Skip Nav Destination
Close Modal
Search Results for
fatigue endurance limit
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 322
Search Results for fatigue endurance limit
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (1997) 46 (9): Ti-109.
Published: 01 September 1997
...) that enhances the fatigue endurance limit. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength as well as fatigue. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: TI-109. Producer...
Abstract
View articletitled, SANDVIK Ti-3Al-2.5V GRADE 9: Corrosion-Resistant High-Strength Titanium Alloy
View
PDF
for article titled, SANDVIK Ti-3Al-2.5V GRADE 9: Corrosion-Resistant High-Strength Titanium Alloy
Sandvik Ti-3Al-2.5V Grade 9 titanium-aluminum alloy offers excellent corrosion resistance, especially to chloride media, and has a high strength-to-weight ratio, which is especially suitable for use in aerospace applications. Tubing can be produced having a CSR (contractile strain ratio) that enhances the fatigue endurance limit. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength as well as fatigue. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: TI-109. Producer or source: Sandvik.
Journal Articles
Alloy Digest (2022) 71 (12): Al-492.
Published: 01 December 2022
... for alloying content and strength. It has excellent fatigue properties, with an endurance limit of 115 MPa in the H32 temper and 125 MPa in the H34 temper. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion...
Abstract
View articletitled, AUSTRAL WRIGHT 5052: Al-2.5Mg-0.25Cr Alloy
View
PDF
for article titled, AUSTRAL WRIGHT 5052: Al-2.5Mg-0.25Cr Alloy
Austral Wright 5052 is a wrought, non-heat-treatable, aluminum-magnesium-chromium alloy (5xxx series) that exhibits a good combination of strength, corrosion resistance, and formability in a wide range of rolled products. It is about mid-way through the series of aluminum-magnesium alloys for alloying content and strength. It has excellent fatigue properties, with an endurance limit of 115 MPa in the H32 temper and 125 MPa in the H34 temper. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-492. Producer or source: Austral Wright Metals.
Journal Articles
Alloy Digest (1958) 7 (5): SA-68.
Published: 01 May 1958
... composition ductility elasticity endurance limit fatigue properties Ferrovac-4340 fracture toughness hardness heat treatability joinability machinability notched tensile strength physical properties workability Filing Code: SA-68 FERROVAC 4340 Steel-Alloy MAY 1958 -DATA ON WORLD WIDE METALS...
Abstract
View articletitled, FERROVAC 4340: Vacuum Melted Alloy Steel
View
PDF
for article titled, FERROVAC 4340: Vacuum Melted Alloy Steel
Ferrovac-4340 is a vacuum melted chromium, nickel, molybdenum alloy steel having high endurance limit, high notched tensile strength, and high transverse ductility. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-68. Producer or source: Vacuum Metals Corporation.
Journal Articles
Alloy Digest (2010) 59 (9): Al-431.
Published: 01 September 2010
... specimen Hardness Shear, ultimate shearing strength, MPa (ksi) Fatigue, endurance limit R.R. Moore type, MPa (ksi)Ultimate, MPa (ksi) Yield, MPa (ksi) Elongation/4D, % T5 260 (38) 240 (35) 10 DOI: 10.31399/asm.ad.al0431 ISSN: 002-614X AL-431B Table 2 Comparative characteristics Temper Corrosion resistance...
Abstract
View articletitled, KAISER ALLOY 6005: Extruded Rod and Bar
View
PDF
for article titled, KAISER ALLOY 6005: Extruded Rod and Bar
Kaiser Alloy 6005 is a pressure vessel material with corrosion resistance and weldability. This datasheet provides information on composition, physical properties, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: AL-431. Producer or source: Kaiser Aluminum.
Journal Articles
Alloy Digest (2010) 59 (12): Al-434.
Published: 01 December 2010
...: (800) 88873-2011 Web: www.Kaiseraluminum.com Table 1 Typical mechanical properties (longitudinal) Temper Tensile, 12.7 mm (0.500 in.) diameter specimen Yield, MPa (ksi) Elongation/4D, % Brinell hardness, 500 kg, 10 mm Ultimate shearing strength, MPa (ksi) Fatigue endurance limit R.R. Moore type, MPa...
Abstract
View articletitled, KAISER ALLOY 7003: Extruded Rod and Bar
View
PDF
for article titled, KAISER ALLOY 7003: Extruded Rod and Bar
Kaiser Alloy 7003 is a medium strength alloy originally developed in Japan. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming and joining. Filing Code: AL-434. Producer or source: Kaiser Aluminum.
Journal Articles
Alloy Digest (2011) 60 (6): Al-437.
