Skip Nav Destination
Close Modal
Search Results for
elastic modulus
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 4417 Search Results for
elastic modulus
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (10): Fe-113.
Published: 01 October 1996
... Precision C is a heat-treatable nickel-iron alloy used in critical diaphragm applications. The alloy composition provides a unique constant elastic modulus value over a temperature range of -50 to 150 deg F. This datasheet provides information on composition, physical properties, hardness...
Abstract
View article
PDF
Precision C is a heat-treatable nickel-iron alloy used in critical diaphragm applications. The alloy composition provides a unique constant elastic modulus value over a temperature range of -50 to 150 deg F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. Filing Code: FE-113. Producer or source: Hamilton Precision Metals Inc.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2009) 58 (11): Al-426.
Published: 01 November 2009
... Alcan 2196 T8511 is produced as extrusions for applications where compression is critical. 2196 Al-Li alloy, with high strength and elastic modulus but low density, is used for floor beams, seat tracks, welded applications, and wing stringers. This datasheet provides information on composition...
Abstract
View article
PDF
Alcan 2196 T8511 is produced as extrusions for applications where compression is critical. 2196 Al-Li alloy, with high strength and elastic modulus but low density, is used for floor beams, seat tracks, welded applications, and wing stringers. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: AL-426. Producer or source: Alcan Inc.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (1): Fe-153.
Published: 01 January 2011
... HPM Precision C is heat treatable and has a constant elastic modulus value. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: Fe-153. Producer or source: Hamilton Precision...
Abstract
View article
PDF
HPM Precision C is heat treatable and has a constant elastic modulus value. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: Fe-153. Producer or source: Hamilton Precision Metals.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (8): Ti-87.
Published: 01 August 1987
... RMI Beta C is a heat-treatable titanium-base alloy that develops a tensile strength of over 200,000 psi in the solution-treated-and-aged condition. It has good ductility and toughness, good fabricability and a low elastic modulus. It has good resistance to general corrosion and it resists hot...
Abstract
View article
PDF
RMI Beta C is a heat-treatable titanium-base alloy that develops a tensile strength of over 200,000 psi in the solution-treated-and-aged condition. It has good ductility and toughness, good fabricability and a low elastic modulus. It has good resistance to general corrosion and it resists hot, aggressive environments containing ferric chloride, sodium chloride, carbon dioxide and hydrogen sulfide. Its applications include coil springs, fasteners, rivets and downhole oil-production equipment. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ti-87. Producer or source: RMI Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1989) 38 (9): Al-299.
Published: 01 September 1989
... ALCOA Alloy 2090 is an aluminum-lithium alloy with 8% lower density and 12% higher elastic modulus than 7075-T6, a major high-strength alloy used in aircarft structures. Special facilities and practices required for casting commercial size aluminum-lithium ingots have been developed to cope...
Abstract
View article
PDF
ALCOA Alloy 2090 is an aluminum-lithium alloy with 8% lower density and 12% higher elastic modulus than 7075-T6, a major high-strength alloy used in aircarft structures. Special facilities and practices required for casting commercial size aluminum-lithium ingots have been developed to cope with the highly reactive nature of lithium in molten aluminum. In general, the alloy should be considered for use in light-weight structures requiring high strength and stiffness. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-299. Producer or source: Aluminum Company of America.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1999) 48 (10): Cu-641.
Published: 01 October 1999
... · h · °F) 153 238 (90 140) Electrical conductivity at 20 °C (68 °F), %IACS 38 Specific heat at 20 °C (68 °F), J/kg · K (Btu/lb · °F) 418.7 (0.1) Melting point, °C (°F) Liquidus 1081 (1978) Solidus 1050 (1922) Mechanical Properties: Modulus of elasticity, GPa (106 psi) 127.7 (18.5) Shear modulus, GPa...
Abstract
View article
PDF
Berylco 7 is beryllium copper alloy with 0.3% beryllium. The alloy has high conductivity, fatigue strength, and wear resistance and is nonmagnetic. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well asfatigue. Filing Code: CU-641. Producer or source: NGK Metals Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1999) 48 (11): Cu-642.
Published: 01 November 1999
.... Beryllium copper alloys have high me- chanical strength and a favorable elastic modulus, which make them highly suitable as a spring material. The elastic modulus is usually the modulus of longitudinal elasticity and is also known as Young s modulus. This value is obtained from the slope of strain against...
Abstract
View article
PDF
Berylco 14 is a beryllium copper alloy with 0.4% Be. The alloy is an automotive industry favorite similar to Berylco 10 (see Alloy Digest Cu-6, April 1953) but with nickel substituting for cobalt. The alloy has high thermal and electrical conductivity, good strength, and superior high-temperature performance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on heat treating. Filing Code: CU-642. Producer or source: NGK Metals Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (9): SS-908.
