Alloy Digest (1965) 14 (10): Ni-106.
Published: 01 October 1965
... Tophet-C is a nickel-base alloy recommended for electrical appliances and other devices whose operating temperatures do not exceed 1850 F. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (1995) 44 (4): SS-384.
Published: 01 April 1995
... CARPENTER STAINLESS TYPE 430 is a chromium stainless steel that is especially useful for all types of decorative trim. This steel is suitable for trim on automobiles, cameras, vending machines, counters and showcases, electrical appliances and finished hardware in the building trade. The alloy...
Journal Articles
Alloy Digest (1981) 30 (2): Ni-265.
Published: 01 February 1981
... NIKROTHAL 6 is a nickel-chromium-iron electrical-resistance alloy for use in appliances and industrial furnaces. Its maximum recommended operating temperature is 1125 C (2055 F). It is highly suitable for heating elements in domestic appliances. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1976) 25 (8): Ni-232.
Published: 01 August 1976
... Ni-Cr 60-16 Alloy is an electrical-resistance alloy suitable for operation at temperatures up to 1700 F (927 C). It is ideal for heavy-duty controls and rheostats because it withstands high overloads. It is used in many domestic appliances and is very useful where space is a factor because of its...
Journal Articles
Alloy Digest (1981) 30 (9): Ni-270.
Published: 01 September 1981
... electrical device across a fluctuating voltage source. Kanthal 70 has a maximum recommended operating temperature of 600 C and is used widely in resistance thermometers and in various appliance and automotive applications. This datasheet provides information on composition, physical properties, and tensile...
Journal Articles
Alloy Digest (1997) 46 (9): Ni-529.
Published: 01 September 1997
... resistance. Filing Code: Ni-529. Producer or source: Kanthal Corporation. Producer or Source: Kanthal Corporation Copyright © ASM International® 1997 1997 ASM International chemical composition corrosion-resistant alloys creep properties electric household appliances electrical resistance...
Journal Articles
Alloy Digest (2013) 62 (10): Ni-710.
Published: 01 October 2013
... composition electric household appliances electrical resistance hardness industrial furnaces Nikrothal TE physical properties tensile properties workability DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2013, ASM International®. All rights reserved. Data shown are typical, not to be used...
Journal Articles
Alloy Digest (1975) 24 (7): Ni-219.
Published: 01 July 1975
... TECHALLOY C (62-16) is a nickel-chromium-iron electrical resistance alloy for operating temperatures up to 1700 F. It can withstand high overloads; this makes it ideal for heavy-duty rheostats and controls. It is highly suitable for heating elements in domestic appliances. It's high electrical...
Journal Articles
Alloy Digest (1981) 30 (5): Ni-268.
Published: 01 May 1981
... NIKROTHAL 8 is a nickel-chromium electrical-resistance alloy for use in appliances and industrial furnaces. Its maximum recommended element temperature in continuous use is 1200 C (2190 F). Nikrothal 8 is non-magnetic, highly resistant to corrosion, and has a lower temperature coefficient...
Journal Articles
Alloy Digest (1977) 26 (7): SS-342.
Published: 01 July 1977
... ALLOY 750 is a low-cost iron-chromium-aluminum electrical-resistance alloy for use in small appliances operating up to 2050 F. It possesses excellent ductility, uniformity and strength for easy fabrication. It is used in a wide range of heating elements. This datasheet provides information...
Journal Articles
Alloy Digest (1996) 45 (1): SS-631.
Published: 01 January 1996
.../asm.ad.ss0631 Copyright © ASM International® 1996 also used for trim on vending machines, counters and showcases, electrical appliances and a host of other things to increase their eye appeal and salability It is equally applicable to finished hardware and moldings as used in the building trade...
Journal Articles
Alloy Digest (1967) 16 (1): Fe-30.
Published: 01 January 1967
... at a maximum temperature of 16000F. It is also used as heating elements for electrical appliances and furnaces. It is not as resistant to chemical media as Tophet-A although it is entire- ly rust proof at room temperature. It is immune to an intergranular rype of corrosion called green rot . The alloy picks...
Journal Articles
Alloy Digest (1958) 7 (2): Ni-39.
Published: 01 February 1958
.... Forms Available: Bat, rod, ribbon, wire and strip. Also insulated wire form. Applicationsz Electric ranges, electric fumaces, radiant heaters, toast- ers, electrical appliances, chemical plant equipment resistors. Manufacturer: Wilbur B. Driver Company Newark, New Jersey ...
Journal Articles
Alloy Digest (2020) 69 (10): TS-802.
Published: 01 October 2020
... and hardness after quench hardening, high wear resistance, improved machinability. Applications Bending and blanking dies for automotive parts, blanking dies for electrical appliances, cold press dies, hydroforming dies. Supplier Hitachi Metals Ltd. Shinagawa Season Terrace, 2-70, Konan 1-chome Minato-ku...
Journal Articles
Alloy Digest (2020) 69 (9): SS-1327.
Published: 01 September 2020
..., home electrical appliances, household applications, indoor decoration Supplier Acerinox, S.A. Santiago de Compostela nº 100. Madrid 28035, Spain Tel: +34 91 398 51 00 Web: www.acerinox.com ISSN: 002-614X SS-1327B ...
Journal Articles
Alloy Digest (2009) 58 (12): SS-1049.
Published: 01 December 2009
... of refrigerated trailers, domestic electrical appliances, kitchen utensils, decorative profiles for furniture, and external facades and interior fittings for buildings. Producer: Arcelor Stainless Processing LLC Sterling Heights, MI 48312 In France: ArcelorMittal Paris FR-93212 La Plaine Saint-Denis Cedex, France...
Journal Articles
Alloy Digest (2023) 72 (7): Al-500.
Published: 01 July 2023
...): Sand casting; permanent mold casting. Applications EN AC-Al Si9Mg is widely used in the automotive industry, in machine construction, and in electrical appliances. Table 3 Ratings of casting characteristics and other properties Characteristic or property Castability Fluidity Resistance to hot tearing...
Journal Articles
Alloy Digest (1977) 26 (9): SS-343.
Published: 01 September 1977
...- atures. With regard to applications. Alloy 815 is highly recommended ior use as heating elements in small appliances - such as hot plates, flat-irons. toasters and rhe like - as well as in electric furnaces. kilns. and various orher types of industrial equipment in which rhe maximum continuous operating...
Journal Articles
Alloy Digest (2013) 62 (6): Cu-821.
Published: 01 June 2013
... BrushForm 65 is designed for both superior performance and high reliability in appliance, automotive, and computer power applications. Alloy BF-65’s combination of properties limits power loss at the contact interface, controls temperature rise from resistive heating, and provides stable contact...
Journal Articles
Alloy Digest (1980) 29 (8): Al-178.
Published: 01 August 1980
... ALUMINUM 5657 is an aluminum-base, wrought, non-heat-treatable alloy of high purity and bright appearance. It has high resistance to general corrosion and to stress-corrosion cracking. It is used widely in the anodized condition for automotive and appliance trim. This datasheet provides...