Alloy Digest (1979) 28 (11): Ag-9.
Published: 01 November 1979
... CONSIL 901 is the most commonly used of the silver-copper electrical contact alloys. It has higher hardness and better resistance to wear than fine silver. It is used widely for light and medium-duty applications involving electrical-contact devices. This datasheet provides information...
Journal Articles
Alloy Digest (1980) 29 (2): Ag-8.
Published: 01 February 1980
... Consil 900 is internally oxidized 90 silver-10 cadmium oxide in which the cadmium oxide particles are extremely small and uniformly dispersed for long electrical-contact life. It often replaces fine silver and conventional silver alloys if the electrical-contact requirements call for higher...
Journal Articles
Alloy Digest (1981) 30 (4): Cu-416.
Published: 01 April 1981
..., current-carrying rings and electrical contacts. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu...
Journal Articles
Alloy Digest (1960) 9 (5): Cu-88.
Published: 01 May 1960
... CONTACT BRONZE is a phosphor bronze possessing excellent spring properties. It is recommended for use in electrical contacts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat...
Journal Articles
Alloy Digest (1984) 33 (7): Ag-10.
Published: 01 July 1984
... CONSIL 906 is an internally oxidized silver-cadmium oxide alloy for electrical contact applications. It has extremely small cadmium oxide particles, desirable for long contact life. The particles exhibit a tree-ring pattern, a characteristics of the multiple oxidation production process. Careful...
Journal Articles
Alloy Digest (1967) 16 (5): Ag-4.
Published: 01 May 1967
... CONSIL 995 is an air-hardenable silver-base alloy having high strength and high electrical conductivity. It does not soften as a result of being heated as in brazing. It is recommended for electrical contacts, cable connectors, spring clips, etc. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1969) 18 (1): W-12.
Published: 01 January 1969
... Sylvania WN-102 is a tungsten-base alloy combining high density with high strength in both compression and tension. It is recommended for radioactive shielding, counterweights, electrical contacts for high currents, gyroscopes, flywheels and governors. This datasheet provides information...
Journal Articles
Alloy Digest (1969) 18 (4): Cu-198.
Published: 01 April 1969
... Elkaloy-A is a copper-base alloy having high strength and toughness coupled with high electrical and thermal conductivity. It is recommended for springs, electrical contacts and resistance welding electrodes. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1969) 18 (7): W-13.
Published: 01 July 1969
... Sylvania WN-103 is a machinable tungsten-base alloy combining high density with high strength in both compression and tension. It is recommended for counterweights, gyroscope components and high current electrical contacts. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1970) 19 (10): Mo-10.
Published: 01 October 1970
... CLIMELT MOLYBDENUM is a commercially pure high melting point metal for applications such as electronic tube components, electric furnace elements, electrical contacts, and electrodes. It is produced by arc casting. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (1979) 28 (12): Cu-385.
Published: 01 December 1979
... ANACONDA Alloy (E) 505 is a low-tin phosphor bronze with excellent resistance to corrosion, excellent ductility and good resistance to fatigue. It has good thermal and electrical conductivity. Its uses include flexible metal hose, electrical contacts, fuse clips and fasteners. This datasheet...
Journal Articles
Alloy Digest (1983) 32 (11): Cu-466.
Published: 01 November 1983
... and as a result, has greater ductility and uniformity. Typical applications of AMCROM include resistance welding electrode tips and wheels, electrical contacts and connectors and high-temperature wire. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (2009) 58 (1): Cu-764.
Published: 01 January 2009
... Luvata C425 is a copper alloy with good spring properties and good electrical and thermal conductivity used in electrical contacts. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information...
Journal Articles
Alloy Digest (2009) 58 (2): Cu-765.
Published: 01 February 2009
... Luvata C422 is a copper alloy with good spring properties and good electrical and thermal conductivity used in electrical contacts. It is often called Ambronze 422. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength...
Journal Articles
Alloy Digest (1969) 18 (6): Cu-201.
Published: 01 June 1969
... AMBRONZE 413 is a copper-tin bronze recommended for plater's plates and electrical contact springs. It is relatively immune to stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1970) 19 (1): Cu-210.
Published: 01 January 1970
... ALRONZE is a high strength, special aluminum bronze having excellent corrosion and stress-corrosion resistance. It is recommended for electrical contacts, springs, gaskets, cutlery, wear plates, etc. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1970) 19 (8): Re-1.
Published: 01 August 1970
... CRM RHENIUM is a commercially pure, high-melting-point metal for applications such as electronics tube components, electrical contacts, thermionic converters, thermocouples, heating elements and rocket thrusters. All products are produced by powder metallurgy. This datasheet provides information...
Journal Articles
Alloy Digest (1970) 19 (12): Mo-11.
Published: 01 December 1970
... CRM MOLYBDENUM-50 RHENIUM is a high-melting-point alloy for applications such as electronics tube components, electrical contacts, thermionic converters, thermocouples, heating elements and rocket thrusters. All products are produced by powder metallurgy. This datasheet provides information...
Journal Articles
Alloy Digest (1971) 20 (11): W-17.
Published: 01 November 1971
... CRM TUNGSTEN-35 Re-18 Mo is a high-melting alloy for applications such as electronic tube components, electrical contacts, nuclear equipment, rocket thrusters, thermocouples and heating elements. All products are produced by powder metallurgy. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1974) 23 (9): Cu-285.
Published: 01 September 1974
... Copper Alloy No. 505 is a 1.25% tin-phosphorus bronze with good tensile and yield strengths and good resistance to corrosion and fatigue. It is recommended for flexible hose and electrical contacts and conductors. This datasheet provides information on composition, physical properties...