Published: 01 June 2011
... Aluminum Foothill Ranch, CA 92610-2831 USA Tel: (800) 873-2011 Web: www.Kaiseraluminum.com ISSN: 002-614X AL-437 Table 1 Typical mechanical properties Temper Tensile, 12.7 mm (0.5 in.) diameter(a) Hardness Rockwell E, 100 kg (0.0625 in.) ball Ultimate shearing strength, MPa (ksi) Fatigue endurance limit...
Abstract
View articletitled, KAISER ALLOY 7033: High Strength Forgings
View
PDF
for article titled, KAISER ALLOY 7033: High Strength Forgings
Kaiser Alloy 7033 is a high strength alloy used in automotive frames. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fatigue. It also includes information on forming, machining, and joining. Filing Code: Al-437. Producer or source: Kaiser Aluminum.
Journal Articles
Alloy Digest (2017) 66 (1): Al-451.
Published: 01 January 2017
... endurance limit, R.R. Moore type, MPa (ksi) 110 (16) Modulus of elasticity, GPa (106 psi) 70 (10.2) Specification Equivalents: ASTM B807 (Extrusions) General Characteristics: One of the magnesium alloys typically used in hydraulic tube and appliance applications. Good corrosion resistance and good...
Abstract
View articletitled, KAISER ALLOY 5052: High Strength Alloy
View
PDF
for article titled, KAISER ALLOY 5052: High Strength Alloy
Kaiser alloy 5052 in pipe and tube is used in hydraulic lines. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on forming, machining, and joining. Filing Code: Al-451. Producer or source: Kaiser Aluminum Corporation.
Journal Articles
Alloy Digest (2017) 66 (2): Al-452.
Published: 01 February 2017
... Ultimate shearing strength, MPa (ksi) 76 (11) Fatigue endurance limit, R.R. Moore type, MPa (ksi) 48 (7) Modulus of elasticity, GPa (106 psi) 69 (10) Specification Equivalents: ASTM B807 (Extrusions) General Characteristics: One of the magnesium alloys. Typically used for condensers and heat exchangers...
Abstract
View articletitled, KAISER ALLOY 3: High Strength Alloy
View
PDF
for article titled, KAISER ALLOY 3: High Strength Alloy
Kaiser Alloy 3003 is a general engineering alloy produced as tubing. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: Al-452. Producer or source: Kaiser Aluminum Corporation.
Journal Articles
Alloy Digest (2016) 65 (7): Al-443.
Published: 01 July 2016
... (0.500 in.) diameter specimen Hardness, Brinell 500 kg (1102 lb), 10 mm (0.4 in.) Ultimate shearing strength, MPa (ksi) Fatigue, endurance limit, R.R. Moore type, MPa (ksi) Modulus of elasticity, GPa (106 psi) Ultimate, MPa (ksi) Yield, MPa (ksi) Elongation, 4D, % T6,T76511 648 (94) 593 (86) 5 170...
Abstract
View articletitled, KAISER ALLOY 7X49: High-Strength Rod and Bar Alloy
View
PDF
for article titled, KAISER ALLOY 7X49: High-Strength Rod and Bar Alloy
Kaiser Alloy 7X49 is used in aircraft structural parts. The alloy has characteristics of high strength and good machinability. Good resistance to stress-corrosion cracking in –T7 type temper. X represents either or 1 or 0 as noted in the tex This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming and joining. Filing Code: Al-443. Producer or source: Kaiser Aluminum Corporation.
Journal Articles
Alloy Digest (1961) 10 (11): Cu-109.
Published: 01 November 1961
... coef. expansion/OF (68572oF) x 10-6 Thermal conductivity, Btu/ft2/ft/hr/oF Modulus of elasticity, psi x 106 7.69 0.278 7.0 .48 9.2 22.0 16.5 PROPERTIES TYPICAL MECHANICAL PROPERTIES Tensile strength, psi Yield strength, psi (0.5%) Elongation, % in 2 Rockwell hardness Fatigue endurance limit, psi Izod...
Abstract
View articletitled, DURONZE 707: Aluminum Silicon Bronze
View
PDF
for article titled, DURONZE 707: Aluminum Silicon Bronze
Duronze 707 is a tough, corrosion and wear resistant aluminum-silicon bronze, with excellent hot working and forging characteristics plus good machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-109. Producer or source: Bridgeport Brass Company.
Journal Articles
Alloy Digest (2019) 68 (11): Al-459.
Published: 01 November 2019
... of elasticity, GPa (106 psi) Ultimate, MPa (ksi) Yield, MPa (ksi) Elongation/4D, % Hardness, Brinell, 500 kg (1102 lb), 10 mm (0.4 in.) Ultimate shearing strength, MPa (ksi) Fatigue endurance limit R.R. Moore type, MPa (ksi) O 90 (13) 34 (5) 35 23 62 (9) 34 (5) 69 (10) H14 124 (18) 117 (17) 9 32 76 (11) 48 (7...
