1-20 of 47 Search Results for

farming equipment

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1978) 27 (12): SA-352.
Published: 01 December 1978
... of its unique microstructure; in fact, it increases from its delivered yield strength of 50,000 psi up to 80,000 psi (or more) in forming. Its final strength depends on the amount of forming. Its many applications include automotive vehicles, farm equipment and heavy construction equipment...
Journal Articles
Alloy Digest (1971) 20 (12): Cu-246.
Published: 01 December 1971
... COMPO H is an oil-impregnated sintered bronze, produced by powder metallurgy techniques, which is widely used in automotive, applicance, farm equipment, and aircraft industry applications. This datasheet provides information on composition, physical properties, tensile properties, and compressive...
Journal Articles
Alloy Digest (1979) 28 (3): SA-356.
Published: 01 March 1979
... of a fully killed, low-carbon, vacuum-degassed, columbium-alloyed steel. This special composition and processing practice minimize harmful nonmetallic inclusions that hamper formability. Typical applications include automotive, construction and farm-equipment components. This datasheet provides information...
Journal Articles
Alloy Digest (1980) 29 (10): SA-377.
Published: 01 October 1980
...); this allows matching strength level to the job requirement. Their wide range of use includes automotive, tractors, farm equipment, bridges and buildings. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion...
Journal Articles
Alloy Digest (1991) 40 (10): Cp-18.
Published: 01 October 1991
... appliances, farm and construction equipment. This datasheet provides information on physical properties, hardness, tensile properties, and compressive strength as well as fracture toughness and creep. It also includes information on corrosion resistance. Filing Code: Cp-18. Producer or source: E. I. Dupont...
Journal Articles
Alloy Digest (1977) 26 (11): CS-69.
Published: 01 November 1977
... suited to the automotive, farm and construction equipment, and appliance industries for such applications as truck bodies, light poles, bumper support members and parts for agricultural implements. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1977) 26 (6): SA-334.
Published: 01 June 1977
... AISI 5147 is a low-chromium (nominally 1% chromium), intermediate-hardenability alloy steel for medium-duty applications. It is normally hardened by quenching in oil. It has a wide range of applications for transportation equipment, farm implements, tools and industrial machinery. This datasheet...
Journal Articles
Alloy Digest (1980) 29 (6): CI-50.
Published: 01 June 1980
... many applications include automotive equipment, farm machinery, bushings and machine tools. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes...
Journal Articles
Alloy Digest (1966) 15 (5): SA-194.
Published: 01 May 1966
... to brittle fracture. Excellent fatigue rest results suggest McLouch ML-50 as an outstanding material for applications subjected to wide ranges of temperature exposure such as experienced with transportation vehicles, outdoor storage tanks and farm equipment. Forms Available: Bars, rods, places, sheet, strip...
Journal Articles
Alloy Digest (2019) 68 (9): SA-852.
Published: 01 September 2019
..., not to be used for specification or final design. handling equipment, farm equipment, industrial machinery and almost anywhere precision, top-quality piston rods are needed. Every IHCP and CPO product undergoes extensive electronic and visual inspection before shipping. This ensures the uses of a piston rod...
Journal Articles
Alloy Digest (1971) 20 (10): SA-269.
Published: 01 October 1971
...: Sheet, strip, light plate (l/4 to 3/8-inch thick). It is also available in Super Diamond floor plate to 3/8-inch thick. Applications: Automotive and truck parts, petroleum and farm equipment, railroad cars and construction equipment. Manufacturer: Alan Wood Steel Company Conshohocken, Pa. 19428. ...
Journal Articles
Alloy Digest (1996) 45 (1): SS-632.
Published: 01 January 1996
... of materials, INCO-WELD C Welding Electrode is useful for dissimilar metal joints and for joining steels whose specific compositions are unknown. It has a wide range of potential welding, maintenance and repair applications including cement and quarry equipment. farm equipment, screw conveyors. tool and die...
Journal Articles
Alloy Digest (1988) 37 (9): Al-290.
Published: 01 September 1988
... bearings; compressor main bearings; steel rolling mill heavy duty bearings; farm equipment track roller bushings; bushings for hydraulic pumps; bearings for high shock loads in landing gear assemblies. Manufacturer: Federal Bronze products. Inc. Newark, New Jersey 07105 ...
Journal Articles
Alloy Digest (1971) 20 (11): SS-263.
Published: 01 November 1971
... applicable to the stainless steels. Forms Available: Sheet, strip. Applications: Automobile mufflers and tailpipes, transformer cases, cold water storage tanks, culverts, shipping containers, hidden structural supports, farm equipment. Manufacturer: Allegheny Ludlum Steel Corporation Division of AUegheny...
Journal Articles
Alloy Digest (1980) 29 (5): CS-83.
Published: 01 May 1980
... hand tools to heavy components for farm equipment and industrial machinery. Forms Available: Billets, rods, bars, hot-rolled strip, cold-rolled strip, wire, and heavy forged and rolled shapes. Applications: Hand tools, wire products, control rods, heavy machinery parts, screwdrivers, pliers, hammers...
Journal Articles
Alloy Digest (1988) 37 (11): Zn-44.
Published: 01 November 1988
...: Industrial and automotive bearing components, bus and transit components, pressure-tight castings, high-strength thin-wallcastings,wear-resistantanti-gaIlingparts,valves, industrial pulleys and sheaves, components for various types of industrial and farm equipment, lock hardware, and electrical components...
Journal Articles
Alloy Digest (1971) 20 (4): SA-263.
Published: 01 April 1971
... to 0.75~inch thick), and structural shapes. Applications: Railroad cars, mine cars, construction equipment, automotive and truck parts, petroleum and farm equipment. Manufacturer: Licensees of international Nickel The International Nickel Company, Inc. New York, New York 10004. ...
Journal Articles
Alloy Digest (1971) 20 (2): SA-260.
Published: 01 February 1971
... rzquir2menIs of AST%l AZO. Forms Available: Plare. bsr. tlars. structural shapes, and blooms (on inquiry). Applications: Structural. piping and pressure vessel applications. Heavy machinery. truck frames. construction and farming equipment, subjected IO impact loading conditions. Applications requiring hot...
Journal Articles
Alloy Digest (1977) 26 (10): Zn-32.
Published: 01 October 1977
... and transit components, pressure-tight castings, high-strength thin-wall castings, wear-resistant anti-galling parts, valves, industrial pulleys and sheaves, components for various types of industrial and farm equipment, lock hardware, and electrical components. Manufacturer: Eastern Alloys, Inc. Maybrook...
Journal Articles
Alloy Digest (1979) 28 (5): SA-359.
Published: 01 May 1979
... payload capability, (4) Lower fabrication costs, and (5) Reduce maintenance costs. Forms Available: Sheet Applications: Uses include components for automotive, construction and farm equipment Typical applications are bumper face bars, bumper reinforcements and brackets, wheel rims, seat components, cross...