Alloy Digest (2013) 62 (9): SA-681.
Published: 01 September 2013
... Dillidur 500V is a water hardened wear-resistant steel with surface hardness at room temperature of 310-370 HB. It has a high resistance to abrasion and impact wear in combination with good welding performance. This steel is used in the production of excavator buckets, stone crushers, and loading...
Journal Articles
Alloy Digest (2011) 60 (9): SA-634.
Published: 01 September 2011
... Dillidur 325L is a wear resistant steel with a surface hardness at room temperature of 325 HB for 10 mm plate thickness. The material is easy to bend, hot work and machine. Due to its increased wear resistance, it is used to produce excavators, conveyors, and materials handling systems as well...
Journal Articles
Alloy Digest (2018) 67 (4): SA-814.
Published: 01 April 2018
.... As per special agreement with the producer, it is possible to supply plates descaled or descaled and primed. Applications The steel may be used at the discretion of the purchaser for wear-exposed structures, e.g., excavating, mining, and earthmoving machinery; truck dump bodies; conveying, crushing...
Journal Articles
Alloy Digest (2003) 52 (10): SA-522.
Published: 01 October 2003
... strength/weight ratios are important in complex fabrications for critical applications. Potential applications include cantilevered components such as excavator booms, front-end leader hoist arms, or dump body frame components. The steel may be ordered to ASTM A 656 Type 7 specification. Product Forms...
Journal Articles
Alloy Digest (1963) 12 (3): SA-143.
Published: 01 March 1963
... such conditions high impact and fatigue re- sistance are secured along with high elastic properties. AISI 3150 steel, when tempered after hardening to about 400 Brinell hardness, shows excellent wear resistance in road-building, excavating and farm machinery parts in contact with non-metallic abrasive materials...
Journal Articles
Alloy Digest (2016) 65 (5): SA-750.
Published: 01 May 2016
... for a wide range of applications including pressed components for automotive seating, fuel systems, and radiators. It is also a popular choice for lifting and excavating where high strength and toughness are paramount. This material offers exceptional flatness, minimized internal stress and high-quality...
Journal Articles
Alloy Digest (2016) 65 (6): SA-758.
Published: 01 June 2016
... components, tow hooks, industrial silos, and lifting and excavating and agricultural machinery. Producer: Tata Steel 1970 CA IJmuiden The Netherlands Tel: +31 (0) 251 496126 www.tatasteeleurope.com ISSN: 002-614X SA-758BFig. 1 Available dimensions of Ympress Laser S420MC ...
Journal Articles
Alloy Digest (2014) 63 (3): SA-696.
Published: 01 March 2014
... the surface of the plate. Number of Tests. Unless otherwise agreed upon with the producer, the Brinell hardness shall be determined from each heat. Applications: The steel may be used at the discretion of the purchaser for wear-exposed structures, e.g., excavating, mining and earth- moving machinery, truck...
Journal Articles
Alloy Digest (2014) 63 (4): SA-699.
Published: 01 April 2014
... of the purchaser for wear-exposed structures, e.g., excavating, mining and earth- moving machinery, truck dump bodies, conveying, crushing and pulverizing equipment, and scrap presses. The processing and application techniques as a whole are of fundamental importance for the successful use of the products...
Journal Articles
Alloy Digest (2014) 63 (10): SA-711.
Published: 01 October 2014
... shall be determined from each heat. Applications: The steel may be used at the discretion of the purchaser for wear- exposed structures, e.g., excavating, mining, and earth-moving machinery; conveying, crushing, and pulverizing equipment; scrap presses; and other machinery. The steel can also be used...
Journal Articles
Alloy Digest (2015) 64 (3): SA-723.
Published: 01 March 2015
... (3.937 in Product Forms Available: Heavy plate 40 100 mm (1.575 3.937 in.) Applications: The steel may be used at the discretion of the purchaser for wear-exposed structures, e.g., excavating, mining, and earth- moving machinery, truck dump bodies, conveying, crushing, and pulverizing equipment...
Journal Articles
Alloy Digest (2014) 63 (1): SA-690.
Published: 01 January 2014
... Crushing and pulverizing equipment Buckets, knives, crushers, feeders Presses Skips Excavators Slurry pipe systems Screw conveyors Producer: NLMK Clabecq B-1460 Ittre, Belgium Tel: +32 2 391 91 00 Fax +32 2 391 98 90 www.eu.nlmk.com ISSN: 002-614X SA-690B ...
Journal Articles
Alloy Digest (2014) 63 (6): SA-702.
Published: 01 June 2014
... shall be determined from each heat. Applications: The steel may be used at the discretion of the purchaser for wear-exposed structures, e.g., excavating, mining, and earth- moving machinery; truck dump bodies; conveying, crushing and pulverizing equipment; scrap presses; paving molds; and in switch...
Journal Articles
Alloy Digest (2014) 63 (8): SA-706.
Published: 01 August 2014
...: The steel may be used at the discretion of the purchaser for wear-exposed structures, e.g., excavating, mining, and earth- moving machinery; truck dump bodies; conveying, crushing, and pulverizing equipment; scrap presses; paving molds; and in switch manufacturing. The processing and application techniques...
Journal Articles
Alloy Digest (1988) 37 (3): SA-429.
Published: 01 March 1988
... and excavator components; plastic injection molds; aircraft parts; rotary kilns; armor. Manufacturer: Lukens Steel Coatesville, Pennsylvania 19320 ...
Journal Articles
Alloy Digest (2014) 63 (11): SA-712.
Published: 01 November 2014
...-exposed structures, e.g., excavating, mining, and earth- moving machinery; conveying, crushing, and pulverizing equipment; and scrap presses and paving molds. The steel can also be used at service temperatures up to 400 °C (752 °F). The processing and application techniques as a whole are of fundamental...
Journal Articles
Alloy Digest (2015) 64 (5): SA-725.
Published: 01 May 2015
... progress, and are suited to the proposed application. The selection of the material is up to the purchaser. The steel may be used at the discretion of the purchaser for wear-exposed structures, e.g., excavating, mining, and earthmoving machinery; truck dump bodies; and conveying, crushing, and pulverizing...
Journal Articles
Alloy Digest (2015) 64 (6): SA-726.
Published: 01 June 2015
... application. The selection of the material is up to the purchaser. The steel may be used at the discretion of the purchaser for wear-exposed structures, e.g., excavating, mining, and earth-moving machinery; truck dump bodies; and conveying, crushing and pulverizing equipment. The processing and application...
Journal Articles
Alloy Digest (2015) 64 (7): SA-727.
Published: 01 July 2015
..., e.g., excavating, mining, and earth-moving machinery; truck dump bodies; and conveying, crushing, and pulverizing equipment. The processing and application techniques as a whole are of fundamental importance for the successful use of the products fabricated from this steel. The processor/ fabricator...
Journal Articles
Alloy Digest (2015) 64 (8): SA-729.
Published: 01 August 2015
.... The steel may be used at the discretion of the purchaser for wear-exposed structures, e.g., excavating, mining, and earth-moving machinery; truck dump bodies; and conveying, crushing, and pulverizing equipment. The processing and application techniques as a whole are of fundamental importance...