Skip Nav Destination
Close Modal
Search Results for
electrical resistance
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 3625
Search Results for electrical resistance
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
TOPHET-D: Electrical Resistance Alloy
Available to Purchase
Alloy Digest (1967) 16 (1): Fe-30.
Published: 01 January 1967
... hardness heat treatability high-temperature alloys machinability physical properties tensile properties Tophet-D workability r-v EST cf I wrniT - D -DATA ON WORLD WIDE METALS AND ALLOYS Filing Code: Fe-30 Iron Alloy JANUARY 1967 TOPHET*-D (Electrical Resistance Alloy) Pvblisbed by Engineering...
Abstract
View articletitled, TOPHET-D: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
View
PDF
for article titled, TOPHET-D: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
Tophet-D is an iron-nickel-chromium alloy recommended for electric furnace heating elements and electrical resistors operating up to 1600 F. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: Fe-30. Producer or source: Wilbur B. Driver Company.
Journal Articles
CHROMIC-C: Electrical Resistance Alloy
Available to Purchase
Alloy Digest (1967) 16 (3): Ni-122.
Published: 01 March 1967
... CHROMIC-C is a nickel-chromium-iron electrical resistance alloy recommended for use in applications where the maximum operating temperature does not exceed 1700 F (927 C). This datasheet provides information on composition, physical properties, and tensile properties. It also includes information...
Abstract
View articletitled, CHROMIC-C: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
View
PDF
for article titled, CHROMIC-C: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
CHROMIC-C is a nickel-chromium-iron electrical resistance alloy recommended for use in applications where the maximum operating temperature does not exceed 1700 F (927 C). This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-122. Producer or source: H. K. Porter Company Inc., Fabricated Metals Division.
Journal Articles
EXCELSIOR: Electrical Resistance Alloy
Available to Purchase
Alloy Digest (1968) 17 (3): Cu-186.
Published: 01 March 1968
... tensile properties workability EXCELSIOR Filing Code: Cu-186 Copper A I loy MARCH 1968 - DATA ON WORLD WIDE METALS AND ALLOYS Publihd by EXCELSIOR (Electrical Resistance Alloy) Engineering Alloys Digest, Inc. Upper Montclair, New Jersey EXCELSIOR is a copper-nickel resistance alloy recommended for low...
Abstract
View articletitled, EXCELSIOR: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
View
PDF
for article titled, EXCELSIOR: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
EXCELSIOR is a copper-nickel resistance alloy recommended for low temperature resistors and heavy duty rheostats. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, and joining. Filing Code: Cu-186. Producer or source: H. K. Porter Company Inc..
Journal Articles
HYTEMCO: Electrical Resistance Alloy
Available to Purchase
Alloy Digest (1971) 20 (7): Ni-165.
Published: 01 July 1971
... HYTEMCO is a nickel-iron alloy with a high temperature coefficient of electrical resistance. It is recommended for electrical instruments and controls, such as ballistic devices and resistance thermometers, operating in air up to 1100 F. This datasheet provides information on composition, physical...
Abstract
View articletitled, HYTEMCO: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
View
PDF
for article titled, HYTEMCO: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
HYTEMCO is a nickel-iron alloy with a high temperature coefficient of electrical resistance. It is recommended for electrical instruments and controls, such as ballistic devices and resistance thermometers, operating in air up to 1100 F. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: Ni-165. Producer or source: Driver-Harris Company.
Journal Articles
MANGANIN: Electrical Resistance Alloy
Available to Purchase
Alloy Digest (1963) 12 (3): Cu-126.
Published: 01 March 1963
... Resistance Alloy) Pvblisbd by Engineering Alloys Digest, ICK Upper Montclair, New Jersq MANGANIN is an alloy of copper, manganese and nickel recommended for resistors in precision builr electrical apparatus and for shunts for D.C. ammeters. Composition: Physical Constants: (at 200~) Standard Shunt Nickel 4 4...
Abstract
View articletitled, MANGANIN: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
View
PDF
for article titled, MANGANIN: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
MANGANIN is an alloy of copper, manganese and nickel recommended for resistors in precision built electrical apparatus and for shunts for D.C. ammeters. This datasheet provides information on composition and physical properties. Filing Code: Cu-126. Producer or source: Driver-Harris Company.
Journal Articles
TOPHET-C: Electrical Resistance Alloy
Available to Purchase
Alloy Digest (1965) 14 (10): Ni-106.
Published: 01 October 1965
... Tophet-C is a nickel-base alloy recommended for electrical appliances and other devices whose operating temperatures do not exceed 1850 F. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance...
