Alloy Digest (1998) 47 (9): Ni-544.
Published: 01 September 1998
... INCOCLAD 671/800HT is produced by co-extruding a duplex billet with Incoloy alloy 800HT as the substrate and Inconel alloy 671 as the corrosion resistant cladding. This datasheet provides information on composition and physical properties. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (2005) 54 (4): Al-392.
Published: 01 April 2005
... Alloy 6063, one of the most popular alloys in the 6000 series, provides good extrudability and a high-quality surface finish. Alloy 6063 is used in a variety of architectural applications. This datasheet provides information on composition, physical properties, hardness, tensile properties...
Journal Articles
Alloy Digest (2005) 54 (5): Al-393.
Published: 01 May 2005
... is considered better than alloy 6061-T6 when 6005 and 6105 are in the T5 temper. Specification Equivalents: UNS A96005 UNS A96105 ALCOA 6005 AND 6105 Filing Code: Al-393 Aluminum May 2005 ALCOA 6005 AND 6105 (Extruded Aluminum Alloys) Alloys 6005 and 6105 belong to the 6xxx series of aluminum alloys...
Journal Articles
Alloy Digest (2005) 54 (6): Al-394.
Published: 01 June 2005
... for 6xxx series alloys are shown in Fig. 1 for several tempers. Machinability: The alloy has good machinability and is considered best when in the T5 or T6 tempers. Chip breakers should be used. ALCOA 6082 Filing Code: Al-394 Aluminum June 2005 ALCOA 6082 (Extruded Aluminum Alloy) Alloy 6082 is part...
Journal Articles
Alloy Digest (2005) 54 (7): Al-395.
Published: 01 July 2005
... (1350) General Characteristics: Alcoa Engineered Products markets several alloys in the 1xxx series for many specialty applications. The alloys are non-heat- treatable, have the highest purity of aluminum compared to other series of aluminum alloys, and are offered as extruded sections with a minimum...
Journal Articles
Alloy Digest (2005) 54 (8): Al-396.
Published: 01 August 2005
... A96101 General Characteristics: Alloy 6101 is prominent in the line of bus conductor extruded products. As a heat treatable wrought alloy, it is best suited for applications involving moderate strength and maximum electrical conductivity. It is similar to alloy 6063, but with minor chemistry changes...
Journal Articles
Alloy Digest (2006) 55 (1): Al-281.
Published: 01 January 2006
... the T6/T6511 temper, chips from machining (particularly turning and drilling) are difficult to break. Chip breakers are recommended, and special machining ALCOA 6061 Filing Code: Al-281 Aluminum Original May 1987 Revised January 2006 ALCOA 6061 (Extruded Precipitation-Hardenable Aluminum Alloy) Alloy...
Journal Articles
Alloy Digest (1969) 18 (3): Cu-197.
Published: 01 March 1969
... METALS AND ALLOYS Psblisbd by Engineering Alloys Digest, Inc. Upper Montclair, New Jersey AMPCOLOY* 666 (Extruded Bearing Bronze Alloy) Ampcoloy 666 is a manganese-bronze ahoy developed for long wearing applications in bushings, gears, cams, etc. It has good non-gall@ characteristics, good corrosion...
Journal Articles
Alloy Digest (1962) 11 (4): Cu-116.
Published: 01 April 1962
... Ampcoloy 405 is a high strength, ductile, corrosion and wear resistant copper alloy available in extruded solid bar form for gears, valve seats, marine hardware, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1965) 14 (10): Cu-156.
Published: 01 October 1965
... Wearite 4-13 is a corrosion and wear resistant extruded aluminum bronze preheat treated to high strength and hardness levels. It is recommended for sliding contact applications where wear resistance and non-galling characteristics are desired. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2008) 57 (9): Al-417.
