straight or U-ben~ round bar, fit- tings, and flanges. Applications: Safurex has been installed in various parts of urea plants. Gne example is ferrules in a stripper that have been in service for three years without any signs of corrosion. Possible appkations in- clude snipper tubes, carbamate condenser...
Journal Articles
Alloy Digest (1978) 27 (11): Cu-362.
Published: 01 November 1978
... thermal treatment, except that stress reliev- ing is optional after heavy machining. Forms Available: Castings made by the following methods: sand, centrif- ugal and continuous. Ingots. Applications: Chandeliers, ferrules, valves, plumbing components, architecture, ornaments, andirons and bushings. ...
Journal Articles
Alloy Digest (1956) 5 (1): Cu-34.
Published: 01 January 1956
... or munm metal are more commonly used for this purpose. Forms Available: Plate, wire, tube, sheet and strip. Applications: Condenser, evaporator and heat exchanger tubes, condenser tube places. distiller ntbes, ferrules. Manufacturer: All brass mills. ...
Journal Articles
Alloy Digest (1971) 20 (4): Cu-231.
Published: 01 April 1971
.... Applications: Condenser tubes and plates, distiller tubes, tube sheets for condensers and heat exchangers, evaporator and heat exchanger tubes, ferrules, salt water piping, distillers tubes, hot water tanks for domestic service, tips for welding torches. Manufacturer: Most copper alloy mills. ...
Journal Articles
Alloy Digest (1977) 26 (10): Cu-342.
Published: 01 October 1977
.... It is used in the as-cast condition without further thermal treatment, except that stress relieving is optional after heavy machining. Forms Available: Castings made by the following methods: sand, centrif- ugal and continuous. Ingots. Applications: Andirons, bushings, chandeliers, ferrules, valves, plumb...
Journal Articles
Alloy Digest (1974) 23 (9): Cu-284.
Published: 01 September 1974
.../asm.ad.cu0284 Copyright © ASM International® 1996 Table 3 - ROOM-TEMPERATURE TENSILE REQUIREMENTS (As specified in ASTM Bl 11 for seamless condenser tubes and ferrule stock) Temper Light-Drawn Hard-Drawn Tensile strength, psi 36000 45000 Yield strength (0.5% extension under load), psi 30000 40000 Heat Treatment...