Abstract
View articletitled, TOPHET-C: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
View
PDF
for article titled, TOPHET-C: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
Tophet-C is a nickel-base alloy recommended for electrical appliances and other devices whose operating temperatures do not exceed 1850 F. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming and joining. Filing Code: Ni-106. Producer or source: Wilbur B. Driver Company.
Journal Articles
NICHROME: Electrical Resistance, Heat and Corrosion Resisting Alloy
Available to Purchase
Alloy Digest (1958) 7 (4): Ni-41.
Published: 01 April 1958
... Upper Monrclair, New Jersey NlCHROME* (An Electrical Resistance, Heat & Corrosion Resisting Alloy) NICHROME is a nickei-chromium-iron alloy . Reg. T.M. of Driver-Harris Co. Composition: Nickel chromium EOY- &bon Iroll 58.00 - 60.00 15.00 - 16.00 0.50 max. 1.75 max. 0.08 max. Remainder adapted for high...
Abstract
View articletitled, NICHROME: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span>, Heat and Corrosion <span class="search-highlight">Resisting</span> Alloy
View
PDF
for article titled, NICHROME: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span>, Heat and Corrosion <span class="search-highlight">Resisting</span> Alloy
NICHROME is a nickel-chromium-iron alloy adapted for high temperature service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-41. Producer or source: Driver-Harris Company.
Journal Articles
Ni-Cr 60-16 Alloy: Electrical Resistance Alloy
Available to Purchase
Alloy Digest (1976) 25 (8): Ni-232.
Published: 01 August 1976
... Ni-Cr 60-16 Alloy is an electrical-resistance alloy suitable for operation at temperatures up to 1700 F (927 C). It is ideal for heavy-duty controls and rheostats because it withstands high overloads. It is used in many domestic appliances and is very useful where space is a factor because of its...
Abstract
View articletitled, Ni-Cr 60-16 Alloy: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
View
PDF
for article titled, Ni-Cr 60-16 Alloy: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
Ni-Cr 60-16 Alloy is an electrical-resistance alloy suitable for operation at temperatures up to 1700 F (927 C). It is ideal for heavy-duty controls and rheostats because it withstands high overloads. It is used in many domestic appliances and is very useful where space is a factor because of its high strength in small sizes and its high electrical resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, forming, heat treating, machining, and joining. Filing Code: Ni-232. Producer or source: Electrical resistance alloy producers.
Journal Articles
ADVANCE: High Electrical Resistance Alloy
Available to Purchase
Alloy Digest (1956) 5 (7): Cu-40.
Published: 01 July 1956
... ADVANCE is a copper-nickel alloy having high electrical resistance, negligible temperature coefficient of resistance and good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fracture...
Abstract
View articletitled, ADVANCE: High <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
View
PDF
for article titled, ADVANCE: High <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
ADVANCE is a copper-nickel alloy having high electrical resistance, negligible temperature coefficient of resistance and good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fracture toughness. It also includes information on casting, forming, heat treating, machining, and joining. Filing Code: Cu-40. Producer or source: Driver-Harris Company.
Journal Articles
Ni-Cr 80-20 Alloy: Electrical Resistance Alloy
Available to Purchase
Alloy Digest (1973) 22 (10): Ni-196.
Published: 01 October 1973
... Ni-Cr 80-20 Alloy is an electrical-resistance alloy suitable for operation at temperatures up to 2100 F (1150 C). It has a low temperature coefficient of resistivity and is also highly resistant to corrosion and oxidation. This datasheet provides information on composition, physical properties...
Abstract
View articletitled, Ni-Cr 80-20 Alloy: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
View
PDF
for article titled, Ni-Cr 80-20 Alloy: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
Ni-Cr 80-20 Alloy is an electrical-resistance alloy suitable for operation at temperatures up to 2100 F (1150 C). It has a low temperature coefficient of resistivity and is also highly resistant to corrosion and oxidation. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-196. Producer or source: Electrical resistance alloy producers.
Journal Articles
Cu-Ni 55-45 Alloy: Electrical Resistance and Thermocouple Alloy
Available to Purchase
Alloy Digest (1974) 23 (1): Cu-274.
Published: 01 January 1974
... Cu-Ni 55-45 Alloy is an electrical-resistance alloy suitable for operation at temperatures up to about 930 F. It has a low temperature coefficient of resistivity and good resistance to corrosion. In thermocouples it can be used up to 1600 F. This datasheet provides information on composition...
