Alloy Digest (1983) 32 (3): Ni-284.
Published: 01 March 1983
.... Its uses include marine components, caustic evaporators and chemical processing equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (1985) 34 (6): Cu-497.
Published: 01 June 1985
... to corrosion. It is used widely for condenser, evaporator and heat-exchanger tubes and associated applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat...
Journal Articles
Alloy Digest (1994) 43 (11): Cu-599.
Published: 01 November 1994
... addition of inhibitor is made to minimize the alloy’s susceptibility to dezincification and stress corrosion. They are used for condenser, evaporator and heat-exchanger tubes and associated applications. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1982) 31 (8): Cu-443.
Published: 01 August 1982
... in such equipment as condensers, evaporators and heat exchangers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-443...
Journal Articles
Alloy Digest (1984) 33 (3): SS-442.
Published: 01 March 1984
... SANDVIK Sanicro 28 is an all-purpose low-carbon stainless steel alloy for service in highly corrosive environments. It has exceptionally high resistance to various types of corrosive attack and has good weldability. Among its numerous applications are evaporator tubes in the production...
Journal Articles
Alloy Digest (1985) 34 (10): Cu-501.
Published: 01 October 1985
... water and is used in marine service. It is used widely for condenser tubes, distiller tubes, heat exchangers, evaporators and water heaters for domestic service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1997) 46 (12): Ti-111.
Published: 01 December 1997
... 3M TITANIUM MATRIX COMPOSITES are produced by electron-beam evaporation to apply Ti-6Al-4V coating to high-strength, high-modulus silicon carbon fibers. The resulting composite has increased strength and stiffness over monolithic titanium/titanium alloy parts. This datasheet provides information...
Journal Articles
Alloy Digest (1987) 36 (7): Cu-526.
Published: 01 July 1987
... to minimize the alloy's susceptibility to dezincification and stress corrosion. It is used widely for condenser, evaporator and heat-exchanger tubes and associated applications. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1960) 9 (3): SA-96.
Published: 01 March 1960
... resistance to certain types of indus- trial fluids, such as some caustic soda solutions and paper mill liquors. In the corrosion resisting field, Nicloy 5 tubes have been used to a considerable exrent in the handling and evaporation of paper mill black liquors for the recovery of chemicals from sulphate...
Journal Articles
Alloy Digest (1994) 43 (2): Pt-5.
Published: 01 February 1994
... as a func- tion of iridium content. Oxidation Resistance: Iridium forms a volatile oxide ar high temperatures. Because of this there is a noticeable loss by evaporation when these alloys are annealed in air above 900°C (1650°F). The loss by evaporation increases with temperature and iridium content Typical...
Journal Articles
Alloy Digest (1959) 8 (7): Cu-77.
Published: 01 July 1959
..., and brines. In general, it has better resistance to corrosion than copper by alkaline and salt solutions. Tubes of this alloy are used in con- densers and coolers in central power stations and ships, and for brine and sea water evaporators, because of its resistance to corrosion-erosion. Specification...
Journal Articles
Alloy Digest (1985) 34 (4): Cu-495.
Published: 01 April 1985
..., it is used widely for the fabrication of equipment for such applications as industrial condensers, refrigerators, heat exchangers and evaporators. Forms Available: Tube. Applications: Mueller Copper 1220 is used in a large number of household, industrial, transportation and miscellan- eous applications...
Journal Articles
Alloy Digest (1984) 33 (5): SS-444.
Published: 01 May 1984
... International® 1996 Table 4 - WET PROCESS SUPERPHOSPHORIC ACID EVAPORATOR - (70% phosphoric acid with 3% sulfates and 60000 ppm fluorides in an 87day test) Weight Loss. mg/cm2 First-Stage Second-Stage Evaporator Evaporator7 Alloy 32oOF (160°C) 370°F (188°C) Carpenter 20Mo-6 34 100 Alloy G 35 83 Alloy 904L 158...
Journal Articles
Alloy Digest (1972) 21 (3): Cu-253.
Published: 01 March 1972
... as industrial condensers, refrigerators, heat exchangers and evaporators. Forms Available: Bar, rod, wire, plate, sheet, strip, pipe, tube, extrusions. Applications: Air conditioners, brewery tubes, condensers. evaporators, heat exchangers, dairy tubes, distiller tubes, kettles, pulp and paper lines, steam...
Journal Articles
Alloy Digest (1974) 23 (9): Cu-284.
Published: 01 September 1974
... by fresh and salt waters, ammonia-free alkaline solutions. many organic chemicals and many dry gases; avoid moist ammonia, strongly oxidizing acids and solutions. sulfur and mercury compounds, cyanides and strong bases. It has wide usage as tubes for evaporators, condensers and heat exchangers. Forms...
Journal Articles
Alloy Digest (1992) 41 (12): Ni-419.
Published: 01 December 1992
..., evaporators, pumps, piping, valves, vessels, expansion bellows, tank trucks, scrubbers, condensers, tank and vessel linings; and for processing and handling sulfuric acid, phospho- ric acid, hydrofluoric acid, nitric acid, nitrates and oxi- dizing salts. 9 Pulp and Paper - wet scrubber linings in systems...
Journal Articles
Alloy Digest (2020) 69 (11): Ni-764.
Published: 01 November 2020
...). Product Forms Bar, rod, wire, plate, sheet, strip. Other shapes are subject to special enquiry. Applications Pipes, tubes, and fittings used in oil and gas extraction, e.g., in heat exchangers, evaporators, washers, immersion pipes in sea water cooled heat exchangers, offshore piping. Components...
Journal Articles
Alloy Digest (1980) 29 (3): Cu-391.
Published: 01 March 1980
... lines, alloy 706 is not especially adapted to handle heavily polluted waters containing sewage and industrial wastes. Alloy 706 finds its greatest application in marine service, in oil refineries for condensers and evaporators, in tide- water steam power plants, in sugar refmeries, in dis- tilleries...
Journal Articles
Alloy Digest (1956) 5 (11): Ni-29.
Published: 01 November 1956
... is to be subjected to shock, but this is rarely necessary. Corrosion Resistance: Exceptionally resistant to sulphuric acid of alI con- centrations even up to boiling point. In boiling sul- phuric acid evaporated to fumes, the corrosion rate is about 0.050 inch per month. It has low corrosion resistance 10. acetic...
Journal Articles
Alloy Digest (1969) 18 (7): Cu-203.
Published: 01 July 1969
... Applications: Conveyor chain links. cams. pump parts. valves and evaporators. Manufacturer: Waukesha Foundry Cornpan! W aukesha. Wisconsin DOI: 10.31399/asm.ad.cu0203 Copyright © ASM International® 1996 ...