Abstract
View articletitled, KAISER ALLOY 1100: Commercially Pure Aluminum
View
PDF
for article titled, KAISER ALLOY 1100: Commercially Pure Aluminum
Kaiser Alloy 1100 is in the commercially pure wrought family (1000 or 1xxx series) of aluminum alloys. It is typically used in applications requiring maximum ductility and relatively low strength. It has good corrosion resistance, workability, and weldability. This datasheet provides information on composition, physical properties, hardness, elasticity, and shear strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as machining and joining. Filing Code: Al-459. Producer or source: Kaiser Aluminum Corporation.
Journal Articles
Alloy Digest (2018) 67 (1): Al-456.
Published: 01 January 2018
.... Table 1 Typical mechanical properties Temper Tensile strength 12.7 mm (0.500 in.) diameter specimen Hardness Brinell, 500 kg (1102 lb), 10 mm (0.4 in.) Ultimate shearing strength, MPa (ksi) Fatigue endurance limit(a), R.R. Moore type, MPa (ksi) Modulus of elasticity, GPa (106 psi) Ultimate, MPa (ksi...
Abstract
View articletitled, KAISER ALLOY K211: Free-Machining Alloy
View
PDF
for article titled, KAISER ALLOY K211: Free-Machining Alloy
Kaiser Alloy K211 is a rod and bar alloy that is RoHS compliant (2011). This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: Al-456. Producer or source: Kaiser Aluminum Corporation.
Journal Articles
Alloy Digest (2008) 57 (1): Fe-143.
Published: 01 January 2008
... also Tables 1 4. Formability: See Table 5. Table 2 Fatigue Endurance Limit at 10 7 Cycles Temperature Fatigue limit, alternate bending Fatigue limit, fluctuating tension(a), max °C °F MPa ksi MPa ksi 20 68 210 30 320 46 196 321 400 58 540 78 Fatigue tests have been performed in both the alternating...
Abstract
View articletitled, INVAR M93: Controlled-Expansion Alloy
View
PDF
for article titled, INVAR M93: Controlled-Expansion Alloy
Invar is an Fe-Ni alloy with 36% Ni content that exhibits the lowest expansion of known metals from very low temperatures up to approximately 230 deg C (445 deg F). Invar M93 is a cryogenic Invar with improved weldability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear and bend strength as well as fracture toughness and fatigue. It also includes information on low temperature performance as well as forming and joining. Filing Code: FE-143. Producer or source: Metalimphy Precision Alloys.
Journal Articles
Alloy Digest (1991) 40 (10): Zn-35.
Published: 01 October 1991
...-40 32-37 Yield strength (0.2% offset) MPa 193-200 200-214 ksi 28-29 29-31 Elongation (2 in % l-2 1-2 Modulus of elasticity, MPa 87.6xW 85.5~103 ksi 12.7xlW 12.4~103 Poisson s ratio 0.29-0.30 0.29-0.30 Hardness, Brinell 82-89 85-90 Vickers (5kg) 110-120 105-115 Fatigue endurance limit (Approximate...
Abstract
View articletitled, ZA-8: Zinc-Base Casting Alloy
View
PDF
for article titled, ZA-8: Zinc-Base Casting Alloy
ZA-8 is a zinc-base foundry alloy capable of being sand, permanent mold gravity or die cast (hot-chamber machine). ZA-8 should be the first choice when considering die casting the ZA family (3 alloys) due to its cost effective hot-chamber castability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness, creep, and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: Zn-35. Producer or source: Noranda Sales Corporation. Originally published November 1980, revised October 1991. See also Zn-48, January 1990.
Journal Articles
Alloy Digest (2011) 60 (3): Al-436.
Published: 01 March 2011
.... T4 temper 6063 has an ultimate tensile strength of at least 131 MPa (19 ksi) in thicknesses up to 13 mm (0.5 in and Table 1 Typical mechanical properties Temper Tensile diameter specimen, 12.7 mm (0.500 in.) Brinell hardness, 500 kg, 10 mm Ultimate shearing strength, MPa (ksi) Fatigue endurance limit...
Abstract
View articletitled, KAISER ALLOY 6063: High Strength Extruded and Drawn Products
View
PDF
for article titled, KAISER ALLOY 6063: High Strength Extruded and Drawn Products
Kaiser Alloy 6063 is a magnesium/silicon alloy. One of the most popular of the heat treatable alloy group. Products include extruded and drawn tube, pipe, rod, bar, and profiles. This alloy has good corrosion resistance, good weldability, and a good anodizing response. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming and joining. Filing Code: Al-436. Producer or source: Kaiser Aluminum. See also Alloy Digest Al-458, July 2019.
Journal Articles
Alloy Digest (1997) 46 (8): Ti-108.
