Alloy Digest (1959) 8 (9): Cu-81.
Published: 01 September 1959
... Revere No. 508 is a highly ductile, malleable and corrosion resistant copper-nickel alloy suitable for condenser and heat exchanger tubes and many engineering applications such as salt water piping aboard ship, many components of salt water and fresh water stills, feed water heater tubes...
Journal Articles
Alloy Digest (1969) 18 (6): Cu-200.
Published: 01 June 1969
... Cupro Nickel, 30%-716 is a high strength copper-nickel-iron alloy for heat exchanger tubes in power plant feed water heaters, and also for oil refinery service. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1985) 34 (10): Cu-501.
Published: 01 October 1985
... water and is used in marine service. It is used widely for condenser tubes, distiller tubes, heat exchangers, evaporators and water heaters for domestic service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1981) 30 (9): Cu-422.
Published: 01 September 1981
...-speed freighters and other craft powered with reciprocating engines Steam Rower plants: Anaconda Alloy 443 is used widely in the exhaust condense-n of stationary steam power plants where cool- ing water velocities are low, and in auxibary coolers and feed- water heaters operating at moderate pressures...
Journal Articles
Alloy Digest (1969) 18 (2): Cr-2.
Published: 01 February 1969
... fuel-fued oil heaters, direct Bred baffles, super heater tube supports and shields. reactor vessels for treating pulping liquors, oil refinery heaters, nitric acid handling equipment, incinerator components, metallurgical heat treating furnace components. Manufacturer: Universal-Cyclops Specialty Steel...
Journal Articles
Alloy Digest (1985) 34 (4): Ni-312.
Published: 01 April 1985
... product forms including seamless pipe and tube, seam-welded pipe, condenser tube, fittings and flanges, sheet and plate, strip, rod and bar, forgings, wire and welding filler metals. Applications: Feed water and steam generator tubing, brine heaters, sea water scrubbers, pickling bath heating coils, heat...
Journal Articles
Alloy Digest (1965) 14 (7): Cu-153.
Published: 01 July 1965
... in moist ammonia or ammonium hydroxide environments. It is the preferred alloy for tubes used in high pressure, high temperature feedwater heaters. It bas excellent resistance to corrosion in many environments of which the following are typical; acetone, alcohols, beet, beet sugar juices, brines, dry...
Journal Articles
Alloy Digest (2004) 53 (3): SS-901.
Published: 01 March 2004
... in. Applications: Typical applications include high-performance exhaust systems, dairy industry applications, heat exchangers, feed water heaters, moisture separator reheater (MSR) tubing, tubes for the sugar industry, and tubes for heaters, dryers, and hot water tanks. Producer: J & L Specialty Steel, LLC...
Journal Articles
Alloy Digest (1997) 46 (7): SS-689.
Published: 01 July 1997
... for applications such as steel-mill furnace rolls, heat-treating fixtures. radiant tubes, refinery tubes. and ethylene- pyrolysis heaters. Producer: Ultra-Cast Inc. Peru, lN 46970 (800)442-0288 (317)472-395 1 (317) 4724771 (fax) ISSN: 002-614X SS-689B ...
Journal Articles
Alloy Digest (1958) 7 (2): Al-63.
Published: 01 February 1958
...- ance, and good wehdabiliy. Formerly known as AIuminum 66s and Harvey 66-S. Forms Available: Extrusions, tube, rod, bar, forgings and impact ex- trusions. Applications: General structures, gas engine and water heater tubes, water line and condenser tubes, scafTolds, rails, booms. mullions...
Journal Articles
Alloy Digest (1993) 42 (11): SS-554.
Published: 01 November 1993
...) Thickness to 0.050 (1.27mm) Specification Equivalents: Unified Numbering System: S44735 ASTM: Al 76; A240; A268; A5 11 ASME Code Case 1921 (Section VIII-Div 1) Applications: Power industry-condensers; geothermal exchangers; feed water heaters CPI-Tower packing, heat exchangers Petroleum Refining-desalter...
Journal Articles
Alloy Digest (1978) 27 (1): SS-347.
Published: 01 January 1978
... such as steam superheater tubing. connection tubing and refinery heaters. Consult the manufacturer for more details. INCOLOY alloy 800H is a version of INCOLOY alloy 800 having a carbon content restricted to the upper portion of the standard range for alloy 800. Additionally, alloy 800H is given an annealing...
Journal Articles
Alloy Digest (1955) 4 (2): SS-25.
Published: 01 February 1955
... conditions. Forms Available: Bars, rods, plates, forgings, sheets, strip and tubing Applications: Annealing boxes, oil burner parts, heaters, recupera- tors, stirring rods, valves and fittings, pyrometer tubes, baffle plates, glass molds, tube hangers, xray tube bases and lead-in wires, furnace parts...
Journal Articles
Alloy Digest (1995) 44 (4): SS-384.
Published: 01 April 1995
... in (127 mm) or II&X. If annealing of Heat Exchanger Type 430 tubing is raquirsd it is recommendedchatitbedone at 14OO/l4WF(7~f~aa least 10 minutes at heat and rapidly cooled in air a a f+ water spray. DOI: 10.31399/asm.ad.al0384 Copyright ┬ę ASM International┬« 1996 Machinability: Jn turning operations...
Journal Articles
Alloy Digest (1998) 47 (4): SS-714.
Published: 01 April 1998
... to 10 percent fatty oil is rec- ommended for high speed steel tools. Water-soluble cutting flu- ids are primarily coolants and are most useful for high speed op- eration with carbide tools. Rough turning speeds with high speed steel tools can be 35-45 sfm with 0.020-0.025 ipr feed and jic,& in. depth...
Journal Articles
Alloy Digest (1956) 5 (1): Ni-22.
Published: 01 January 1956
..., flame tubes, slator blades, dies and cores for die-casting aluminum and bronze and brass, furnace tubes, thermocouple sheaths, precision molds for glass, first-stage blading for steam turbines, com- bustion components of aircraft, cabin heaters, gas tur- bine tubes. Manufacturers: Henry Wiggin & Co...
Journal Articles
Alloy Digest (2006) 55 (6): Cu-744.
Published: 01 June 2006
...-Al bronze 247 36 0.075 4.3 Hiduron 191 425 62 0.02 4.8 DOI: 10.31399/asm.ad.cu0744 Applications: Defense applications include control elements of submarines, pump shafts, mechanical seals, gears, hose couplings, propeller shafts, and drive bushes. The alloy is used as tubes and tube plates for heavy...
Journal Articles
Alloy Digest (1986) 35 (9): SS-475.
Published: 01 September 1986
..., flanges. disc and ring forgings. Applications: Nitric acid coolers, acetic anhydride cracking tubes. steam super-heater tubing, heating element sheathing and others. Manufacturer: Vereinigte Deutsche Metallwerke AG Werdohl. West Germany. In USA: VDM Technologies Corporation Parsippany. New Jersey 07054. ...
Journal Articles
Alloy Digest (1984) 33 (8): SS-450.
Published: 01 August 1984
... 310S, a few typical uses include annealing boxes, chemical plant equipment, fire box sheets, furnace linings, heat exchangers, oil-refining equipment, kiln linings and tube hangers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1975) 24 (3): SS-307.
Published: 01 March 1975
... as steel-mill furnace rolls. heat-treating fixtures, radiant tubes, refinery tubes and ethylene pyrolysis heaters. Manufacturers: Foundries that produce stainless steel castings. ...