Published: 01 September 2008
... joinability machinability physical properties tensile properties workability ALCAN 2024-T3, T351X (Aluminum-Copper-Magnesium Alloy Extruded Bar) This datasheet covers Alcan 2024 alloy in T3 and T351x tempers. The alloy possesses good damage tolerance. Chemical Composition, wt (Typical) Silicon 0.50 max...
Journal Articles
Alloy Digest (2009) 58 (8): Al-424.
Published: 01 August 2009
... International ALCAN 2027 T3511 chemical composition corrosion-resistant alloys fatigue properties heat treatability physical properties tensile properties workability ALCAN 2027 T3511 (Aluminum-Copper-Magnesium, Manganese-Zirconium Alloy Extruded Bar) This datasheet covers Alcan 2027 T3511...
Journal Articles
Alloy Digest (2010) 59 (9): Al-431.
Published: 01 September 2010
... (Extruded Rod & Bar) KAISER ALLOY 6005 Chemical Composition, wt (Nominal) Silicon 0.60 0.90 Iron 0.35 max Copper 0.10 max Manganese 0.10 max Magnesium 0.40 0.60 Chromium 0.10 max Zinc 0.10 max Titanium 0.10 max Others, each 0.05 max Others, total 0.15 max Aluminum bal Physical Properties: Density...
Journal Articles
Alloy Digest (2010) 59 (10): Cu-789.
Published: 01 October 2010
... MemberServiceCenter@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Copper October 2010 Cu-789 Ampcoloy 95 has slightly higher mechanical properties than most alloys in its class. Applications include spot welding electrodes. AMPCOLOY® 95 (Extruded High-Performance Copper Alloy) AMPCOLOY®...
Journal Articles
Alloy Digest (2010) 59 (10): Al-432.
Published: 01 October 2010
... MemberServiceCenter@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Aluminum October 2010 Al-432 Kaiser Alloy 6041 is a lead-free alternative to 6262 with good corrosion resistance. KAISER ALLOY 6041 (Extruded Rod & Bar) KAISER ALLOY 6041 Chemical Composition, wt (Nominal) Silicon 0.50...
Journal Articles
Alloy Digest (2010) 59 (11): Al-433.
Published: 01 November 2010
...-0002, 440-338-5151 MemberServiceCenter@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Aluminum November 2010 Al-433 Kaiser Alloy 6082 is a high strength alloy used in structures requiring good corrosion resistance. KAISER ALLOY 6082 (High Strength Extruded Rod & Bar) KAISER...
Journal Articles
Alloy Digest (2010) 59 (12): Al-434.
Published: 01 December 2010
..., Materials Park, OH 44073-0002, 440-338-5151 MemberServiceCenter@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Aluminum December 2010 Al-434 Kaiser Alloy 7003 is a medium strength alloy originally developed in Japan. KAISER ALLOY 7003 (Extruded Rod and Bar) KAISER ALLOY 7003...
Journal Articles
Alloy Digest (2011) 60 (3): Al-436.
Published: 01 March 2011
... Kaiser Alloy 6063 is a magnesium/silicon alloy. One of the most popular of the heat treatable alloy group. Products include extruded and drawn tube, pipe, rod, bar, and profiles. This alloy has good corrosion resistance, good weldability, and a good anodizing response. This datasheet provides...
Journal Articles
Alloy Digest (1985) 34 (7): SA-410.
Published: 01 July 1985
... STROLOY 5C is a high-strength low-alloy steel developed for seamless hot-or-cold finished tubing and extruded shapes in the water-quenched-and-tempered condition. In this condition the steel exhibits high tensile and yield strengths and good ductility. It can be are welded readily using...
Journal Articles
Alloy Digest (1985) 34 (7): Ni-317.
Published: 01 July 1985
... temperatures. It can be hot upset, forged, deep drawn, impact extruded and welded. Applications include highly corrosive environments in agrichemical, petrochemical, pulp and paper, oil and gas, marine and other chemical process industries. This datasheet provides information on composition, physical...