Skip Nav Destination
Close Modal
Search Results for
endurance limit
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 348 Search Results for
endurance limit
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1958) 7 (5): SA-68.
Published: 01 May 1958
... Ferrovac-4340 is a vacuum melted chromium, nickel, molybdenum alloy steel having high endurance limit, high notched tensile strength, and high transverse ductility. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Abstract
View article
PDF
Ferrovac-4340 is a vacuum melted chromium, nickel, molybdenum alloy steel having high endurance limit, high notched tensile strength, and high transverse ductility. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-68. Producer or source: Vacuum Metals Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1997) 46 (9): Ti-109.
Published: 01 September 1997
...) that enhances the fatigue endurance limit. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength as well as fatigue. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: TI-109. Producer...
Abstract
View article
PDF
Sandvik Ti-3Al-2.5V Grade 9 titanium-aluminum alloy offers excellent corrosion resistance, especially to chloride media, and has a high strength-to-weight ratio, which is especially suitable for use in aerospace applications. Tubing can be produced having a CSR (contractile strain ratio) that enhances the fatigue endurance limit. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength as well as fatigue. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: TI-109. Producer or source: Sandvik.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1967) 16 (8): SA-214.
Published: 01 August 1967
... FAGERSTA K825 is a tough, shock resistant alloy steel having high tensile strength and endurance limit in the heat treated condition. It is recommended for shafts, bolts, countershafts, etc. in moderately stressed applications. This datasheet provides information on composition, physical...
Abstract
View article
PDF
FAGERSTA K825 is a tough, shock resistant alloy steel having high tensile strength and endurance limit in the heat treated condition. It is recommended for shafts, bolts, countershafts, etc. in moderately stressed applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, machining, and joining. Filing Code: SA-214. Producer or source: Fagersta Steels Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1961) 10 (10): SA-121.
Published: 01 October 1961
... AISI 4650 is an oil hardening, medium-carbon alloy steel having high mechanical properties, endurance limit and shock resistance. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat...
Abstract
View article
PDF
AISI 4650 is an oil hardening, medium-carbon alloy steel having high mechanical properties, endurance limit and shock resistance. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-121. Producer or source: Alloy steel mills and foundries.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2022) 71 (12): Al-492.
Published: 01 December 2022
... for alloying content and strength. It has excellent fatigue properties, with an endurance limit of 115 MPa in the H32 temper and 125 MPa in the H34 temper. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion...
Abstract
View article
PDF
Austral Wright 5052 is a wrought, non-heat-treatable, aluminum-magnesium-chromium alloy (5xxx series) that exhibits a good combination of strength, corrosion resistance, and formability in a wide range of rolled products. It is about mid-way through the series of aluminum-magnesium alloys for alloying content and strength. It has excellent fatigue properties, with an endurance limit of 115 MPa in the H32 temper and 125 MPa in the H34 temper. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-492. Producer or source: Austral Wright Metals.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (5): Al-175.
Published: 01 May 1968
... 35000 Tensile yield strength, psi (0.2%) 12000 25000 Elongation, % in 2 2.5 2.5 Brine11 hardness (500 Kg) 65 80 Shear strength, psi 28000 Endurance limit, psi 8500 Compressive yield strength, psi (0.2%) - 26000 Table 2 - TYPICAL SANDCAST PROPERTIES -T51 -T61 Tensile strength, psi 28000 39000 Tensile...
Abstract
View article
PDF
ALLCAST 41A is an aluminum-silicon-copper casting alloy. It responds to an age-hardening heat treatment and is recommended for light weight, high strength, pressure-tight castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on high temperature performance as well as heat treating, machining, and joining. Filing Code: Al-175. Producer or source: Apex Smelting Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2017) 66 (4): Cu-860.
Published: 01 April 2017
... Bearium B-4, B-8, B-10, and B-11 are copper-base, high-lead bearing bronzes with superior resistance to scoring and seizure beyond the endurance and danger limits of ordinary bearing bronzes. It is used in applications involving high speeds, poor lubrications, heat-generating loads, elevated...
Abstract
View article
PDF
Bearium B-4, B-8, B-10, and B-11 are copper-base, high-lead bearing bronzes with superior resistance to scoring and seizure beyond the endurance and danger limits of ordinary bearing bronzes. It is used in applications involving high speeds, poor lubrications, heat-generating loads, elevated temperatures, dusty and gritty surroundings, or when a liquid other than oil is used as the lubricant. It is produced in four grades: B-4, B-8, B-10, and B-11. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on casting, forming, heat treating, machining, and joining. Filing Code: Cu-860. Producer or source: MetalTek International. Originally published as Bearium Metal, Alloy Digest Cu-258, September 1972, revised April 2017.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1976) 25 (12): Cu-324.
Published: 01 December 1976
... FEDERAL BRONZE 822 is a copper-base, high-lead bearing bronze with superior resistance to scoring and seizure beyond the endurance and danger limits of ordinary bearing bronzes. It is used in applications involving high speeds, poor lubrication, heat-generating loads, elevated temperatures, dusty...