Published: 01 September 2004
... Sandvik Bioline 1RK91 tensile properties thermal properties UNS S46910 Chemical Composition, wt (Nominal) Chromium 12 Nickel 9 Molybdenum 4 Copper 2 Iron bal Physical Properties: Density, kg/m3 (lb/in.3 ) 7833 (0.283) See also Tables 1 and 2. Mechanical Properties: The modulus of elasticity...
Abstract
View article
PDF
Sandvik Bioline 1RK91 (a Sandvik Nanoflex material) is a precipitation-hardening stainless steel grade specifically designed for applications requiring high strength combined with good ductility in the final product, and high formability in the as-delivered condition. The strength is increased after aging of the final product. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as heat treating and surface treatment. Filing Code: SS-908. Producer or source: Sandvik Steel Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2006) 55 (12): Co-115.
Published: 01 December 2006
... of 400°C (750 °F), together with its excellent corrosion resistance, open up a wide range of potential applications. The variation in elastic modulus with temperature does not differ significantly from that in other alloys. Phynox shows no tendency for brittleness at low temperatures. Forming: Many...
Abstract
View article
PDF
Phynox is a high yield strength cobalt alloy with a range of physical, chemical, and technological properties that make it useful for a wide variety of applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CO-115. Producer or source: Metalimphy Precision Alloys Inc.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2001) 50 (12): Ti-124.
Published: 01 December 2001
..., guaranteed min 759 (110) Solution treated and aged, guaranteed min 1103 (160) Elongation, 51 mm (2 in.) gage length, % Solution treated 15 Solution treated and aged 6 Elastic modulus, tension, GPa (106 psi) Solution treated 93 96 (13.5 14.0) Solution treated and aged 102 (14.8) Elastic modulus, torsion, GPa...
Abstract
View article
PDF
RMI Ti Beta-C/Pd alloy is a Ti-3Al-8V-6Cr-4Zr-4Mo-0.05Pd alloy also referred to as Grade 20. It is a palladium-containing version of RMI Beta-C alloy possessing equivalent physical and mechanical properties, but with enhanced corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength as well as fracture toughness and creep. It also includes information on high temperature performance. Filing Code: TI-124. Producer or source: RMI Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2010) 59 (7): Ni-680.
Published: 01 July 2010
... 316 (70 600) 13.9 (7.7) 21 538 (70 1000) 14.4 (8.0) 21 649 (70 1200) 15.1 (8.4) 21 760 (70 1400) 16.0 (8.9) Table 2 Elastic modulus, modulus of rigidity and Poisson s ratio Temperature, ºC (ºF) Elastic modulus, GPa (106 psi) Modulus of rigidity, GPa (106 psi) Poisson s ratio 21 (70) 200 (29.0) 77...
Abstract
View article
PDF
Although LSS 718 EP is a premier aerospace nickel-base alloy, it has a significant presence in exploration and production (EP) of oil and gas and this modification is meant for those applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Ni-680. Producer or source: Latrobe Specialty Steel Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2016) 65 (5): SS-1245.
Published: 01 May 2016
... on material thickness and other factors. Table 1 Physical properties Temperature, °C (°F) Specific heat, J/kg·K (Btu/lb·°F) Thermal diffusivity, m2/s (ft2/s) Thermal conductivity, W/m·K (Btu/(h·ft·°F)) Mean coefficient of thermal expansion, 10 6/K (10 6/°F) Static elastic modulus, GPa (106 psi) RT 0.466...
Abstract
View article
PDF
MTEK 25-35LS is a solid solution Fe-Ni-Cr-Nb casting alloy with good high temperature creep strength. This datasheet provides information on composition, physical properties, microstructure, elasticity, and tensile properties. It also includes information on casting, heat treating, machining, and joining. Filing Code: SS-1245. Producer or source: MetalTek International.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (4): Cer-11.
Published: 01 April 1992
... carbide and 30% silicon nitride. PROPERTIES Table 1 - ADVANCER KILN FURNITURE PROPERTIES pw=tY Density, bulk Apparent porosity Thermal coefficient of expansion 86 to 2732°F (30 to 1 500°C) Thermal conductivity @ 2100°F (1149OC) Temperature, maximum use Modulus of elasticity Modulus of rupture (room...
Abstract
View article
PDF
ADVANCER NITRIDE BONDED SILICON CARBIDE has exceptional high-temperature strength. Its oxidation resistance assures long life. It is a low-mass ceramic that is ideally suited to kiln furniture. This datasheet provides information on composition, physical properties, elasticity, and shear strength. Filing Code: Cer-11. Producer or source: Norton Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1994) 43 (1): Ni-444.
Published: 01 January 1994
...) 32-212OF (O-100°C) Electrical resistivity at 68 F (20°C), microhm-cm Annealed Aged Modulus of elasticity, rigidity 0.296 (8.19) 0.297 (8.22) 8.19 8.22 See Table 2 6.5 (11.2) 127 121 See Table 1 Typical Table l-ELASTIC MODULUS, MODULUS OF RIGIDlTY AND POISSON S RATIO PROPERTIES Modulus of Temperature...
