Alloy Digest (1993) 42 (5): Ni-430.
Published: 01 May 1993
... NICROFER 5923 hMo, often called Alloy 59, was developed with extra low carbon and silicon contents and with a high alloy level of molybdenum to optimize its corrosion resistance. Nicrofer 5923hMo has a face-centered cubic structure. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1997) 46 (6): Co-103.
Published: 01 June 1997
... Conicro 5010W has a face-centered cubic structure and is a cobalt-base alloy containing chromium, tungsten, and nickel. The alloy is used in aerospace applications and in the heat-treatment industry. This datasheet provides information on composition, physical properties, and elasticity. It also...
Journal Articles
Alloy Digest (1978) 27 (9): In-2.
Published: 01 September 1978
.../cu in. (At 680F) 0.336 Indium 50 g/cu cm (At 200C) 9.32 Lead 50 Crystal structure Face-centered cubic Melting point, oC (OF) (Liquidus) 209 (408) *The manufacturer can supply C (OF) (Solidus) 180 (356 details on the identity and per- Thermal coef. expansion/oC (At 2OoC) 27x 10 -2 centages...
Journal Articles
Alloy Digest (2016) 65 (2): Co-125.
Published: 01 February 2016
... °C (2000 °F), and good sulfidation resistance. This alloy also has good forming and welding characteristics, which make it useful in fabricating gas turbine components such as combustion cans and transition ducts. The alloy has a face- center cubic structure. High tungsten content provides solid...
Journal Articles
Alloy Digest (2006) 55 (6): Co-111.
Published: 01 June 2006
... thermal treatment. After annealing with a rapid quench, the alloy has a face-centered cubic structure. Biocompatibility: Although there is no universally accepted definition for bio- compatibility of biomaterials, a medical device should be safe for its intended use. Conichrome alloy has been employed...
Journal Articles
Alloy Digest (2002) 51 (6): Ni-498.
Published: 01 June 2002
... of concentrations and at high temperatures; improved resistance to sensitization; and excellent cold and hot formability and weldability. Nimofer 6629 has a face-centered cubic structure. The alloy's balanced composition retards the kinetics of Ni4Mo phase precipitation in the tempera- ture range 700-850°C (1290...
Journal Articles
Alloy Digest (2019) 68 (5): Ni-753.
Published: 01 May 2019
... to 1000 °C (1832 °F) Good resistance to high temperature corrosion Metallurgical Structure Nicrofer 6022 hMo has a face-centered cubic structure. At temperatures in the range 600 900 °C (1112 1652 °F) intermetallic phases are precipitated after long- term exposure, as well as some carbides...
Journal Articles
Alloy Digest (1990) 39 (6): Co-68.
Published: 01 June 1990
... strengthening and aging at 1225°F (663°C) for 4 hours, air cooling results in ultra high strength. MP159 is typically supplied in the solution annealed and work strengthened condition. Microstructure: Solution annealing produces a single phase, face-centered cubic structure (TS about 125 ksi and Rockwell...
Journal Articles
Alloy Digest (1979) 28 (1): Ni-259.
Published: 01 January 1979
...-70000 15000-30000 5040 B68 max. Hard 90000- 110000 70000- 100000 15-3 B90 min. Spring 90000-l 25000 70000- 110000 15-3 B95 min. Heat Treatment: Nimag 120 is a single-phase material with a face-centered cubic structure. It cannot be hardened or strengthened by any thermal treatment, only by cold work...
Journal Articles
Alloy Digest (1979) 28 (7): Ni-261.
Published: 01 July 1979
... s ii 0 400 800 12C0 I COC 2000 Temperature, F Fit 3 - 8hoft-tima elevated-temperature tensile propwties of annealed material. Heat Treatment: Niiag 130 cannot be hardened or strengthened by any thermal treatment, only be cold working. It is a single-phase material with a face-centered cubic...
Journal Articles
Alloy Digest (1995) 44 (2): SS-582.