Abstract
View article
PDF
FEDERAL BRONZE 822 is a copper-base, high-lead bearing bronze with superior resistance to scoring and seizure beyond the endurance and danger limits of ordinary bearing bronzes. It is used in applications involving high speeds, poor lubrication, heat-generating loads, elevated temperatures, dusty and gritty surroundings, or where a liquid other than oil is used as the lubricant. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on casting, heat treating, machining, joining, and surface treatment. Filing Code: Cu-324. Producer or source: Federal Bronze Products Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1972) 21 (9): Cu-258.
Published: 01 September 1972
... BEARIUM METAL is a copper-base, high-lead bearing bronze with superior resistance to scoring and seizure beyond the endurance and danger limits of ordinary bearing bronzes. It is used in applications involving high speeds, poor lubrication, heat-generating loads, elevated temperatures, dusty...
Abstract
View article
PDF
BEARIUM METAL is a copper-base, high-lead bearing bronze with superior resistance to scoring and seizure beyond the endurance and danger limits of ordinary bearing bronzes. It is used in applications involving high speeds, poor lubrication, heat-generating loads, elevated temperatures, dusty and gritly surroundings, or where a liquid other than oil is used as the lubricant. It is produced in three grades: B-4, B-8 and B-10. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on casting, heat treating, machining, joining, and surface treatment. Filing Code: Cu-258. Producer or source: Bearium Metals Corporation. Revised as Bearium B-4, B-8, B-10, B-11, Alloy Digest Cu-860, April 2017.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1958) 7 (5): Ti-16.
Published: 01 May 1958
... in R R. Moore rotating beam fatigue machines at 10,000 cpm showed 62.000 psi endurance limit at 107 cycles for smooth specimens which is 65% of the room temperature ulcimao strength, and using a 0.010 root radius notch, the notched endurance limit is 36.000 psi or 38% of the ultimate strength at room...
Abstract
View article
PDF
REM-CRU A-70 is the grade of unalloyed titanium used where higher strength is required. It is specified for many moderately stressed aircraft parts. (Formerly known as RC-70.) This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive, shear, and bearing strength as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ti-16. Producer or source: Rem-Cru Titanium Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1964) 13 (6): Al-138.
Published: 01 June 1964
... Max. Brine11 hardness (500 Kg.) 90 Compressive yield strength, psi (0.2%) 19000 Shear strength, psi 27000 Endurance limit, psi (5x108 cycles) 14500 Table 2 - TYPICAL HEAT TREATED PROPERTIES Tensile strength, psi Tensile yield strength, psi Elongation, % in 2 Brine11 hardness (500 Kg) Compressive...
Abstract
View article
PDF
Aluminum 333 is an aluminum-copper-silicon casting alloy recommended for high temperature applications requiring leak tightness. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on casting, heat treating, machining, and joining. Filing Code: Al-138. Producer or source: Aluminum Company of America.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1991) 40 (4): SA-457.
Published: 01 April 1991
...) Tensile strength, psi 115ooo-130000 Yield point, psi 75ooo-looooo Elongation (2 % 45-35 Reduction in area, % 5040 Brinell hardness 217-300* Izod impact, ft-lbs (Room temperature) SO-90 Charpy impact, ft-lbs (-50°F? 1 OF) 37-40 *Depends on thickness of material. Table 2 -COMPARATIVE ENDURANCE LIMIT CRR...
Abstract
View article
PDF
JESSOP No. 9, super high tensile steel, is one of the toughest and most wear resistant steels of its class in existence. Primarily developed as a high tensile, non-magnetic armor plate, it has since been widely used for equipment subject to severe battering. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness and fatigue. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-457. Producer or source: Jessop Steel Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1957) 6 (8): Al-54.
Published: 01 August 1957
... 0.33 PROPERTIES Table 1 - TYPICAL DIE CAST PROPERTIES Tensile strength, psi 45000 Yield strength, psi (0.2%) 27000 Elongation, 7, in 2 8.0 Brinell hardness (500/10/30) 80 Endurance limit, psi 23000 (5 x 108 cycles) Shear strength, psi 28000 Charpy impact, ft. lbs. 8.0 Table 2 - TYPICAL ELEVATED...
Abstract
View article
PDF
APEX 418 is an aluminum die casting alloy having excellent combination of high strength and corrosion resistance, also high ductility and finishing qualities. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting and machining. Filing Code: Al-54. Producer or source: Apex Smelting Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2009) 58 (11): SA-611.
Published: 01 November 2009
... Mesh Table 1 Rotating bending fatigue performance of Ancorsteel 4300 + 0.6 wt.% graphite Cooling rate Ultimate tensile strength 90% endurance limit 50% endurance limit °C/min °F/min MPa ksi MPa ksi MPa ksi 42 201.6 1035 150 310 45 315 46 94 169.2 1170 170 325 47 340 49 Samples compacted at 690 MPa (50...
