1-20 of 1100 Search Results for

electrical equipment

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1968) 17 (7): Cu-189.
Published: 01 July 1968
... Hitenso-1622 is a copper-cadmium alloy characterized by high strength, abrasion resistance and relatively high electrical conductivity. (Formerly known as Hitenso BB-961). It is recommended for electrical equipment, trolley wire, low temperature transmission lines and relays. This datasheet...
Journal Articles
Alloy Digest (1988) 37 (2): Co-83.
Published: 01 February 1988
... CARPENTER HIPERCO 50 is a magnetic soft alloy used primarily as magnetic core in electrical equipment requiring high permeability at very high magnetic flux densities. These magnetic characteristics permit weight reduction, reduction of copper turns and insulation in the end product in comparison...
Journal Articles
Alloy Digest (1953) 2 (2): SA-6.
Published: 01 February 1953
... ALLEGHENY 88X is a manganese type nonmagnetic, austenitic steel of high strength and of mild corrosion resistance, for electrical equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1963) 12 (2): Fe-22.
Published: 01 February 1963
... INDALLOY is a sintered magnetic material recommended for permanent magnets in generators, motors and other electrical equipment. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating and machining...
Journal Articles
Alloy Digest (1967) 16 (9): Co-52.
Published: 01 September 1967
... Covandur is a free-machining iron-cobalt-vanadium alloy designed for use in electrical equipment in which high magnetic permeability at very high flux densities is essential. This datasheet provides information on composition and physical properties. It also includes information on forming, heat...
Journal Articles
Alloy Digest (1964) 13 (5): Fe-25.
Published: 01 May 1964
... CARPENTER HIGH PERMEABILITY 49 is an iron-nickel alloy of high magnetic permeability recommended for magnetic and electrical equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1968) 17 (7): Fe-34.
Published: 01 July 1968
... ALNICO-I is an un-oriented permanent magnet iron-base aloy recommended for general purposes in electrical and magnetic equipment. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating and machining...
Journal Articles
Alloy Digest (1963) 12 (12): Cu-136.
Published: 01 December 1963
... Characteristics: Riverside No. 105 is of outstanding importance because of its relatively high electrical con- ductivity. Cold rolled to good spring strengths, in strip form, it is particularly adaptable co fuse clips, movable and fixed contacts, and for similar parts of electrical equipment. It is highly...
Journal Articles
Alloy Digest (1965) 14 (9): SS-172.
Published: 01 September 1965
... SANDVIK SANICRO 31 is an iron-nickel-chromium alloy having good resistance to corrosion and oxidation and good mechanical properties at elevated temperatures. It is recommended for electrical sheathing, pyrometer tubes, equipment for heat treating and furnace tubes and other equipment...
Journal Articles
Alloy Digest (1977) 26 (5): Cu-333.
Published: 01 May 1977
... Copper Alloy No. 175 is a wrought copper alloy that combines high strength with good electrical and thermal conductivities. It can be hardened by aging after a solution treatment. It is used for a variety of electrical hardware components and for industrial welding equipment. This datasheet...
Journal Articles
Alloy Digest (1984) 33 (2): Cu-472.
Published: 01 February 1984
... CR 155 is a silver-copper to which magnesium and phosphorus have been added to deoxidize the copper and give a precipitation-strengthening copper (alloy) having great strength and resistance to heat without an equipment loss in electrical conductivity. It is readily formable and can meet a large...
Journal Articles
Alloy Digest (1986) 35 (11): Ni-343.
Published: 01 November 1986
... ENPLATE NI-423 is a nickel-phosphorus alloy deposited by chemical reduction without electric current. It is deposited by a stable, relatively high-speed functional electroless nickel process that produces a low-stress coating with good ductility and excellent resistance to corrosion. Its many uses...
Journal Articles
Alloy Digest (1971) 20 (11): W-17.
Published: 01 November 1971
... CRM TUNGSTEN-35 Re-18 Mo is a high-melting alloy for applications such as electronic tube components, electrical contacts, nuclear equipment, rocket thrusters, thermocouples and heating elements. All products are produced by powder metallurgy. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1977) 26 (7): Ni-247.
Published: 01 July 1977
... TECHALLOY Nickel 205 is a wrought nickel-base alloy containing small additions of magnesium and titanium. It has a high Curie temperature and a high magnetostriction coefficient. It is used for many electrical and electronic components and for equipment employing magnetostrictive effects...
Journal Articles
Alloy Digest (1977) 26 (10): SS-345.
Published: 01 October 1977
... ALLOY 875 is an iron-chromium-aluminum electrical-resistance alloy with excellent resistance to oxidation at elevated temperatures. It was developed primarily for use as the heating element in industrial furnaces, kilns and other equipment where continuous operating temperatures up to 2350 F may...
Journal Articles
Alloy Digest (1979) 28 (9): SA-364.
Published: 01 September 1979
... CABOT ESR 4330 Mod is a modified 4330 alloy steel produced by electric-furnace, melting, vacuum degassing and electroslag remelting (ESR) by use of small-heat-size technology. Electroslag refining improves cleanliness and lowers the sulfur content to provide improved isotropy, ductility...
Journal Articles
Alloy Digest (1980) 29 (4): SA-371.
Published: 01 April 1980
... CABOT ESR 4140 is a chromium-molybdenum alloy steel produced by electric-furnace melting, vacuum degassing and electroslag remelting by use of small-heat-size technology. Electroslag refining improves cleanliness and lowers the sulfur content to provide improved isotropy, ductility and toughness...
Journal Articles
Alloy Digest (1981) 30 (5): Fe-63.
Published: 01 May 1981
... TECHALLOY FECRALLOY A is a new, flexible iron-chromium-aluminum electrical-resistance alloy for heating elements. It greatly resists embrittlement and oxidation; in fact, it has outstanding resistance in air and other hot oxidizing gases to 2372 F (1300 C). Its useful life is many times longer...
Journal Articles
Alloy Digest (1983) 32 (4): SA-388.
Published: 01 April 1983
... INGERSOLL-RAND OILFIELD PRODUCTS ESR 4330 MOD is a modified 4330 alloy steel produced by electric-furnace melting, vacuum degassing and electroslag remelting with the use of small-heat-size technology. Electroslag refining improves cleanliness and lowers the sulfur content to provide improved...
Journal Articles
Alloy Digest (1983) 32 (6): SA-391.
Published: 01 June 1983
... INGERSOLL-RAND OILFIELD PRODUCTS ESR 4140 is a chromium-molybdenum alloy steel produced by electric-furnace melting, vacuum degassing and electroslag remelting. Electroslag refining improves cleanliness and lowers the sulfur content to provide improved isotropy, ductility and toughness. ESR 4140...