Journal Articles
Alloy Digest (1990) 39 (8): Cp-10.
Published: 01 August 1990
... International compressive strength KEVLAR 49 machinability physical properties shear strength tensile properties - DIGEST- I 1 AUGUST 1990 DATA ON WORLD WIDE METALS AND ALLOYS acspvnjlMl99o.A5yc P-w Alg DipI. Inc l201-aala1 ~yp~tobedk 2? CanHeld SUuU. Orange, NJ. 07WY I USA KEVLAFP49 Fabric...
Journal Articles
Alloy Digest (1993) 42 (5): Ni-432.
Published: 01 May 1993
... Hastelloy Alloy G-30 filler metal is used as matching composition filler metal for fabrication of Hastelloy G-30 wrought and cast products and as filler metal for fabrication of G/G-3 alloy wrought products. It is also used for weld repair of high chromium castings and for weld overlay cladding...
Journal Articles
Alloy Digest (1981) 30 (11): Cb-10.
Published: 01 November 1981
... of fabrication associated with columbium. Fansteel 80 Metal can be fabricated easily at room temperature and high-quality ductile welds are possible. Its applications include nuclear, liquid metal loops and structures for high-temperature environments. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1999) 48 (7): Ni-557.
Published: 01 July 1999
... Haynes alloy 75 is an 80 nickel-20 chromium alloy with both good oxidation resistance and good mechanical properties at high temperatures. It is amenable to all forms of fabrication and welding. A typical application for sheet metal is fabrications in gas turbine engines. This datasheet provides...
Journal Articles
Alloy Digest (1973) 22 (11): Cb-20.
Published: 01 November 1973
... FANSTEEL 291 METAL is a columbium-base alloy that can be readily fabricated, machined and welded. It is used in the high-temperature range 2800-3500 F where excellent strength-to-weight ratio can be used to advantage. It is also used in the lower temperature range 2000-2700 F because of its...
Journal Articles
Alloy Digest (2015) 64 (9): Ni-723.
Published: 01 September 2015
... Pyromet alloy 706 has similarities to alloy 718, but improves fabricability and welding. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming...
Journal Articles
Alloy Digest (1991) 40 (6): Cu-561.
Published: 01 June 1991
... Copper C10300 combines good electrical conductivity with excellent hot and cold fabricability and joining characteristics (welding and brazing). This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes...
Journal Articles
Alloy Digest (1979) 28 (6): SS-366.
Published: 01 June 1979
... CARPENTER STAINLESS 18Cr-2Ni-12Mn is a high-manganese, nitrogen-strengthened austenitic stainless steel with an excellent combination of toughness, ductility, strength, fabricability and corrosion resistance. It provides substantially higher yield and tensile strengths than AISI Type 304...
Journal Articles
Alloy Digest (2012) 61 (2): SS-1115.
Published: 01 February 2012
... Kubota Alloy HF is a heat-resisting stainless steel casting suitable for long-term service at temperatures between 538-871 deg C (1000-1600 deg F). It is frequently used as an alternative to the 2.25%Cr-1%Mo steels due to its greater ease of fabrication. This datasheet provides information...
Journal Articles
Alloy Digest (2013) 62 (2): SS-1135.
Published: 01 February 2013
... fabricability of this alloy, combined with its basic corrosion resistance and economy have significantly broadened the utility of ATI 409HP stainless steel. ATI 409HP consists of four grades: UNS S40900, S40910, S40920, and S40930. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2019) 68 (9): Ni-755.
Published: 01 September 2019
... Haynes HR-233 has excellent oxidation resistance and improved fabricability and weldability. The alloy can be used to 1150 deg C (2100 deg F). This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high...
Journal Articles
Alloy Digest (2019) 68 (11): Cu-899.
Published: 01 November 2019
... Wieland-K57 (UNS C70350) is copper alloyed with low nickel for good fabricability for parts in the electrical industry. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength as well as fatigue. It also includes...
Journal Articles
Alloy Digest (2019) 68 (12): Cu-901.
Published: 01 December 2019
... Wieland-K73 (UNS C19005) is copper alloyed with low nickel for good fabricability for parts in the electrical industry. This datasheet provides information on composition, physical properties, and bend strength as well as fatigue. It also includes information on corrosion resistance as well...
Journal Articles
Alloy Digest (2018) 67 (3): SA-813.
Published: 01 March 2018
... ArcelorMittal 9% nickel alloy steel plates are for use in the water quenched and tempered or double normalized condition. They are intended for the fabrication of welded pressure vessels. This datasheet provides information on composition, physical properties, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1978) 27 (4): SA-345.
Published: 01 April 1978
... STROLOY 787 is an age-hardenable, high-strength, low-alloy steel with excellent low-temperature toughness and weldability. It is suitable for mechanical or pressure tubing applications in most of the tube sizes produced by the manufacturer. It is an excellent choice for fabrication of structural...
Journal Articles
Alloy Digest (1978) 27 (6): CS-73.
Published: 01 June 1978
... Uniflux V70 is a continuous flux-cored welding electrode (wire) that is used to deposit carbon steel weld metal. Welding is protected by a shielding atmosphere of either 75% argon-25% carbon dioxide or 100% carbon dioxide. Uniflux V70 is used widely in shipbuilding and other fabricating industries...
Journal Articles
Alloy Digest (1989) 38 (6): Cu-547.
Published: 01 June 1989
... COPPER No. C15715 is a dispersion hardened copper fabricated by powder metallurgy techniques. Its electrical conductivity is 92% IACS and its annealed tensile strength (0.050 in. diameter wire) is 52000-66000psi, depending on annealing temperature. This datasheet provides information...
Journal Articles
Alloy Digest (1989) 38 (9): Cp-2.
Published: 01 September 1989
... K-KARB (Carbon-Carbon) is a graphitized structural graphite fabricated from a graphitized cloth precursor. The layers of graphitized cloth are laminated and bonded together with a graphitic matrix forming a light weight, high strength graphite. This datasheet provides information on physical...
Journal Articles
Alloy Digest (1989) 38 (12): Cu-544.
Published: 01 December 1989
... COPPER No. C15700 is a dispersion hardened copper fabricated by powder metallurgy techniques. It has good strength and electrical conductivity. It has applicability at elevated temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1990) 39 (11): Cp-11.
Published: 01 November 1990
... AVIMID N / GRAPHITE is a carbon-fiber/polyimide, high-temperature composite tooling material developed to fabricate quality parts from prepregs based on thermoplastics. This datasheet provides information on physical properties, and tensile properties as well as fracture toughness. It also...