Alloy Digest (1983) 32 (4): Cu-457.
Published: 01 April 1983
... fixtures, faucets and general hardware. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as creep. It also includes information on high temperature performance and corrosion resistance as well as casting...
Journal Articles
Alloy Digest (2019) 68 (5): Cu-887.
Published: 01 May 2019
..., plate, profile or structural shape, flats/rectangular bar DOI: 10.31399/asm.ad.cu0887 Applications Typical uses include: Plumbing: faucets, pump components, pipe fittings, plumbing goods, water pump impellers Industrial: housings, small gears Producer Concast Metal Products Co. Wakeman, OH 44889...
Journal Articles
Alloy Digest (1997) 46 (4): Cu-612.
Published: 01 April 1997
.... and plating. The above-noted prop- erties are all important to the faucet manufacturing industry. With respect to corrosion in water, the leachate mte for lead and bis- muth in drinking water are extremely low. Federalloy melts and casts similarly to leaded brass. Because bismuth is less reactiv than lead...
Journal Articles
Alloy Digest (1997) 46 (6): Cu-614.
Published: 01 June 1997
... and C84400. This includes mechanical strength. pressure tightness, corrosion resis- tance. and polishing. buffing, and plating. The above-noted prop- erties are all important to the faucet manufacturing industry. With respect to corrosion in water, the leachate rate for lead and bismuth in drinking water...
Journal Articles
Alloy Digest (1965) 14 (11): Cu-157.
Published: 01 November 1965
..., bolts, fasteners, faucet handles, plumbing fixtures, stop-cocks, valve bodies. Manufacturer: Noranda Copper Mills, Ltd. Montreal, Quebec, Canada ...
Journal Articles
Alloy Digest (1997) 46 (3): Cu-611.
Published: 01 March 1997
... to alloys UNS C83600 and C844OO. This in- cludes mehanical strength, pressure tightness, corrosion resis- tance. and polishing, buffing. and plating. The above-noted prop- erties are all important to the faucet manufacturing industry. With respect to corrosion in water, the leachate tate for lead and bis...
Journal Articles
Alloy Digest (2011) 60 (3): Cu-796.
Published: 01 March 2011
... applications include bicycle spoke nipples, drawer handles, drawer pulls, faucet seats and stems. Producer: Ansonia Copper & Brass Ansonia, CT 06401 USA Tel: (800) 512-1703 Fax: (203) 735-3787 Ansonia Copper & Brass, Inc. Waterbury, CT 06708 USA Tel: (800) 512-1703 or (203) 735-3787 Web: www.ansoniacb.com ISSN...
Journal Articles
Alloy Digest (1965) 14 (1): Cu-147.
Published: 01 January 1965
.... It is extremely plastic hot, combining good cor- rosion resistance with excellent mechanical properties. Forms Available: Extruded rods and shapes, forgings, rolled or drawn rods. Applications: Bucket strainers, faucet handles, gears, hardware, lock parts, plumbing fittings, shower heads, sink strainers, stop...
Journal Articles
Alloy Digest (2002) 51 (12): Cu-695.
Published: 01 December 2002
... also has applications in machined parts such as fittings, faucets, valves, and components for instru- ments and is used for coffee machines. Producer: Swissmetal Metalworks Ltd, Plant Boillat CH-2732 Reconvilier, Switzerland +41-32 482 0 482 +41-32 482 0 116 (fax) www.swissmetal.com In USA: Avins...
Journal Articles
Alloy Digest (2011) 60 (4): Cu-797.
Published: 01 April 2011
... products. Specific applications include faucet stems and seats, gauges, lock hardware, and valve stems, seats, and trim. Producer: Ansonia Copper & Brass, Inc. Waterbury, CT, 06708 USA Tel: (800) 512-1703 or (203) 735-3787 Web: www.ansoniacb.com ISSN: 002-614X CU-797B ...
Journal Articles
Alloy Digest (1991) 40 (9): Zn-1.
Published: 01 September 1991
...: Ingot, die castings. Applications: Automotive components (housings, heat sinks, trim, handles), electronics, household faucets, hand tools and a wide variety of general purpose applications where net shape, precision and physical properties are important. Producer: Noranda Sales Corporation Toronto...
Journal Articles
Alloy Digest (1976) 25 (12): Cu-323.
Published: 01 December 1976
... applications including couplings and fit- tings, taps, cocks, faucets, valves, flanges and water mixers for bathrooms; housings for water-meters and thermostats; pump housings, shafts and wheels; end pieces for brake lines in cars. buses and trucks; marine hardware; halyard and sheet winches for boats...
Journal Articles
Alloy Digest (2021) 70 (3): Cu-918.
Published: 01 March 2021
... of the machinability of UNS C36000, free-cutting brass. The rating is based on relative speed for equivalent tool life See Table 5. Information on annealing sourced from C36000, Copper Applications Development Association. Adapters; bolts, screws, and nuts; faucet components; fit- Stress Relieving. If cold working...
Journal Articles
Alloy Digest (1979) 28 (8): Cu-378.
Published: 01 August 1979
... and under carefully controlled conditions. Forms Available: Castings made by the following methods: sand, centrifugal and continuous. Ingots. Applications: Plumbing futures, cocks, faucets, stops, waste fittings, air and gas fittings, general hardware fittings and low-pressure valve fittings. Manufacturers...
Journal Articles
Alloy Digest (2001) 50 (3): Cu-662.
Published: 01 March 2001
... awareness of health and the environ- ment, adoption of the name EnviroBrass should achieve a high degree of acceptance by the specifiers and purchasers of faucets, valves, water meters, and other plumbing devices. SeBiLOY will continue to be used and will sometimes appear alone or in paren- theses following...