Alloy Digest (1986) 35 (10): Fe-73.
Published: 01 October 1986
... CMI-B Magnetic Iron is an ultra-low-carbon magnetic iron especially processed for good magnetic properties and processability. It is used for relays and other electromagnetic applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (2010) 59 (2): CS-152.
Published: 01 February 2010
.... Compressibility ratings of 7.1 g/cm3 at 550 MPa (40 tsi) provide outstanding sintered properties at lower compacting pressures. Because of its low oxygen and nitrogen levels, the powders are used extensively for electromagnetic applications. See Fig. 2 for compressibility. The product can be summarized...
Journal Articles
Alloy Digest (1973) 22 (6): Ni-191.
Published: 01 June 1973
... MU GUARD 80 is a nickel-iron-molybdenum alloy. It is furnished in strip and foil form and provides optimum initial and maximum permeabilities for electromagnetic shielding applications. It is a high purity, soft magnetic alloy produced by powder metallurgy techniques. This datasheet provides...
Journal Articles
Alloy Digest (1977) 26 (3): SS-337.
Published: 01 March 1977
... Carpenter 430FR Solenoid Quality stainless steel is a ferritic chromium-iron alloy developed especially for A.C. and D.C. magnetic circuit applications such as solenoid valve core components and electromagnetic relay cores. The electrical resistivity of 430FR is approximately 25% higher than other...
Journal Articles
Alloy Digest (1987) 36 (1): Fe-75.
Published: 01 January 1987
... CMI-C Magnetic Iron is a low-carbon magnetic iron especially processed with a critical strain for optimum uniformity. Maximum magnetic properties are achieved following suggested final anneal applied to fabricated parts. Its applications include electromagnet cores, plungers and pole pieces...
Journal Articles
Alloy Digest (2016) 65 (2): CS-196.
Published: 01 February 2016
... Ancorsteel phosphorus alloys are ferrous base powders for PM parts requiring superior electromagnetic performance. Compared with parts made from pure, high compressibility iron powders, those made from the phosphorus alloys have higher resistivity, permeability and induction, and reduced coercive...
Journal Articles
Alloy Digest (1970) 19 (1): Fe-41.
Published: 01 January 1970
... weight and size are prime requisites. Forms Available: Hot rolled sheet, hot rolled plate. forged bar, casting; and hot rolled strip. Applications: Motors and generators, pole pieces for electromagnets and permanent magnets. Manufacturer: Westinghouse Electric Corporation Metal Fabrication Division...
Journal Articles
Alloy Digest (2011) 60 (8): Co-122.
Published: 01 August 2011
..., longitudinal field anneal DOI: 10.31399/asm.ad.co0122 Applications: Typical applications are flexible electromagnetic shielding, magnetic sensors, and high frequency cores. Producers: Metglas, Inc. Conway, SC 29562 USA Tel: 800-518-7654 Tel: 843-349-7319 Fax: 843-349-6815 Hitachi Metals Hong Kong Hong Kong Tel...
Journal Articles
Alloy Digest (1992) 41 (2): Cp-20.
Published: 01 February 1992
.... Their low volume loading provides ease of processing with no extraordinary tool or machine wear. Colorability, impact and mold shrinkage are similar to those of the base resin. Applications: Electrostatic discharge shielding. Electromagnetic interference shielding. Forms Available: Fully compounded products...
Journal Articles
Alloy Digest (2004) 53 (6): Cu-717.
Published: 01 June 2004
... applications that have ambient temper- atures or conform to UL ratings, and backplane connectors where high-speed signals are combined with power and control lines. A requirement for processor sockets is conductivity while providing adequate strength. Applications such as electromagnetic interfer- ence (EMI...
Journal Articles
Alloy Digest (2002) 51 (10): Fe-124.
Published: 01 October 2002
... and high electrical resistivity makes the alloy a candidate for the applications such as actuators, relays, fuel injectors, switched reluctance motors, magnetic bear- ings, flywheels, sensors, high-performance electromagnets, and linear motors. For solenoid applications, it is a particularly important...
Journal Articles
Alloy Digest (2023) 72 (4): Cu-940.
Published: 01 April 2023
... electrical conductivity; non-magnetic; good electromagnetic shielding effectiveness; heat-treatable; high strength; excellent corrosion resistance; fair machinability; See Table 3 for ratings of fabrication characteristics. Product Forms Bar; wire. Applications L. Klein Declafor 1015 is used to produce...
Journal Articles
Alloy Digest (2019) 68 (10): SA-854.
Published: 01 October 2019
... inspection operation should be performed after heat treating. This material is also electromagnetically tested using eddy current and pre-tested for machinability through the producer s testing procedure. Fatigue is one of the most common causes of mechanical failures for metals in-service. Considering...
Journal Articles
Alloy Digest (2016) 65 (3): CS-197.
Published: 01 March 2016
... × 10 5) 41.5 (9.9) 44.0 (25.4) 535 (0.128) 12.8 (7.11) 250 (482) 7730 (0.278) 9.96 × 10 6 (10.7 × 10 5) 43.5 (10.4) 43.3 (25.0) 562 (0.134) 13.0 (7.22) DOI: 10.31399/asm.ad.cs0197 Nondestructive examination: ultrasonic inspection + electromagnetic inspection according to API SR2 (5% of the specified...
Journal Articles
Alloy Digest (2016) 65 (4): CS-198.
Published: 01 April 2016
... inspection + electromagnetic inspection according to API SR2 (5% of the specified wall thickness) Wall thickness is measured and recorded on 100% of the pipe surface Storage and handling recommendation: Avoid pollution by contact with carbon or low allow steel (pipe or parts) Avoid atmospheric...
Journal Articles
Alloy Digest (2016) 65 (5): CS-199.
Published: 01 May 2016
... 11960. Nondestructive examination: ultrasonic inspection + electromagnetic inspection according to API SR2 (5% of the specified wall thickness) Wall thickness is measured and recorded on 100% of the pipe surface Table 1 Physical properties Temperature, °C (°F) Density, kg/m3 (lb/in.3) Thermal...
Journal Articles
Alloy Digest (2016) 65 (2): CS-195.
Published: 01 February 2016
... overall performance than API L80-13CR thanks to better toughness, tighter chemical composition, finer grain size, and more stringent inspection requirements than API 5CT PSL 2 for L80- 13CR. Nondestructive examination: ultrasonic inspection + electromagnetic inspection according to API SR2 (5...
Journal Articles
Alloy Digest (2016) 65 (11): SS-1254.
Published: 01 November 2016
...: ultrasonic inspection + electromagnetic inspection according to API SR2 (5% of the specified wall thickness). Wall thickness is measured and recorded on 100% of the pipe surface. Storage and handling recommendation is as follows. Avoid pollution by contact with carbon or low allow steel (pipe or parts...
Journal Articles
Alloy Digest (2016) 65 (8): CS-201.
Published: 01 August 2016
...). Product Forms Available: Pipe and tubing with diameters 60 273 mm (2.375 10.75 in.) and weights as per API 5CT / ISO 11960. Nondestructive examination: ultrasonic inspection + electromagnetic inspection according to API SR2 (5% of the specified wall thickness). Wall thickness is measured and recorded...
Journal Articles
Alloy Digest (1957) 6 (10): Fe-15.
Published: 01 October 1957
... curve. Three principles ate employed in these applications! namely, shunt applied to a permanent magnet, shunt apphed to reactance circuit, and shunt applied to electromagnet. In addition to the application for temperature compensation, there is a group of possible applications which em difference...