1-20 of 540 Search Results for

fabricated components

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2008) 57 (11): SA-587.
Published: 01 November 2008
... Domex 420 MC is a hot-rolled, high-strength low-alloy (HSLA) steel for cold forming operations. It is available in thicknesses of 1.80-15.00 mm. The alloy meets or exceeds the requirements of S420MC in EN 10149-2. Applications include a wide range of fabricated components and steel structures...
Journal Articles
Alloy Digest (2009) 58 (3): SA-594.
Published: 01 March 2009
... Domex 550MC is a hot-rolled, high-strength low-alloy (HSLA) steel for cold forming operations. It is available in thicknesses of 2.00-12.80 mm. The alloy meets or exceeds the requirements of S550MC in EN 10149-2. Applications include a wide range of fabricated components and steel structures...
Journal Articles
Alloy Digest (2009) 58 (1): SA-591.
Published: 01 January 2009
... Domex 460 MC is a hot-rolled, high-strength low-alloy (HSLA) steel for cold forming operations. It is available in thicknesses of 2.00-13.00 mm. The alloy meets or exceeds the requirements of S460MC in EN 10149-2. Applications include a wide range of fabricated components and steel structures...
Journal Articles
Alloy Digest (2009) 58 (2): SA-592.
Published: 01 February 2009
... Domex 500MC is a hot-rolled, high-strength low-alloy (HSLA) steel for cold forming operations. It is available in thicknesses of 2.00-13.00 mm. The alloy meets or exceeds the requirements of S500MC in EN 10149-2. Applications include a wide range of fabricated components and steel structures...
Journal Articles
Alloy Digest (1986) 35 (8): SA-421.
Published: 01 August 1986
... be fabricated readily. Applications include weight-sensitive components subject to high stress such as frames for large off-highway haulers. This datasheet provides information on composition, physical properties, microstructure, elasticity, and tensile properties as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (2003) 52 (10): SA-522.
Published: 01 October 2003
... by being one of a family of alloy that can be fabricated readily. Applications include weight-sensitive components subject to high stress such as frames for large off-highway equipment. This datasheet provides information on composition, physical properties, microstructure, elasticity, and tensile...
Journal Articles
Alloy Digest (2003) 52 (12): Ni-618.
Published: 01 December 2003
... RA718 is a nickel alloy precipitation hardened by gamma prime and double prime. It is readily fabricated and is weldable even in the aged condition. The alloy is used for gas turbine components at temperatures up to 650 deg G (1200 deg F) as well as for cyogenic equipment. This datasheet provides...
Journal Articles
Alloy Digest (1997) 46 (8): SA-486.
Published: 01 August 1997
... Oregon Formalloy 400 (0.17C-1.50Mn maximum)combines through hardness and toughness with superior flame cutting, forming, and welding characteristics not found in typical abrasion resistant (AR) steels. This user-friendly grade permits more latitude in design and fabrication for such uses as dump...
Journal Articles
Alloy Digest (1997) 46 (9): SA-487.
Published: 01 September 1997
..., bucket components, and mining and construction equipment Formalloy 500 is a trademark of Oregon Steel Mills. Chemical Composition, wt.Ok: Carbon Manganese Phosphorus SUlfiU Silicon chromium Molybdenum Boron 0.30 max. 1.15 max. 0.015 max. 0.005 max. 0.60 max. 0.65 max. 0.40 max. o.ooo5 min. Fabricability...
Journal Articles
Alloy Digest (1967) 16 (9): Cb-12.
Published: 01 September 1967
... Columbium WC-103 is a columbium-base alloy having good high temperature strength, good weldability and fabricability. It is recommended for high performance rocket engine components for temperatures up to 2800 F for controlled periods of time. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1968) 17 (1): Cb-14.
Published: 01 January 1968
... Columbium SCB-291 is a columbium-base alloy having excellent high temperature properties and good fabricability. It is recommended for nuclear reactors, space vehicles, jet and missile components. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (1963) 12 (5): SA-146.
Published: 01 May 1963
... Udimet B is a series of four 18%-nickel steels of ultra high strength and good toughness at room and at elevated temperatures. They are easily fabricated and weldable, and are recommended for the aircraft and missile industries for high temperature components. This datasheet provides information...
Journal Articles
Alloy Digest (1966) 15 (10): Cb-11.
Published: 01 October 1966
... COLUMBIUM-1% Zr is a readily fabricable, moderate strength columbium-base alloy for high temperature service. It is double consumable-electrode vacuum are melted. It is recommended for missiles, spacecraft and high temperature components. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1978) 27 (4): SA-345.
Published: 01 April 1978
... sizes produced by the manufacturer. It is an excellent choice for fabrication of structural components or for use in pressure tubing subjected to a low-temperature environment. *STROLOY is a registered trademark of Babcock and Wilcox. Composition: Physical Constants: (Approximate) Range Density, lb/cu...
Journal Articles
Alloy Digest (1981) 30 (11): Ni-272.
Published: 01 November 1981
... stainless steels and heat-resisting alloy components. Major application is in fabricating high-temperature jet-engine parts. This datasheet provides information on composition, physical properties, microstructure, tensile properties. It also includes information on heat treating and joining. Filing Code: Ni...
Journal Articles
Alloy Digest (1982) 31 (11): SS-416.
Published: 01 November 1982
... JESSOP JS15Cr-5Ni is a martensitic, precipitation-hardening, chromium-nickel-copper stainless steel. It offers high strength and hardness in combination with good resistance to corrosion. Typical applications include aircraft components and a variety of fabricated parts for use in corrosive, high...
Journal Articles
Alloy Digest (1979) 28 (3): SA-356.
Published: 01 March 1979
... ARMCO FORMABLE 50 HR is a hot-rolled high-strength low-alloy steel that provides excellent ductility, weldability and edge-tear resistance at a minimum yield strength of 50,000 psi (345 MPa). It has unusually good fabricating properties that are the result of closely controlled processing...
Journal Articles
Alloy Digest (1979) 28 (5): SA-359.
Published: 01 May 1979
... sheared edges bent with the shear burr in tension to simulate press brake for- ming in the shop. Armco FORMABLE 70 HR forms similar to ASTM A607, and performs better in some drawing operations In spite of its high strength, FORMABLE 70 HR can be fabricated satisfactorily for parts and components requiring...
Journal Articles
Alloy Digest (1980) 29 (12): Fe-61.
Published: 01 December 1980
... CARPENTER Consumet Electrical Iron is a double-melted low-carbon iron recommended for fabricating or machining of thin-wall parts that must be vacuum tight. Melting and manufacture are controlled closely to provide freedom from porosity and internal defects. This iron is recommended for components...
Journal Articles
Alloy Digest (1981) 30 (5): SA-380.
Published: 01 May 1981
... ARMCO SSS 100A is a low-carbon, fine-grained, quenched-and-tempered alloy steel. It is strong, tough and readily fabricated with equipment and facilities suited to its high strength. It has a minimum yield strength of 100,000 psi. Among its many uses are structural components in heavy-duty...