Published: 01 August 1997
... solu- tionsandisimmtmetoSCCinseawater. f2ormsbn Fatigue Titanium, unlike many other mamials. does notshowadeueaseinfatigueperlbrmanceinthepresenceof seawater. Both fatigue endurance limits and fatigue sack growth IZltCS~thCSameiIlairandSeaWata. Hydrogen Embrittlement There is no signifhnt absorption...
Abstract
View articletitled, SANDVIK TITANIUM GRADE 2: Corrosion-Resistant Unalloyed Titanium
View
PDF
for article titled, SANDVIK TITANIUM GRADE 2: Corrosion-Resistant Unalloyed Titanium
Sandvik titanium Grade 2 is chemically pure (CP) titanium produced as seamless and SeamFree tubing. The alloy is resistant to a wide variety of chloride media and is used to handle seawater. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: TI-108. Producer or source: Sandvik.
Journal Articles
Alloy Digest (2014) 63 (6): Fe-163.
Published: 01 June 2014
...-46850D, MPa m (ksi in) 82 (75) Fatigue endurance limit, k t = 2.2, MPa (ksi) Smooth 758 (110) Notched 379 (55) Typical room temperature properties and elevated temperature tensile properties are shown in Tables 1 and 2, respectively. Heat Treatment: Maraging Cycle. Hold 3 6 hours at 482 °C (900 °F...
Abstract
View articletitled, MARVAC 250 VIM-VAR: High-Strength Maraging Steel
View
PDF
for article titled, MARVAC 250 VIM-VAR: High-Strength Maraging Steel
Marvac 250 is a clean high-strength maraging steel capable of 1654 MPa (240 ksi) yield strength. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on forming, heat treating, machining, and joining. Filing Code: Fe-163. Producer or source: Latrobe Specialty Steel Company.
Journal Articles
Alloy Digest (1977) 26 (11): CS-69.
Published: 01 November 1977
... generally decreases as the carbon and alloy content increases. When substituting these higher yield strength steels for lower carbon SAE 1008 or 1010 steels, use welding practices that provide the properties required for a given application. Fatigue Properties: The fatigue endurance limit of steels...
Abstract
View articletitled, ARMCO GAINEX STEELS: Hot Rolled Carbon Steels
View
PDF
for article titled, ARMCO GAINEX STEELS: Hot Rolled Carbon Steels
ARMCO GAINEX Steels comprise a family of five low-cost structural carbon steels. This family includes: GAINEX-35, GAINEX-40, GAINEX-45, GAINEX-50 and GAINEX SA (Strain ageable); the numbers following GAINEX refer to minimum specified (ordered) yield strengths in 1000 psi. These steels are well suited to the automotive, farm and construction equipment, and appliance industries for such applications as truck bodies, light poles, bumper support members and parts for agricultural implements. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: CS-69. Producer or source: Armco Inc., Eastern Steel Division.
Journal Articles
Alloy Digest (2002) 51 (9): SS-862.
Published: 01 September 2002
.../min without lubrication using a Sandvik GC235 insert. DOI: 10.31399/asm.ad.ss0862 See Fig. 1 for fatigue performance. In rotating bend Wöhler fatigue tests, higher-strength Datalloy 2 with a 0.2% offset yield strength in excess of 965 MPa (140 ksi) has been shown to have a fatigue endurance limit...
Abstract
View articletitled, DATALLOY 2: Nonmagnetic Stainless Steel
View
PDF
for article titled, DATALLOY 2: Nonmagnetic Stainless Steel
Datalloy 2 is an enhanced corrosion-resistant nonmagnetic stainless steel. The composition contains a high level of manganese and nitrogen to stabilize the austenite. Applications include replacement of standard chromium-manganese steels in drill string components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as machining. Filing Code: SS-862. Producer or source: Allvac Ltd.
Journal Articles
Alloy Digest (2014) 63 (7): Fe-164.
Published: 01 July 2014
..., Charpy V-notch on materials, solution annealed and aged at 482 °C (900 °F), J (ft·lbf) RT 27 (20) 73 °C ( 100 °F) 22 (16) 129 °C ( 200 °F) 18 (13) Fracture toughness, minimum value per MIL-S-46850D, MPa m (ksi in.) 66 (60) Fatigue endurance limit, smooth, MPa (ksi) 862 (125) Heat Treatment: Maraging...
Abstract
View articletitled, MARVAC 300 VIM-VAR: High-Strength Maraging Steel
View
PDF
for article titled, MARVAC 300 VIM-VAR: High-Strength Maraging Steel
Marvac 300 is a clean high-strength maraging steel capable of 1862 MPa (270 ksi) minimum yield strength. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: Fe-164. Producer or source: Latrobe Specialty Steel Company.