Published: 01 February 1995
.... Machining: Nicrofer 2509 Si 7 should be machined in the solution-treated condition. Nicrofer 2509 Si 7 is a newly developed austenitic low carbon nickel-chromium alloy containing 7 wt.% silicon and has a face-centered cubic structure. This wrought alloy exhibits excellent ductility in the solution annealed...
Journal Articles
Alloy Digest (1982) 31 (10): Ni-280.
Published: 01 October 1982
... an austenitic (Face-centered-cubic) structure. Thus it machines with a tough chip but it has a slightly better finish than most austenitic stainless steels. Workability: Hot Working: Nicrofer 3620 Cb can be forged, upset and headed satisfactorily. Hot working should be carried out in the temper- ature range...
Journal Articles
Alloy Digest (1994) 43 (10): Ni-466.
Published: 01 October 1994
...; IS0 NiCr2lMo14W3 ASTM: B366, B574. B575, B619, B622, B626 W.-Nr. 2.4602 VdTUV 479 General Characteristics: Nicrofer 5621hMoW has a face-centered cubic structure. The nickel-chromium-molybdenum alloy Nicrofer 5621 hMoW with extremely low silicon and carbon content is not prone to grain-boundaty...
Journal Articles
Alloy Digest (1996) 45 (7): Ni-513.
Published: 01 July 1996
... at temperanlres up to 150 OC (300 OF). Specification Equivalents: FraKe AFNOR NC3Ok W.-Nr. 2.4642 USA &Z Izz Spec.B 163*,B 167.B 168.B 166 Spcc. SB 163.. SB 167. SB 168. SB 166 lso bXH9Fd =-robes only General Characteristics: Nicrofer 6030 has a single-phase face-centered cubic structure and is a nickel-chromium...
Journal Articles
Alloy Digest (2011) 60 (9): SS-1101.
Published: 01 September 2011
... resistance at high temperatures Excellent life time Ease of working and processing Reduced nickel content compared to Cronifer II Metallurgical Structure. This alloy has a face-centered-cubic structure. Products Available: Cronifer 40B is available in the following standard product forms: Strip. Cold...
Journal Articles
Alloy Digest (1993) 42 (7): Ni-436.
Published: 01 July 1993
...: Nicrofer 4626MoW has a face-centered cubic structure; it is a solid solution nickel-chromium-iron alloy with molyMenum, co bah and tungsten. The ahoy has very good mechanical properties and creep resistance up to 1200°C (2200°F). This is combined with excellent resistance to oxidation, carbmization...
Journal Articles
Alloy Digest (1996) 45 (1): Ni-496.
Published: 01 January 1996
... a face-centered cubic structure. Chromium carbides, nitrides and carbonitrides can occur in the matrix. Nicrofer 7520 is readily fabricated by usual industrial procedures. Hot and cold working, however. require high-power machines. owing to the Applications: Components for indusuiaJ and aircraft gas...
Journal Articles
Alloy Digest (1982) 31 (12): Ni-281.
Published: 01 December 1982
... thermal treatment; it can be hardened only by cold working. It is a single-phase material with a face-centered cubic structure. Machinability: RA 200 has machining characteristics quite similar 10 mild steel; however, it is somewhat harder and tougher. For RA 200 lower speeds and feeds are suggested than...
Journal Articles
Alloy Digest (1964) 13 (2): Mg-56.
Published: 01 February 1964
.... Workability: Cast ingots can be extruded. hammer or press forged or rolled directly into sheers. Sheer stock exhibits a high degree of formability at room temperature or slightly elevated temperatures. Because of its body-centered cubic structure (in contrast with the hexagonal-close packed alloys), LA141A...
Journal Articles
Alloy Digest (2012) 61 (7): Ni-698.
Published: 01 July 2012
... temperature is austenite (face centered cubic). Available Products: Plate and sheet Applications: This alloy is fit for various applications in chemical, petrochemical, energy, and environmental energy fields: e.g., sulfuric acid cooler, reactors for hydrofluoric acid, acetic acid, and acetic and acetic...