Alloy Digest (1964) 13 (1): TS-142.
Published: 01 January 1964
... CROMO-N tool steel is a low-carbon, high-chromium grade, specially developed to provide optimum resistance to heat-checking during service at elevated temperatures. It is recommended for aluminum die casting dies, extrusion press tooling, aluminum and copper forging dies, and mandrels...
Journal Articles
Alloy Digest (1973) 22 (2): TS-250.
Published: 01 February 1973
... operations use a sulphurized mineral oil as the cutting fluid. Recommended cutting speeds and feeds are given in Table 4. Applications: Hot-work applications involving severe shock and drastic temper- ature changes, extrusion press tooling, hot-work dies and backers, dummy blocks, bolt headers, hot-work...
Journal Articles
Alloy Digest (1957) 6 (5): TS-58.
Published: 01 May 1957
...-45 Hot gripper dies - C48-52 Hot press dies C43-48 Hot forging dies C40-45 Extrusion dies, (aluminum) C48-52 Extrusion press liners C41-43 Extrusion press rams - C44-46 Billets, bars and forgings. Applications: Extrusion dies, extrusion press rams, forging machine dies, extrusion press liners, back...
Journal Articles
Alloy Digest (1971) 20 (11): Cu-245.
Published: 01 November 1971
... contributes to its excellent hot working properties. However, it has only fair cold working properties. The alloy can be joined by several of the standard welding processes and by soldering or brazing. It is used for a variety of press-forged parts and for architectural extrusions. Forms Available: Bar, rod...
Journal Articles
Alloy Digest (1967) 16 (2): Mo-8.
Published: 01 February 1967
... of arc-cast TZM, which has the same composition. Suggested uses are dies for extrusion, hot pressing, and die casting and for a wide structural components that operate at high temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1972) 21 (1): Cu-249.
Published: 01 January 1972
... part soluble oil. Workability: COPPER ALLOY No. 485 can be hot worked readily in the temperature range of 1200 to 1500°F by press forging, rolling and extrusion. Based on such variables as pressure, die wear, and hot plasticity, the alloy has a forgeability rating of 90 (Forging Brass is rated 100...
Journal Articles
Alloy Digest (2018) 67 (1): TS-746.
Published: 01 January 2018
...) 48 650 ºC (1202 ºF) 38 General Characteristics Al extrusion die steel and hot-working press die steel that has better high-temperature strength and softening resistance than DAC. This alloy has higher resistance to softening by multiple nitriding for extrusion dies. See Fig. 1 for a comparison...
Journal Articles
Alloy Digest (1996) 45 (9): Be-8.
Published: 01 September 1996
...-beryllium alloys are sim- pler to use and easier to fabricate. Tooling designed for aluminum Products Available: Hot isostatic pressed biiek extruded bar, and rolled sheets. Producer: Brush Wellman, Inc. Elmore. OH 43416-9502 (419) 862-4171 (419) 8624174 (fax) ...
Journal Articles
Alloy Digest (1968) 17 (12): Mg-66.
Published: 01 December 1968
...: In forging, maximum properties are obtained by working at the maximum amount and at minimum temperatures, but is limited by the power of the forge. In hammer forging, a temperature below 425°C (738°F) will give cold cracking. Press forging can be done as low as 400°C (752°F) if the material and the tools...
Journal Articles
Alloy Digest (1969) 18 (1): Co-57.
Published: 01 January 1969
... DELORO STELLITE 4 is a cobalt-base alloy having high wear resistance, good high temperature strength. It is a machinable casting alloy recommended for hot extrusion and pressing dies, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Journal Articles
Alloy Digest (2010) 59 (3): TS-687.
Published: 01 March 2010
... and forming, cold extrusion, deep drawing, and powder pressing. UDDEHOLM VANCRON 40 (Nitrided Powder Metal Tool Steel) UDDEHOLM VANCRON 40 Chemical Composition, wt (Typical Analysis) Carbon 1.1 Silicon 0.5 Manganese 0.4 Chromium 4.5 Molybdenum 3.2 Tungsten 3.7 Vanadium 8.5 Nitrogen 1.8 Iron bal Physical...
Journal Articles
Alloy Digest (1957) 6 (1): Mg-30.
Published: 01 January 1957
... WHITE LIGHT-MF is a wrought magnesium-base alloy that does not respond to age-hardening heat treatment for increased hardness and strength. It is a general purpose extrusion alloy for applications where medium strength and economy are prime factors. This datasheet provides information...
Journal Articles
Alloy Digest (2017) 66 (11): TS-743.
Published: 01 November 2017
... Characteristics: Hot work tool steel with higher toughness than DAC for Al extrusion dies with high hardness or hot forging press dies with good crack resistance. Fig. 3 Transition property of Charpy impact value Fig. 4 Summary of properties Fig. 5 Quenched and tempered hardness curve Fig. 6 Quenching speed vs...
Journal Articles
Alloy Digest (1966) 15 (10): Al-159.
Published: 01 October 1966
...%) R.T. 50400 34500 Elongation 9c in 2 6.4 Notched Tensile Suength psi 53400 Notched-Unnotched Tensile Strength Ratio 1.06 -320 57600 42600 4.4 56300 0.98 Table4 - LONGITIJDINALPROPERTIESOF EXTRUSIONS ( A inch wall thickness, fully heat treated) Solution Treated Press Quenched and Aged and Aged Tensile...
Journal Articles
Alloy Digest (2008) 57 (3): TS-662.
Published: 01 March 2008
... increments Bright steel Round 2 17 diameter ground, 2 30 diameter drawn Sheets Rectangular Width up to 2000, thickness 2 20 Cold rolled Round Up to approximately 500 diameter Applications: This tool steel is used for die casting tools, hot pressing tools, and extrusion tools, all mainly for heavy metals...
Journal Articles
Alloy Digest (2000) 49 (10): TS-582.
Published: 01 October 2000
... to a hardness of approximately 200 BHN. Applications: Some typical hot work applications for Magnadie steel include dummy blocks and mandrels for brass and aluminum extrusion, extrusion dies for aluminum and magnesium, hot press dies, punches and dies for shell piercing, die inserts for forging dies, and hot...
Journal Articles
Alloy Digest (1966) 15 (3): TS-177.
Published: 01 March 1966
... with intermediate cooling to room temper- ature is always recommended. This steel is usually tempered to a hardness of Rockwell C48-52. Hot pressing tools for brass are cemper- ed to about Rockwell C50-52 and cores for die casting dies to about Rockwell C48-50. Machinability: This steel in the annealed condition...
Journal Articles
Alloy Digest (1967) 16 (4): TS-191.
Published: 01 April 1967
... PRESSURDIE-1 is an air-hardening hot work tool and die steel having high heat resistance and good high temperature strength properties. It is recommended for die casting dies, extrusion and forging dies. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (2017) 66 (12): TS-745.
Published: 01 December 2017
... Characteristics: Excellent heat crack and wear resistance at elevated temperature. Steel for precision die casting and hot press die. See Fig. 1 for a comparison on the characteristics of YSS hot work tool steels. Applications: General use in hot forging dies with hardness HRC 45 50. General use in extrusions...
Journal Articles
Alloy Digest (1968) 17 (3): Al-173.
Published: 01 March 1968
... is normally accomplished by quenching in air or water from the extrusion temperature at the press. The practices listed above are satisfactory for furnace heat treatment by the user.) Machinability: Cutting tools should have large top and side rake angles, smooth surfaces, keen cutting edges, and ample chip...