Alloy Digest (1984) 33 (3): Cu-99.
Published: 01 March 1984
... AMZIRC is an oxygen-free copper containing zirconium. AMZIRC copper was developed for applications demanding high electrical conductivity and the retention of strength at elevated temperatures. Applications include stud bases for power transmitters and rectifiers, switches and circuit breakers...
Journal Articles
Alloy Digest (1998) 47 (12): Ni-548.
Published: 01 December 1998
... MO-RE 40MA is a fully austenitic heat-resistant alloy for elevated temperature applications. The alloy is microalloyed for creep strength and oxidation resistance. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (2000) 49 (11): Cb-25.
Published: 01 November 2000
... Alloy C-103 is a niobium alloy with a high strength/density ratio for elevated temperature applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance...
Journal Articles
Alloy Digest (1974) 23 (11): Al-211.
Published: 01 November 1974
... ALUMINUM 222.0 is an age-hardenable aluminum alloy for sand and permanent mold castings. It is hard and wear resistant and has good strength at elevated temperatures. Applications include cylinder heads and pistons. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1960) 9 (10): Al-96.
Published: 01 October 1960
... Aluminum 2219 alloy is an aluminum alloy recommended for elevated temperature applications and for welded structures where post weld heat treatment can be employed. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (2006) 55 (7): Al-399.
Published: 01 July 2006
... Alloy 2124 is a heat treatable plate alloy that was developed for elevated-temperature application. Copper is the main alloying addition. 2124-T851 plate is an improvement in fracture toughness compared to 2024-T851. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1959) 8 (6): Mg-42.
Published: 01 June 1959
... MAGNESIUM HZ 32A is a magnesium-base alloy containing thorium, zirconium and zinc. It is recommended for elevated temperature applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (1960) 9 (4): Mo-1.
Published: 01 April 1960
... MOLYBDENUM, 0.5% Ti is a high melting point alloy recommended for highly stressed elevated temperature applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high...
Journal Articles
Alloy Digest (2020) 69 (5): SS-1318.
Published: 01 May 2020
... ATI 309S (UNS S30908) is a chromium-nickel austenitic stainless steel that is typically used for elevated-temperature applications. The alloy’s high chromium and nickel contents provide comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction...
Journal Articles
Alloy Digest (2020) 69 (10): SS-1328.
Published: 01 October 2020
... ATI 310S is a 25Cr-20Ni austenitic stainless steel that is typically used for elevated temperature applications. Owing to its higher chromium and nickel contents the alloy provides comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room...
Journal Articles
Alloy Digest (2021) 70 (4): SS-1333.
Published: 01 April 2021
... AK Steel 309 is a chromium-nickel austenitic stainless steel. It is typically used for elevated temperature applications. Its high chromium and nickel contents provide comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature...
Journal Articles
Alloy Digest (1978) 27 (11): Ni-258.
Published: 01 November 1978
... for elevated-temperature applications in gas turbines and in critical components for missiles. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on forming, heat treating, machining, joining, and surface...
Journal Articles
Alloy Digest (1976) 25 (5): Cu-312.
Published: 01 May 1976
... Copper No. 150 contains nominally 0.15% zirconium. It retains high conductivity with good hardness, strength and ductility at elevated temperatures. Applications include collector rings, bearings and current-carrying shafts. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1969) 18 (4): Ti-57.
Published: 01 April 1969
... HARVEY HA 5158 is an alpha-beta, heat treatable titanium alloy recommended for elevated temperature applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1985) 34 (5): Ni-314.
Published: 01 May 1985
... at room and elevated temperatures. Its applications include heat treating furnace equipment, chemical equipment in various industries, and power plant equipment. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (1977) 26 (5): TS-318.
Published: 01 May 1977
... was designed primarily for die castings dies used with aluminum base alloys, its well-balanced mechanical proper- ties at elevated temperatures make it useful for many other applications, as well. Forms Available: Billets, bars, rods and forgings. Applications: Dies for aluminum die casting, forging-machine...
Journal Articles
Alloy Digest (1980) 29 (7): Ti-78.
Published: 01 July 1980
... RMI 5A1-5Sn-2Zr-2Mo-Si is an alpha-type titanium alloy recommended for high-temperature applications in the 800-1000 F range. In the mill annealed condition it has a typical room-temperature yield strength of 126,000 psi and a typical yield strength (in short-time elevated-temperature tensile test...
Journal Articles
Alloy Digest (1975) 24 (4): SS-309.
Published: 01 April 1975
... CRUTEMP 25 is a fully austenitic stainless steel with outstanding resistance to scaling at elevated temperatures. It also has high strength at elevated temperatures and its weldability is excellent. It is used in such applications as automotive emission control systems and gas turbines...
Journal Articles
Alloy Digest (1987) 36 (11): TS-484.
Published: 01 November 1987
... to shock and abrasion at elevated temper- atures. Its good hot hardness enables it to handle many hot-work jobs without washing out or changing size. B-47 has very good mechanical properties at elevated temperatures where typical applications include extrusion dies for brass, hot-punch tools and forging...
Journal Articles
Alloy Digest (1961) 10 (6): TS-105.
Published: 01 June 1961
... Potomac A is a medium carbon, alloy steel that can maintain strength at elevated temperatures up to 1000 F. It is recommended for hot die applications and for structure components where strength at elevated temperatures is important. This datasheet provides information on composition, physical...