Abstract
View article
PDF
ALTEMP 718 ALLOY is an austenitic nickel-base superalloy used in applications requiring high strength to approximately 1400 F (760 C) and oxidation resistance to approximately 1800 F (982 C). The alloy is age-hardenable. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as heat treating and joining. Filing Code: Ni-444. Producer or source: Allegheny Ludlum Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (8): Co-122.
Published: 01 August 2011
... Electrical resistivity, µ · m ( circular-mil/ft) 136 Curie temperature, ºC (ºF) 365 (689) See Fig. 1 through 4. Mechanical Properties: Hardness, 50 g (0.1 lb) load, HV 900 Tensile strength, MPa (ksi) 1000 2000 (145 290) Elastic modulus, GPa (106 psi) 100 110 (14.5 16.0) Lamination factor, % > 79 General...
Abstract
View article
PDF
Metglas alloy 2705M is an amorphous cobalt-base alloy designed for shielding and high frequency cores. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. Filing Code: Co-122. Producer or source: Metglas Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (9): Co-123.
Published: 01 September 2011
... temperature, ºC (ºF) 225 (437) See Fig. 1 3. Mechanical Properties: Vicker s hardness, 50 g load, HV 960 Tensile strength, MPa (ksi) 1000 2000 (145 290) Elastic modulus, GPa, (106 psi) 100 110 (14.5 16.0) Metglas is a registered trademark of Metglas, Inc. Fig. 1 Typical DC hysteresis loop Fig. 2 Typical...
Abstract
View article
PDF
Metglas alloy 2714A is a cobalt based alloy with ultrahigh permeability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. Filing Code: Co-123. Producer or source: Metglas Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (11): Fe-157.
Published: 01 November 2011
... resistivity, m ( circular-mil/ft) 1.38 (830) Curie temperature, °C (°F) 358 (676) See Fig. 1 3. Mechanical Properties: Vicker s hardness, 50 g (0.1 lb) load, HV 860 Tensile strength, MPa (ksi) 1000 2000 (145 290) Elastic modulus, GPa (106 psi) 100 110 (15 16) General Characteristics: Metglas magnetic alloy...
Abstract
View article
PDF
Metglas Alloy 2605S3A is an iron-base alloy with high permeability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: Fe-157. Producer or source: Metglas Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2001) 50 (12): Ti-123.
Published: 01 December 2001
... max Residual elements, total 0.40 max Titanium bal Physical Properties: Density, kg/m3 (lb/in.3 ) 4520 (0.163) Beta transus, °C (°F) 1015 (1859) Mechanical Properties: Elastic modulus, GPa (106 psi) 105 120 (15.2 17.4) Tensile strength, typical, MPa (ksi) 1000 (145) Yield strength, 2% offset, typical...
Abstract
View article
PDF
TIMETAL 367 is a Ti-6Al-7Nb medium-strength alpha-beta alloy for surgical implants. The alloy is analogous to TIMETAL 367 6-4 (revised as Ti-6Al-4V, Alloy Digest Ti-66, September 1992), but with niobium as the more biocompatible alloying element. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on heat treating. Filing Code: TI-123. Producer or source: Timet.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1957) 6 (7): SS-58.
Published: 01 July 1957
... Thermal conductivity, BTU/ff /ft/hr/OF. (at 212OF.) Thermal coef. ;;ygioF& tn/m/°F. 6816&F Modulus of elasticity, psi (in tension) PROPERTIES Table 1 - TYPICAL TENSILE PROPERTIES Room Room Room Room 1200 1400 Room Tensile Strength psi 115000 125000 : 50000 37000 102000 95000 Table 2 - EFFECT- OF COLD...
Abstract
View article
PDF
ENDURO 201 is a non-hardenable austenitic chromium-nickel-manganese steel, capable of easily attaining high tensile strength and excellent ductility by moderate or severe cold working. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-58. Producer or source: Stainless steel foundries.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (4): Zr-4.
Published: 01 April 1968
...) Iron 0.07-0.20 Tin 1.2-1.7 Chromium 0.05-O. 15 Nickel 0.03-0.08 Fe+Cr+Ni 0.18-0.38 Zirconium Remainder Density, lb;cu.in. Modulus of elasticity, psi x 106 Thermal conducciviey, Btu, ft2!ft /hr/OF at 77 F ac 752OF Elastic modulus race of change with temperature (dE/dT), psi/OF Poisson s ratio Neutron...
Abstract
View article
PDF
ZIRCONIUM Gr. 32 is an alloy with a low neutron cross-section, good high temperature mechanical properties and excellent corrosion resistance in water and steam. It is a reactor grade zirconium-tin alloy for corrosion resistance in irradiated water. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Zr-4. Producer or source: AMAX.