Abstract
View article
PDF
Ancorsteel 4300 alloy ferrous powder simulates wrought steel compositions and is a cost-effective alternative to alloys requiring secondary processing. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on heat treating and powder metal forms. Filing Code: SA-611. Producer or source: Hoeganaes Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1964) 13 (5): CI-33.
Published: 01 May 1964
... Copyright © ASM International® 1996 Table 5 - TYPICAL FATIGUE PROPERTIES Type SP-80 SF-60 SH-100 Condition As-cast Annealed As-cast Tensile Strength psi 80000 60000 100000 Unnotched Fatigue Endurance Endurance Limit Ratio 39000 0.49 30000 0.50 43000 0.43 45oV Notch Endurance Endurance Limit Ratio 21000 0.35...
Abstract
View article
PDF
DUCTLIRON is a high-carbon ferrous material containing graphite in the form of nodules or spheroids. It possesses unusually high ductility, strength and castability. It is furnished in three different grades, namely, SF-60, SP-80 and SH-100. Alloyed grades are also available under different designations as AQS-HS and WS. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on casting, heat treating, machining, and joining. Filing Code: CI-33. Producer or source: Rosedale Foundry.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1970) 19 (7): SA-254.
Published: 01 July 1970
... SECTIONS (Under 4 inches diameter) (Heated at 15000F for 30 minutes. auair cooled, aged at 9OOoF for 3 hours, air cooled.) Tensile strength, psi 294000 Yield strength, psi (0.2%) 288000 Elongation, B in 4D 11 Reduction of area, k Rockwell hardness 2: Endurance limit, psi (Smooth specimens) 125000 Endurance...
Abstract
View article
PDF
NIMARK 300 is a vacuum melted low carbon, 18% nickel alloy steel which attains yield strengths in excess of 270,000 psi. It is recommended for high strength, shock resisting applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-254. Producer or source: Carpenter.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1959) 8 (6): Al-79.
Published: 01 June 1959
...%) Elongation* $33 in 2 (500,/10) Strength psi Ho34 29000 37 29000 14 14 30 2 18000 21000 H38 43000 38000 8 85 24000 59ooo 8: 24000 19ooo Endurance Limit psi 17000 18000 18500 19000 Fatigue Strength psi 17000 18000 19000 * % of 4D (round specimens l/8 in. diameter or over), 4.5 A, (round specimens l/8...
Abstract
View article
PDF
ALCAN 57S is a medium strength wrought aluminum alloy having excellent resistance to corrosion especially by salt water. It is not heat treatable. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-79. Producer or source: Aluminum Company of Canada Ltd.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1954) 3 (4): Ti-3.
Published: 01 April 1954
... with excellent forgeabihy at higha tunperatures because of its two-phase strucmre. Storage for times up to 1000 hours at temperatures up to 1000 deg. F has no effect on the tensile properties determined at the storage temperature. C-l 30AM alloy has a room temperature endurance limit of 90,000 psi when tested...
Abstract
View article
PDF
Rem-Cru C-130AM titanium-base alloy was developed with a minimum yield strength of 130,000 psi for fabrication into bars and forgings. It was formerly known as Rem-Cru RC-130B. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as creep and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ti-3. Producer or source: Rem-Cru Titanium Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1955) 4 (7): Al-29.
Published: 01 July 1955
...%. - Nickel 0.1 max. Freezing range, C. -. ;:5-625 ZiIlC 01 max. ,%lidification shrinkage, ye (approx. ) 6 Lead 0.1 max. Modulus of elasticity, psi 10,300,000 Tin 0.05 max. Aluminum Remainder Tensile strength, psi Proof stress, psi (0.1%) Elongation, 70 in 2 Brinell hardness Endurance limit, psi Shear...
Abstract
View article
PDF
ALAR 00.5 is a 5% silicon-aluminum casting alloy having high corrosion resistance. It is suitable for pressure-tight and thin-walled castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-29. Producer or source: B. K. L. Alloys Ltd.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (10): Al-180.
Published: 01 October 1968
... strength, psi 22000 24000 Endurance limit, psi 10000 11000 Table 2 - TYPICAL HEAT TREATED PROPERTIES - Sand Cast (Solution treated at 950°F and aged at 310°F) Aged 3 hours Aged 16 hours Tensile strength, psi 32000-38000 40000-48000 Yield strength, psi (0.2%) 2 2000-28000 37000-42000 Elongation, % in 2 2 1...
Abstract
View article
PDF
FEDERATED F460 is a heat treatable, aluminum-base, sand and permanent mold casting alloy having good foundry characteristics and pressure tightness. It is recommended for general purpose castings in either the as-cast or heat treated condition. The F460PT grade is specially processed during manufacture to reduce the apparent solidification shrinkage with no change in chemical specification or mechanical properties. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-180. Producer or source: Federated Metals Corporation, ASARCO Inc..