Alloy Digest (2009) 58 (11): Al-426.
Published: 01 November 2009
... Alcan 2196 T8511 is produced as extrusions for applications where compression is critical. 2196 Al-Li alloy, with high strength and elastic modulus but low density, is used for floor beams, seat tracks, welded applications, and wing stringers. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2005) 54 (9): Al-397.
Published: 01 September 2005
..., each 0.05 max 0.05 max 0.05 max Others, total 0.15 max 0.15 max 0.15 max Balance Aluminum Aluminum Aluminum Mechanical Properties: S-basis properties for alloys 7055, 7178, and 7075 are compared in Tables 1 and 2. The fracture toughness values measured for the 7055-T74511 extrusions exceed those...
Journal Articles
Alloy Digest (2010) 59 (2): Al-428.
Published: 01 February 2010
... The 7xxx series alloys contain zinc as the main alloying element, usually in combination with magnesium and copper. Alcoa’s high-strength 7055 alloy is supplied as plate and extrusions and used for compressive strength applications. This datasheet provides information on composition, tensile...
Journal Articles
Alloy Digest (2015) 64 (10): Mg-81.
Published: 01 October 2015
... Elektron 675 is an extrusion alloy designed for high strength to 250 deg C (482 deg F). This datasheet provides information on physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (1992) 41 (2): Al-321.
Published: 01 February 1992
... AA 6463 is a heat treatable extrusion alloy used for architectural and trim sections. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (1975) 24 (6): Zn-19.
Published: 01 June 1975
... NJZ ALLOY No. 5 is produced from high-grade zinc with additions of lead and cadmium. It is primarily used for impact extrusions and has medium hardness and good resiliency. Its applications include such items as battery cans and chemical containers. This datasheet provides information...
Journal Articles
Alloy Digest (1967) 16 (3): Al-164.
Published: 01 March 1967
... BA.704 is a heat treatable aluminum extrusion alloy having high tensile and fatigue strengths. It is recommended for aircraft components, gears, fittings and machinery parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1967) 16 (12): Al-170.
Published: 01 December 1967
... AND ALLOYS Psuisu by . . Wi--9AuqrW-I= Upper Moatdsir, New m ALCAN 8335 (Extrusion Alloy) Alcan B33S is an aluminum alloy recommended for architectural shapes requiring hard, corrosion resistant, colored finishes. It contains enough magnesium to render it heat treatable. Composition: Magnesium Silicon Copper...
Journal Articles
Alloy Digest (2005) 54 (12): Al-398.
Published: 01 December 2005
... (0.095) Mechanical Properties: Modulus of elasticity in tension, GPa (106 psi) 78 (11.3) The data in Table 1 and Fig. 1 3 show how the two tempers com- pare in static, damage tolerant, and corrosion properties. The T83 temper can meet or exceed the strength of 7075-T6511 and 7050- T76511 extrusions...
Journal Articles
Alloy Digest (2006) 55 (10): Al-401.
Published: 01 October 2006
... Alcoa extrusion alloy 2026 was developed as an improvement over 2024 and 2224 extrusions in aerospace structural applications where the governing selection criteria are high damage tolerance, good fatigue resistance, and a high degree of manufacturability. In addition to improved damage tolerance...
Journal Articles
Alloy Digest (2009) 58 (6): Al-422.
Published: 01 June 2009
... composition compressive strength corrosion-resistant alloys fatigue properties physical properties tensile properties workability ALCOA 2099-T83 and 2099-T8E67 (Aluminum Extrusion Alloy) This is an aluminum-lithium alloy developed for aerospace applications. Lithium lowers the density. Chemical...
Journal Articles
Alloy Digest (1957) 6 (1): Mg-30.
Published: 01 January 1957
... WHITE LIGHT-MF is a wrought magnesium-base alloy that does not respond to age-hardening heat treatment for increased hardness and strength. It is a general purpose extrusion alloy for applications where medium strength and economy are prime factors. This datasheet provides information...
Journal Articles
Alloy Digest (1959) 8 (4): Al-77.
Published: 01 April 1959
... NORAL 62S is an aluminum extrusion alloy that responds to an age hardening heat treatment. It has good strength and excellent fabricating characteristics. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive, shear, and bearing...
Journal Articles
Alloy Digest (1980) 29 (3): Al-181.
Published: 01 March 1980
... ALUMINUM 6070 is a high-strength, heat-treatable extrusion alloy. It was developed for structural applications. It has high resistance to general corrosion and stress-corrosion cracking. Its many applications include marine hardware, electric-transmission towers and bridges. This datasheet...
Journal Articles
Alloy Digest (1972) 21 (1): Co-64.
Published: 01 January 1972
... BUDERUS 58-28 (Extrusion Die Alloy) BUDERUS 58-28 is a cobalt alloy having high strength and excellent toughness at elevated temperatures. Composition: Nominal Physical Constants: Thermal coef. expansion/o(: Carbon 0.20 Cobalt 58 Chromium 28 Molybdenum 5.5 Iron Remainder 20 to looe 20 to 4OOoC 20 to 6OOoC...
Journal Articles
Alloy Digest (1959) 8 (8): Mg-43.
Published: 01 August 1959
... MAGNESIUM AZ61A is a magnesium extrusion alloy having a strength level between that of AZ31B and ZK60A. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive, shear, and bearing strength as well as fatigue. It also...
Journal Articles
Alloy Digest (1962) 11 (9): Mg-53.
Published: 01 September 1962
... Alloy MAGNESIUM AZ31B SEPTEMBER 1962 -DATA ON WORLD WIDE METALS AND ALLOYS MAGNESIUM AZ31 B Publiibcd by Engineering Alloys Digest. Inc. (Magnesium Sheet, Plate and Extrusion Alloy) Upper MontcI:ir, New Jersey Magnesium AZ31B Composition: Aluminum zinc Manganese Silicon Copper Nickel Iron Calcium Others...
Journal Articles
Alloy Digest (1952) 1 (1): Mg-1.
Published: 01 September 1952
... Dowmetal ZK60A is an ageable extrusion alloy for use where high strength magnesium extrusions with good toughness are required. It has small grain size, low notch sensitivity and a relatively high resistance to stress corrosion. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1963) 12 (8): Al-128.
Published: 01 August 1963
... machinability physical properties tensile properties workability I Filing Code: Al-128 Aluminum Alloy I ALCAT AUGUST 1963 I -DATA ON WORLD _ _ __ - __ _ __ _- _ _ _ ALCAN 8515 (Aluminum Extrusion Alloy) Prblisbed by Engineering Alloys Digest, Inc. upper Montclair, New J~#I Alcan B51S is a medium strength...
Journal Articles
Alloy Digest (1966) 15 (5): Mg-59.
Published: 01 May 1966
... shear strength tensile properties workability ~MAGNEMJM HM 31~1 I -DATA ON WORLD Filing Code: Mg-59 Magnesium Alloy MAY 1966 WIDE METALS AND ALLOYS MAGYESIUM HM31A (Magnesium Extrusion Alloy) Pnblisbd by Engineering Alloys Digest, Inc. Upper Montclair, New Jay Magnesium HM31A is a magnesium-thorium...