1-20 of 62 Search Results for

economizer tubes

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2005) 54 (8): SA-550.
Published: 01 August 2005
... S-TEN1 is a steel alloy containing copper and antimony to make it more resistant to dew-point corrosion than conventional carbon steels. It is used as tubing in economizers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It...
Journal Articles
Alloy Digest (2016) 65 (6): SA-754.
Published: 01 June 2016
... S-TEN2 is a steel alloy containing copper to make it more corrosion resistant to dew point corrosion than conventional carbon steels. It is used as tubing in economizers. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1994) 43 (8): SS-571.
Published: 01 August 1994
... SUMITOMO DP8 is a duplex stainless steel. Duplex stainless steels are designed to be economical and reliable for material applications in the production of oil and gas to resist the environments there of carbon dioxide, hydrogen sulfide and chlorides. This family of alloys is also resistant to...
Journal Articles
Alloy Digest (2010) 59 (3): SS-1056.
Published: 01 March 2010
... Incoloy alloy 25-6HN is a 6% Mo superaustenitic stainless steel. It offers an excellent combination of strength, ductility, and resistance to corrosion by a variety of media at an economical price. It is readily formed and welded. The properties of the alloy are enhanced by its content of nitrogen...
Journal Articles
Alloy Digest (1969) 18 (2): TS-214.
Published: 01 February 1969
... Böhler (or Boehler) WMD is a multi-alloy economical hot work tool steel useful for a wide range of hot work applications, such as headers, upsetters, extrusion and die casting tools and dies, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, and...
Journal Articles
Alloy Digest (2021) 70 (2): SS-1331.
Published: 01 February 2021
... ATI 20-25+Nb is an austenitic stainless steel intended primarily for elevated-temperature service. This alloy fills a performance gap between conventional heat-resistant stainless steels and nickel-base superalloys, providing high performance with an economical composition. This datasheet provides...
Journal Articles
Alloy Digest (1980) 29 (11): SA-378.
Published: 01 November 1980
... The 21/4% Nickel Steel possesses a combination of moderate strength and superior resistance to brittle fracture at subzero temperatures. It is one of the most economical materials for the construction of equipment to operate at temperatures as low as -90 F. It is intended primarily for welded...
Journal Articles
Alloy Digest (1986) 35 (1): SA-414.
Published: 01 January 1986
... ALLOY STEEL 21/4 Ni possesses a combination of moderate strength and superior resistance to brittle fracture at subzero temperatures. It is one of the most economical materials for the construction of equipment to operate at temperatures as low as 90 F. It is intended primarily for welded pressure...
Journal Articles
Alloy Digest (1974) 23 (7): SS-297.
Published: 01 July 1974
... ALLEGHENY STAINLESS AM-363 is an economical, low-carbon martensitic stainless steel. It is higher in strength than annealed austenitic stainless steels but maintains their excellent forming and welding properties. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1981) 30 (9): Cu-422.
Published: 01 September 1981
... flowing at a velocity of 56 ft. per second, and fresh water at 7-8 ft. per second. bfarine Service: In marine service, tubes of Alloy 443 have proved extremely serviceable and economical in condensers and heat exchangers handling fresh and sea water at moderate veIoclties. These qualities suit it...
Journal Articles
Alloy Digest (1992) 41 (1): Cer-10.
Published: 01 January 1992
... is an extremely versatile and economical material. Its workability allows an extensive range and flexibility in fabrication. 11 is well suited to the casting of special shapes. ZYALOX MV20 is a dense mull& in a glassy matrix formulatcd to offer a high quality economical insulating tubing. Forms...
Journal Articles
Alloy Digest (2010) 59 (7): Zr-13.
Published: 01 July 2010
... corresponds to 0.2% offset yield strength. (b) Ap0.2, % See Fig. 2. Fabricability: Bending. Zirconium tubing can be bent at room temperature using standard bend tooling and techniques. When bending thin walled tubing or if a tight bend radius is needed, a mandrel should be used for adequate support of the ID...
Journal Articles
Alloy Digest (2006) 55 (3): SS-955.
Published: 01 March 2006
... manganese and nickel, which results in finer grain sizes in heat- affected zones (HAZ) and weld structures that improve impact toughness and formability in heavy sections. When weld filler is needed, AWS E/ER 309L is most often specified. This alloy exhibits excellent tube welding characteristics due to its...
Journal Articles
Alloy Digest (2001) 50 (4): Mo-18.
Published: 01 April 2001
... almost all of the larger switchgear contacts, as well as for some of the lighter duty applications. The PSR procedure is one that may be more economical for mak- ing small Elkonite parts. Contacts manufactured by the PSR pro- cess are furnished in sizes of 0.125 in. wide, 0.156 in. diameter and 0.40 in...
Journal Articles
Alloy Digest (1959) 8 (6): SS-90.
Published: 01 June 1959
... heat resisting alloy suitable for high temperarures up to 1900°F. It has proven economical in most applications where continuous temperatures from 1400.1800 F. are encountered. It is not a&ted seriously by short exposures up to 19OO F., although it is softer and weaker at this temperature. Its high...
Journal Articles
Alloy Digest (1992) 41 (9): SS-534.
Published: 01 September 1992
... resistivity and operating temperature and the longest ser- vice life with excellent oxide formation. Aluchrom 1 has excellent oxidation and dielectric strength. It is used ad- ditionally with vertical quartz tube heaters. Aluchrom S has high resistivity and low specific gravity. It is also used in flat irons...
Journal Articles
Alloy Digest (2005) 54 (12): Ni-629.
Published: 01 December 2005
... stress cracking, and good thermal stability at an economical price. By cold work, tubes are available in a variety of strength levels. Product Forms Available: Inconel alloy 050 is available as tube in several cold worked tem- pers. INCONEL® ALLOY 050 Filing Code: Ni-629 Nickel December 2005 INCONEL...
Journal Articles
Alloy Digest (1971) 20 (5): Cu-233.
Published: 01 May 1971
... produced by normal, economical processing such as used to produce copper. A high softening temperature (no significant softening occurs below 750oF, 4000C) and restricted grain growth prevent excessive softening at soldering temperatures and lJlaStiC encapsulation temperatures, making the aBoy desir&e for...
Journal Articles
Alloy Digest (1973) 22 (6): Ni-191.
Published: 01 June 1973
..., soft mag- netic materials, when stressed or formed in any way, will lose some shielding efficiency. Therefore, when fabri- cating shields, all fabrication should he done prior to the final heat treatment. However, for those applications where a prefabricated shield is impractical or un- economical, it...
Journal Articles
Alloy Digest (2011) 60 (2): SS-1083.
Published: 01 February 2011
... environments as high-temperature seawater and flue gas desulfurization plants. This is an economical stainless steel as powerful as Hastelloy alloys and pure titanium in many environments. Product Forms Available: Plate, sheet and strip Applications: Seawater environments: desalination systems, seawater heat...