Abstract
View articletitled, Cu-Ni 55-45 Alloy: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> and Thermocouple Alloy
View
PDF
for article titled, Cu-Ni 55-45 Alloy: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> and Thermocouple Alloy
Cu-Ni 55-45 Alloy is an electrical-resistance alloy suitable for operation at temperatures up to about 930 F. It has a low temperature coefficient of resistivity and good resistance to corrosion. In thermocouples it can be used up to 1600 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as casting, forming, heat treating, machining, and joining. Filing Code: Cu-274. Producer or source: Electrical resistance and thermocouple alloy producers.
Journal Articles
TECHALLOY C: Electrical Resistance Alloy
Available to Purchase
Alloy Digest (1975) 24 (7): Ni-219.
Published: 01 July 1975
... TECHALLOY C (62-16) is a nickel-chromium-iron electrical resistance alloy for operating temperatures up to 1700 F. It can withstand high overloads; this makes it ideal for heavy-duty rheostats and controls. It is highly suitable for heating elements in domestic appliances. It's high electrical...
Abstract
View articletitled, TECHALLOY C: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
View
PDF
for article titled, TECHALLOY C: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
TECHALLOY C (62-16) is a nickel-chromium-iron electrical resistance alloy for operating temperatures up to 1700 F. It can withstand high overloads; this makes it ideal for heavy-duty rheostats and controls. It is highly suitable for heating elements in domestic appliances. It's high electrical resistance and high strength in small sizes make it very useful where space is a factor. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-219. Producer or source: Techalloy Company Inc..
Journal Articles
TECHALLOY A: Electrical Resistance Alloy
Available to Purchase
Alloy Digest (1975) 24 (8): Ni-220.
Published: 01 August 1975
... TECHALLOY A (80-20) is a nickel-chromium electrical resistance alloy for operating temperatures up to 2150 F. It is non-magnetic, highly corrosion resistance, and has a lower temperature coefficient of resistance than other alloys for heater elements. This datasheet provides information...
Abstract
View articletitled, TECHALLOY A: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
View
PDF
for article titled, TECHALLOY A: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
TECHALLOY A (80-20) is a nickel-chromium electrical resistance alloy for operating temperatures up to 2150 F. It is non-magnetic, highly corrosion resistance, and has a lower temperature coefficient of resistance than other alloys for heater elements. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-220. Producer or source: Techalloy Company Inc..
Journal Articles
TECHALLOY 294: Electrical Resistance Alloy
Available to Purchase
Alloy Digest (1975) 24 (10): Cu-301.
Published: 01 October 1975
... TECHALLOY 294 is a copper-nickel alloy with constant electrical resistance over a wide range of temperatures. It is used widely in rheostats and controls where the maximum operating temperature does not exceed 1000 F. Its low temperature coefficient of electrical resistance and its stability make...
Abstract
View articletitled, TECHALLOY 294: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
View
PDF
for article titled, TECHALLOY 294: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
TECHALLOY 294 is a copper-nickel alloy with constant electrical resistance over a wide range of temperatures. It is used widely in rheostats and controls where the maximum operating temperature does not exceed 1000 F. Its low temperature coefficient of electrical resistance and its stability make it highly useful in sizes for instruments and resistors. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-301. Producer or source: Techalloy Company Inc..
Journal Articles
TECHALLOY D: Electrical Resistance Alloy
Available to Purchase
Alloy Digest (1976) 25 (4): Fe-57.
Published: 01 April 1976
... TECHALLOY D is an iron-nickel-chromium electrical-resistance alloy suitable for operating in air up to 1400-1600 F. It resists heat, oxidation and corrosion to an outstanding degree. It is used as heating elements in industrial furnaces that operate in the temperature range of 1500-1800 F...
Abstract
View articletitled, TECHALLOY D: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
View
PDF
for article titled, TECHALLOY D: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
TECHALLOY D is an iron-nickel-chromium electrical-resistance alloy suitable for operating in air up to 1400-1600 F. It resists heat, oxidation and corrosion to an outstanding degree. It is used as heating elements in industrial furnaces that operate in the temperature range of 1500-1800 F with controlled atmospheres, and in the range 1400-1600 F in air. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Fe-57. Producer or source: Techalloy Company Inc..
Journal Articles
ALLOY 750: Electrical Resistance Alloy
Available to Purchase
Alloy Digest (1977) 26 (7): SS-342.
Published: 01 July 1977
... ALLOY 750 is a low-cost iron-chromium-aluminum electrical-resistance alloy for use in small appliances operating up to 2050 F. It possesses excellent ductility, uniformity and strength for easy fabrication. It is used in a wide range of heating elements. This datasheet provides information...
Abstract
View articletitled, ALLOY 750: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
View
PDF
for article titled, ALLOY 750: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
ALLOY 750 is a low-cost iron-chromium-aluminum electrical-resistance alloy for use in small appliances operating up to 2050 F. It possesses excellent ductility, uniformity and strength for easy fabrication. It is used in a wide range of heating elements. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-342. Producer or source: Hoskins Manufacturing Company.
Journal Articles
ALLOY 815: Electrical Resistance Alloy
Available to Purchase
Alloy Digest (1977) 26 (9): SS-343.
Published: 01 September 1977
... heat treatability joinability machinability physical properties tensile properties workability Filing Code: ss-343 Stainless Steel SEPTEMBER 1977 IpPmmR - DATA t3N W6RLD WIDE MlWALS AND Al ALLOY 815* (Electrical-Resistance Alloy) ALLOY 815 is a general-purpose iron-chromium-aluminum alloy...
Abstract
View articletitled, ALLOY 815: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
View
PDF
for article titled, ALLOY 815: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
ALLOY 815 is a general-purpose iron-chromium-aluminum alloy for moderately high-temperature applications up to 2150 F. It was developed especially to provide greater ductility and hot strength than was previously available in other low-cost alloys of similar composition. It is used in a wide variety of small appliances and various types of industrial equipment. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-343. Producer or source: Hoskins Manufacturing Company.
Journal Articles
ALLOY 875: Electrical Resistance Alloy
Available to Purchase
Alloy Digest (1977) 26 (10): SS-345.
Published: 01 October 1977
... ALLOY 875 is an iron-chromium-aluminum electrical-resistance alloy with excellent resistance to oxidation at elevated temperatures. It was developed primarily for use as the heating element in industrial furnaces, kilns and other equipment where continuous operating temperatures up to 2350 F may...
Abstract
View articletitled, ALLOY 875: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
View
PDF
for article titled, ALLOY 875: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
ALLOY 875 is an iron-chromium-aluminum electrical-resistance alloy with excellent resistance to oxidation at elevated temperatures. It was developed primarily for use as the heating element in industrial furnaces, kilns and other equipment where continuous operating temperatures up to 2350 F may be required. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-345. Producer or source: Hoskins Manufacturing Company.
Journal Articles
TECHALLOY FECRALLOY A: Electrical Resistance Alloy
Available to Purchase
Alloy Digest (1981) 30 (5): Fe-63.
Published: 01 May 1981
... TECHALLOY FECRALLOY A is a new, flexible iron-chromium-aluminum electrical-resistance alloy for heating elements. It greatly resists embrittlement and oxidation; in fact, it has outstanding resistance in air and other hot oxidizing gases to 2372 F (1300 C). Its useful life is many times longer...
Abstract
View articletitled, TECHALLOY FECRALLOY A: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
View
PDF
for article titled, TECHALLOY FECRALLOY A: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Alloy
TECHALLOY FECRALLOY A is a new, flexible iron-chromium-aluminum electrical-resistance alloy for heating elements. It greatly resists embrittlement and oxidation; in fact, it has outstanding resistance in air and other hot oxidizing gases to 2372 F (1300 C). Its useful life is many times longer than that of heating elements made from conventional resistance alloys. The alloy can be formed easily on standard equipment and, if necessary, heating elements can be removed easily and repaired; also, the alloy is so ductile that it can be rewound. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: Fe-63. Producer or source: Resistalloy Ltd.
Journal Articles
BRIGHTRAY ALLOY C: Electrical Resistance Wire
Available to Purchase
Alloy Digest (1988) 37 (2): Ni-355.
Published: 01 February 1988
... International® 1996 1996 ASM International BRIGHTRAY ALLOY C chemical composition electrical applications physical properties temperature coefficient of resistivity tensile properties BRIGHTRAY ALLOY C Filing Code: Ni-355 Nickel Alloy FEBRUARY 1988 - DATA ON WORLD WIDE METALS AND ALLOYS Q...
Abstract
View articletitled, BRIGHTRAY ALLOY C: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Wire
View
PDF
for article titled, BRIGHTRAY ALLOY C: <span class="search-highlight">Electrical</span> <span class="search-highlight">Resistance</span> Wire
BRIGHTRAY alloy C is an 80 20 nickel chromium alloy containing long-life additions which make it suitable for applications subject to frequent switching and wide temperature fluctuations. It may be used at operating temperatures up to 1150 C (2100 F). It has a relatively low temperature coefficient of resistance coupled with high resistivity. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: Ni-355. Producer or source: Inco Alloys International Inc..