Alloy Digest (1987) 36 (1): Cu-520.
Published: 01 January 1987
... ZHC COPPER is a high-electrical-conductivity alloy developed to satisfy the requirements of high-power electronic circuits. It has high strength compared to other metals of equivalent conductivity, good bend formability, excellent stress-relaxation resistance and is readily soldered. It also is...
Journal Articles
Alloy Digest (2017) 66 (1): Cu-855.
Published: 01 January 2017
... Kobelco alloy KLF 170 has high strength and high conductivity for electronic applications. The alloy is nominally Cu-0.7Ni-0.13P-0.1 Fe-0.1Zn. KLF 170 has electrical conductivity equivalent to C19400 and strength equivalent to 42 alloy. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1976) 25 (7): Cu-314.
Published: 01 July 1976
...: CDA Copper Alloy No. 192. (Exception: Chase 192.HC has higher conductivity.) General Characteristics: Chase 192.HC is a high-conductivity alloy with high strength in comparison with copper and a number of copper alloys. Its tensile strength is more than equivalent to alloys of much higher alloy...
Journal Articles
Alloy Digest (2010) 59 (12): Cu-792.
Published: 01 December 2010
...: Copper December 2010 Cu-792 PMX alloy C14530 was released to support legacy programs which are by themselves not large enough to justify major research for an independent alloy. PMX ALLOY C14530 (High Conductivity Cu-Sn-Te Alloy) PMX ALLOY C14530 Chemical Composition, wt (Nominal) Copper 99.80 min bal...
Journal Articles
Alloy Digest (2016) 65 (11): Cu-853.
Published: 01 November 2016
... is shown in Table 2. Softening resistance is shown in Fig 1. Specification Equivalents: UNS C14415 Copyright © 2016, ASM International®. All rights reserved. KOBELCO KFC (High Conductivity Copper Alloy) Filing Code: Cu-853 Copper :: November 2016 Materials Park, Ohio 44073-0002 :: 440.338.5151 :: Fax...
Journal Articles
Alloy Digest (1977) 26 (10): Cu-341.
Published: 01 October 1977
... CHASE 14310 is a high-conductivity copper with excellent resistance to thermal softening. It is a deoxidized, electronic grade of copper with excellent formability, weldability and plateability. It is available in strip form and has a wide range of applications. This datasheet provides information...
Journal Articles
Alloy Digest (1977) 26 (5): Cu-332.
Published: 01 May 1977
... Copper Alloy No. 815 is an age-hardenable cast copper-chromium alloy. It is characterized by high electrical and thermal conductivities combined with medium hardness and strength in the age-hardened condition. It is used for components requiring high electrical conductivity or high thermal...
Journal Articles
Alloy Digest (1972) 21 (10): Cu-260.
Published: 01 October 1972
... same brightening solutions used for copper. Specification Equivalents: CDA Copper Alloy No. 195. General Characteristics: OLIN STRESCON ALLOY 195 is a precip itation-hardenable copper ahoy which has an electrical conductivity of 50% IACS in the aged condition. In spring temper, its yield strength at...
Journal Articles
Alloy Digest (1966) 15 (5): Al-155.
Published: 01 May 1966
... Aluminum 6101 is a heat treatable wrought alloy recommended for applications involving maximum electrical conductivity with moderately high strength, such as bus conductors. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear...
Journal Articles
Alloy Digest (2010) 59 (9): Cu-788.
Published: 01 September 2010
... PMX alloy C19015 is an improved conductivity alloy with other engineering characteristics for electronics and mixed power signal applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high...
Journal Articles
Alloy Digest (2016) 65 (12): Cu-854.
Published: 01 December 2016
... 150~175 Bend formability is shown in Table 1. Softening resistance is shown in Fig. 1. Specification Equivalents: UNS C19240 Copyright © 2016, ASM International®. All rights reserved. KOBELCO SUPERKFC (High-Conductivity Copper Alloy) Filing Code: Cu-854 Copper :: December 2016 Materials Park, Ohio...
Journal Articles
Alloy Digest (2017) 66 (2): Cu-857.
Published: 01 February 2017
... Kobelco Alloy KLF 194 has high strength and high conductivity for electronic applications. The alloy is nominally Cu-2.2Fe-0.03P-0.5Zn. KLF 194 is produced differently and has slightly different properties than C194. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2000) 49 (12): Cu-656.
Published: 01 December 2000
... expansion, 10 6/K (10 6/°F) 16.2 (9.0) Thermal conductivity, W/m·K (Btu/(ft · h · °F)) 183 (106) Electrical conductivity, %IACS 48 Resistivity, µ · m ( circular-mil/ft) 0.0359 (22) Mechanical Properties: Modulus of elasticity, GPa (106 psi) 114 (16.5) See also Table 1. Specification Equivalents: UNS...
Journal Articles
Alloy Digest (1964) 13 (8): Cu-144.
Published: 01 August 1964
... OFHC copper is a high conductivity, oxygen free grade of copper furnished in two grades, namely, Regular Grade and Certified Grade. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also...
Journal Articles
Alloy Digest (2003) 52 (5): Cu-702.
Published: 01 May 2003
... Outokumpu C 1453 is a high-conductivity copper alloy with excellent softening resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength as well asfatigue. Filing Code: CU-702. Producer or source: Outokumpu...
Journal Articles
Alloy Digest (1975) 24 (4): Cu-295.
Published: 01 April 1975
... AMPCOLOY 910 is copper containing 0.12% zirconium. It retains high conductivity with good strength, hardness and ductility at elevated temperatures. It is used in a variety of applications such as collector rings, current-carrying shafts and bearings. This datasheet provides information on...
Journal Articles
Alloy Digest (1965) 14 (9): Cu-155.
Published: 01 September 1965
... MALLORY 53B is an economical copper alloy combining high strength with high heat and electrical conductivity and excellent corrosion resistance. It is heat treatable. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive...
Journal Articles
Alloy Digest (1967) 16 (6): Cu-177.
Published: 01 June 1967
... Mallory 22 is a high strength, high conductivity copper-base alloy supplied in the form of forgings. It is heat treatable and is recommended for resistance welding electrodes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It...
Journal Articles
Alloy Digest (1962) 11 (3): Cu-115.
Published: 01 March 1962
... corrosion characteristics as copper. It is, therefore, often used to replace copper com- ponents where good machinability is required. Specification Equivalent: ASTM-B-301-58 General Characteristics: Mueller tellurium copper combines the high electrical and thermal conductivity and good corrosion resistance...
Journal Articles
Alloy Digest (2001) 50 (7): Cu-669.
Published: 01 July 2001
... Wieland-K80 is a high-conductivity copper alloy with an excellent capacity for both cold work and hot forming This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion...