1-20 of 4973 Search Results for

elongation

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1990) 39 (8): CI-62.
Published: 01 August 1990
... 55-06 and 70-02 Ductile Dura-Bar are continuously cast ductile irons with about 50 and 75% pearlitic microstructures, respectively. 55-06 has about the same tensile strength as SAE 1045 as-hot-rolled steel. Its maximum yield strength and elongation are equivalent to a eutectoid carbon steel. 70-02...
Journal Articles
Alloy Digest (2023) 72 (2): CI-102.
Published: 01 February 2023
... ACO Eurobar EN-GJS-350-22C is a ferritic spheroidal graphite cast iron that is produced by the continuous casting process. It has a minimum tensile strength of 350 MPa (51 ksi) and a minimum elongation of 22%. It is specifically designed for applications where tensile strength is less important...
Journal Articles
Alloy Digest (2023) 72 (3): CI-103.
Published: 01 March 2023
... ISO1083/JS/350-22-RT is a ferritic spheroidal graphite cast iron that has a minimum tensile strength of 350 MPa (51 ksi) and a minimum elongation of 22%, when measured on test pieces machined from separately cast samples. It is specifically designed for applications where tensile strength is less...
Journal Articles
Alloy Digest (2023) 72 (4): CI-104.
Published: 01 April 2023
... ISO1083/JS/400-18-LT is a ferritic spheroidal graphite cast iron that has a minimum tensile strength of 400 MPa (58 ksi) and a minimum elongation of 18%, when measured on test pieces machined from separately cast samples. It has a tensile strength exceeding that of the highest-tensile-strength...
Journal Articles
Alloy Digest (2023) 72 (5): CI-105.
Published: 01 May 2023
... ISO1083/JS/400-15 is a ferritic spheroidal graphite cast iron that has a minimum tensile strength of 400 MPa (58 ksi) and a minimum elongation of 15%, when measured on test pieces machined from separately cast samples. It has a tensile strength exceeding that of the highest-tensile-strength grade...
Journal Articles
Alloy Digest (2023) 72 (6): Al-499.
Published: 01 June 2023
... Rio Tinto A356.2 is a heat-treatable, aluminum-silicon-magnesium casting alloy (3xx.x series) that is available in the ingot form for remelting. It is used extensively for producing general-purpose sand and permanent mold castings that require a combination of medium strength with good elongation...
Journal Articles
Alloy Digest (2019) 68 (1): Ni-749.
Published: 01 January 2019
... Manaurite XMR is a heat resistant alloy for hydrocarbon processing. It is a modified version of Manaurite XM (Alloy Digest Ni-748, December 2018) designed to withstand creep elongation at high temperature, while also being able to be welded after aging. This datasheet provides information...
Journal Articles
Alloy Digest (2019) 68 (11): SA-856.
Published: 01 November 2019
... Strenx™ 1100 Plus is a high-strength, hot-rolled, quenched and tempered, structural steel with a minimum yield strength of 1100 MPa (160 ksi) and very good weld performance. The strength, elongation, and impact toughness of weldments fulfill minimum guarantees of the base metal. This datasheet...
Journal Articles
Alloy Digest (1977) 26 (10): Zn-32.
Published: 01 October 1977
... to the general-purpose ZA-12 alloy (Alloy Digest Zn-31, September 1977) except for its higher strength and elongation, but with higher casting temperatures and poor heavy-section castability. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength...
Journal Articles
Alloy Digest (1975) 24 (7): Zn-20.
Published: 01 July 1975
... NJZ ALLOY No. 10 is an alloy with medium tensile strength and elongation. It is produced from a high-grade zinc base by additions of cadmium, iron, and lead. It combines good ductility with stiffness and its applications include hardware and laundry tags. This datasheet provides information...
Journal Articles
Alloy Digest (2021) 70 (8): Al-479.
Published: 01 August 2021
... applications requiring high strength and elongation, and sound castings. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting and heat treating. Filing Code: Al-479. Producer...
Journal Articles
Alloy Digest (2021) 70 (9): Al-480.
Published: 01 September 2021
... with good elongation, and good corrosion resistance. This alloy can be produced to a wide range of mechanical properties by making small adjustments to the magnesium content and/or heat treatment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (2021) 70 (10): Al-481.
Published: 01 October 2021
... is used in the as-cast condition, and exhibits good mechanical properties, especially elongation, which are superior to those of conventional aluminum-silicon alloys. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue...
Journal Articles
Alloy Digest (2021) 70 (11): Mo-21.
Published: 01 November 2021
... that is stable at temperatures up to 2000 °C (3630 °F). After recrystallization, the elongated grain structure with jagged grain boundaries provides a measurable increase in ductility and creep resistant strength over that seen with pure molybdenum. Ed Fagan Molybdenum Lanthanum Oxide is the preferred material...
Journal Articles
Alloy Digest (2021) 70 (12): Al-483.
Published: 01 December 2021
... with good elongation, and good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-483...
Journal Articles
Alloy Digest (1968) 17 (2): Al-172.
Published: 01 February 1968
... SILAFONT-5 is a heat treatable aluminum casting alloy recommended for sand and die castings. It has high strength, medium elongation, good corrosion resistance. It is suited for castings subject to impact and shock. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1995) 44 (6): Al-335.
Published: 01 June 1995
... ALUMINUM ALLOY(S) 206.0 and A206.0 are structural castings in the heat treated temper for applications requiring high tensile and yield strengths with moderate elongation. This datasheet provides information on composition, physical properties, tensile properties, and compressive, shear...
Journal Articles
Alloy Digest (1995) 44 (7): Al-336.
Published: 01 July 1995
... ALUMINUM ALLOY 201.0 is a structural casting alloy available as sand, permanent mold and investment castings. It is used in structural casting members, applications requiring high tensile and yield strengths with moderate elongation, and where high strength and energy-absorption capacity...
Journal Articles
Alloy Digest (1956) 5 (6): Mg-25.
Published: 01 June 1956
... DOWMETAL AZ91C is a heat treatable magnesium base alloy suitable for sand and permanent mold castings. It combines good tensile strength and yield strength with good elongation and is used in both the solution heat treated condition (T4) and in the solution heat treated plus artificially aged...
Journal Articles
Alloy Digest (1979) 28 (8): Fe-58.
Published: 01 August 1979
...: a tensile strength of 71,000 psi and an elongation of 41%; also, it is tough at cryogenic temperatures. Among its many applications are electronic components, cryogenic parts and aircraft controls. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...