Alloy Digest (1967) 16 (6): TS-194.
Published: 01 June 1967
... LUMDIE is a tungsten-chromium hot work steel recommended for die casting dies, forging and extrusion dies. It is an air hardening steel having high temperature properties and heat resistance. It is particularly suited for long run die casting dies, brass forging dies, and for various extrusion...
Journal Articles
Alloy Digest (1989) 38 (2): TS-496.
Published: 01 February 1989
... are hot-punch tools, forging dies and inserts, brass extrusion dies, permanent molds for brass casting and hot-extrusion die inserts for steel. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on high...
Journal Articles
Alloy Digest (1982) 31 (7): TS-401.
Published: 01 July 1982
... are hot-punch tools, forging dies and inserts, brass extrusion dies, permanent molds for brass casting and hot-extrusion die inserts for steel. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat...
Journal Articles
Alloy Digest (1964) 13 (8): TS-150.
Published: 01 August 1964
... Seneca Hot Die is a tungsten-chromium-vanadium type hot work steel having good red hardness and abrasion resistance. It is recommended for forging dies, copper extrusion dies, die casting dies, and other hot work tools and dies. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1967) 16 (9): TS-197.
Published: 01 September 1967
... Thermold 75 is a chromium-molybdenum-cobalt hot work steel that has outstanding resistance to softening when tempering, and also very good thermal fatigue characteristics. It is recommended for aluminum die casting dies, forging dies and extrusion dies. This datasheet provides information...
Journal Articles
Alloy Digest (1981) 30 (4): TS-381.
Published: 01 April 1981
... be water cooled in service. It is suitable for hot-work applications involving severe conditions of shock and sudden temperature changes. Its many applications include hot shear blades, forging dies, extrusion dies, punches and other types of hot-work tools. This datasheet provides information...
Journal Articles
Alloy Digest (1985) 34 (5): TS-440.
Published: 01 May 1985
... for Hotform Ultra include die-casting dies, core pins and inserts, piercing dies and hot-extrusion dies. This datasheet provides information on composition and physical properties. It also includes information on wear resistance as well as forming, heat treating, machining, and joining. Filing Code: TS-440...
Journal Articles
Alloy Digest (1985) 34 (6): TS-442.
Published: 01 June 1985
..., extrusion dies, hot header dies, mandrels, punches and piercing tools. Consult the manufacturer for specific recommendations. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on high temperature...
Journal Articles
Alloy Digest (1985) 34 (9): TS-446.
Published: 01 September 1985
...-work applications where machinability is of primary importance. Its many uses include forging and heading dies, aluminum extrusion dies, mandrels and mold dies for plastics. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information...
Journal Articles
Alloy Digest (1985) 34 (12): TS-451.
Published: 01 December 1985
... of applications includes can dies, coining dies, extrusion dies, slitters, roofing knives, burnishing tools and punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-451...
Journal Articles
Alloy Digest (1986) 35 (1): TS-453.
Published: 01 January 1986
... checking and may be water cooled in service. It is suitable for hot-work applications involving severe conditions of shock and sudden temperature changes. Its many applications include hot shear blades, forging dies, extrusion dies, punches and other types of hot-work tools. This datasheet provides...
Journal Articles
Alloy Digest (1986) 35 (12): TS-467.
Published: 01 December 1986
... NU-DIE XL is a manufactured to meet the demanding specifications for long-run die-casting dies for aluminum. Sound centers are produced in both large and smaller sizes. Its many applications include die-casting dies, die inserts, cores and extrusion dies for aluminum and magnesium. This datasheet...
Journal Articles
Alloy Digest (1965) 14 (5): Co-44.
Published: 01 May 1965
... Deloro-Stellite-7 is a cobalt base casting alloy possessing excellent corrosion resistance and high temperature strength together with good ductility and excellent resistance to thermal shock. It is recommended for gas turbine blades, brass casting dies and extrusion dies. This datasheet provides...
Journal Articles
Alloy Digest (1972) 21 (1): Ni-167.
Published: 01 January 1972
... PYROTOOL 7 has been designed to display high tensile and yield properties with good hardness at temperatures up to 1300 F. It is used for high-temperature tooling, extrusion dies, forging dies, rams, mandrels, holders, rings, dummy blocks, liners, etc. This datasheet provides information...
Journal Articles
Alloy Digest (1974) 23 (9): Ni-208.
Published: 01 September 1974
... HAYNES Alloy No. 273 is a nickel-base, hard-facing alloy developed to provide extra life for hot-working equipment such as hot-forging dies, hot-shear blades and hot-extrusion dies. It is deposited by using a composite electrode with nickel-base core and the balance of the alloying elements...
Journal Articles
Alloy Digest (1967) 16 (4): TS-192.
Published: 01 April 1967
... Mustang-LC is a tungsten-molybdenum high-speed steel specially developed for hot work applications requiring long die life. It is recommended for hot forming and swaging dies, hot extrusion dies, hot punches, etc. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1967) 16 (11): TS-199.
Published: 01 November 1967
... Böhler (or Boehler) WPZ is a high alloy special steel designed to withstand the optimal requirements made on hot work steel. It is recommended for rod and tube extrusion dies, and for injection and compression molding dies. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1969) 18 (9): TS-223.
Published: 01 September 1969
... HALCOMB 425 is a hot work tool steel having excellent resistance to shock and abrasion at elevated temperatures. It is recommended for brass and copper extrusion dies, forging dies and inserts, and hot punches. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1970) 19 (2): TS-227.
Published: 01 February 1970
... THERMOLD-H23 is a chromium-tungsten hot work tool and die steel characterized by high strength at elevated temperatures and good resistance to heat checking. It is recommend for extrusion dies and die casting dies. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1971) 20 (2): Ni-161.
Published: 01 February 1971
... PYROTOOL W has been designed to possess high strength and hardness at temperatures up to 1500 F (816 C). Applications include high-temperature tooling, extrusion dies, dummy blocks, rings, holders, forging dies and mandrels. This datasheet provides information on composition, physical properties...