Skip Nav Destination
Close Modal
Search Results for
ducts
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 114 Search Results for
ducts
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1971) 20 (2): Ni-162.
Published: 01 February 1971
... TOPHET H is a heating-element alloy specifically designed for use in duct heaters and clothes dryers where hot strength and long life are of most importance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information...
Abstract
View article
PDF
TOPHET H is a heating-element alloy specifically designed for use in duct heaters and clothes dryers where hot strength and long life are of most importance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ni-162. Producer or source: Wilbur B. Driver Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (11): SS-913.
Published: 01 November 2004
... Sirius S15 is a high-temperature stainless steel with the elements silicon, cerium, and lanthanum added for an oxidation resistance that is better than AISI Type 310. Applications are in burners, recuperators, and ducts. This datasheet provides information on composition, physical properties...
Abstract
View article
PDF
Sirius S15 is a high-temperature stainless steel with the elements silicon, cerium, and lanthanum added for an oxidation resistance that is better than AISI Type 310. Applications are in burners, recuperators, and ducts. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming and joining. Filing Code: SS-913. Producer or source: Industeel USA, LLC.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (8): SS-937.
Published: 01 August 2005
... Sirius 314 is a high-temperature stainless steel with the elements of silicon, cerium, and lanthanum added for better oxidation resistance compared to AISI Type 310. Applications are in burners, recuperators, and ducts. This datasheet provides information on composition, physical properties...
Abstract
View article
PDF
Sirius 314 is a high-temperature stainless steel with the elements of silicon, cerium, and lanthanum added for better oxidation resistance compared to AISI Type 310. Applications are in burners, recuperators, and ducts. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming and joining. Filing Code: SS-937. Producer or source: Industeel USA, LLC.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1988) 37 (4): Ni-330.
Published: 01 April 1988
... remarkable corrosion resistance in the especially corrosive areas of flue gas desulfurization systems, such as outlet ducting leading to the stack. It has also been used to solve corrosive problem areas in municipal sewage treatment plants. Specification Equivalents: ASTM B 575. UNS N 10276. ASME SB-575...
Abstract
View article
PDF
JESSOP JS Alloy 276 is a nickel-chromium alloy with high molybdenum and moderate tungsten but low iron and silicon contents. This composition provides superior corrosion resistance to a wide variety of environments. It has found wide acceptance in the chemical and petrochemical process industry, flue gas desulfurization systems and the pulp and paper industries. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and joining. Filing Code: Ni-330. Producer or source: Jessop Steel Company. Originally published March 1986, revised April 1988.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1985) 34 (3): Ni-311.
Published: 01 March 1985
... IN ABSORBER SLURRY, MAXIMUM PITTING OR CREVICE ATTACK* [Units are mpy (mm/yr)] Absorber Outlet Material Quencher Absorber Bypass Outlet Duct Duct AlSl 316L 22 (55) 21 (53) 35 (.90)1 35 (.88 I2 (30) AlSl 317LMo 20 (50) 22 (55) 29 (.73) 33 (85) Alloy 825 I5 (38) 29 (.73) 33 (.85) 39 (1.00) 50 (1.28 Alloy 904L...
Abstract
View article
PDF
INCO Alloy C-276 is a nickel-molybdenum-chromium-tungsten alloy with outstanding corrosion resistance that is maintained even in the welded condition. It also has excellent resistance to oxidizing media. It is widely used in the severest environments encountered in chemical processing, pollution control, industrial and municipal waste treatment, pulp and paper production, and other fields. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-311. Producer or source: Huntington Alloys.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1963) 12 (4): Cu-20.
Published: 01 April 1963
... by the fabricator, reaches strengths and hardnesses appreciably higher than bronze. Through good formability, it offers cost-saving opportunities by eliminating hardening. It combines good duct&ty with high strength and hardness, good eIectricaI and thermal conductivity, and excellent resistance to wear and fatigue...
Abstract
View article
PDF
Berylco 165 is a lower cost version of the standard 1.9 percent beryllium copper alloy. It offers good formability in the unhardened condition with high final properties following precipitation hardening. It is also available in the mill hardened condition which, without heat treatment by the fabricator, reaches strengths and hardnesses appreciably higher than bronze. Through good formability, it offers cost-saving opportunities by eliminating hardening. It combines good ductility with high strength and hardness, good electrical and thermal conductivity, and excellent resistance to wear and fatigue. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: Cu-20. Producer or source: Beryllium Corporation. Originally published November 1954, revised April 1963.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (10): SS-910.
Published: 01 October 2004
... to 14,000 up to 551 Applications: Typical applications include grids, burners, and suction boxes in sintering plants; heat recuperators, charging mechanisms, circulation, and piping in blast furnaces and cooling ovens; extraction hoods, flue gas ducts, and dampers in steel melting and smelters; rollers...
Abstract
View article
PDF
Sirius S12 is an austenitic stainless steel for high-temperature service. The carbon content is optimized for creep resistance, and the alloy contains additions of silicon to outperform the conventional grades in oxidation. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming and heat treating. Filing Code: SS-910. Producer or source: Industeel USA, LLC.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2016) 65 (2): Co-125.
Published: 01 February 2016
... °C (2000 °F), and good sulfidation resistance. This alloy also has good forming and welding characteristics, which make it useful in fabricating gas turbine components such as combustion cans and transition ducts. The alloy has a face- center cubic structure. High tungsten content provides solid...
Abstract
View article
PDF
ATI 188 Alloy is a high temperature cobalt alloy with oxidation resistance to 1093 deg C (2000 deg F). This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance as well as forming and heat treating. Filing Code: Co-125. Producer or source: Allegheny Ludlum.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1959) 8 (6): Ti-1.
Published: 01 June 1959
... by stress relief anneal at 80tY F or full anneal at 1250°F to eliminate possible delayed breakage. Forms Available: Applicatioms: Airaaft skins, structural braces, ducts and shrouds. Various a&raft forgiogq jet atginc axnpoaalb aad other parts operating at tan- up to about 7OO F. MMUfOCtOWC Republic steel...
Abstract
View article
PDF
Republic RS-120 is a titanium alloy containing manganese as its principle alloying element. It shows pronounced hardening and strengthening by a low temperature heat treatment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: Ti-1. Producer or source: Republic Steel Corporation, Titanium Division. Originally published June 1953, revised June 1959.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1962) 11 (7): Cu-119.
Published: 01 July 1962
... No. 9494 is recommended for pro- ducts demanding qualities of non-leaded phosphor bronze yet which must be cut, threaded or milled. For high speed automatic cutters. It has good strength and ductility. Forms Available: Rods Bolts, nuts, shafts, pinions, screws, bearings, gears, plugs, screw machine...
Abstract
View article
PDF
Seymour No. 9494 is a leaded phosphor bronze having high strength, good corrosion resistance and improved machinability. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-119. Producer or source: Seymour Manufacturing Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (2): SA-546.
Published: 01 February 2005
... in Fig. 1 in a comparative wear test con- ducted in a paddle wear machine for hot-rolled materials. Specification Equivalents: This material conforms and is supplied to European Standard EN 10131, including tolerances. General Characteristics: Prompted by demand for product durability, wear, and perform...
Abstract
View article
PDF
Docol 450 Wear is an ultra-high strength steel that is used for many wear application in transportation and construction products. This datasheet provides information on composition, physical properties, microstructure, hardness, tensile properties, and bend strength. It also includes information on wear resistance as well as joining. Filing Code: SA-546. Producer or source: SSAB Swedish Steel Inc.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (5): Ni-625.
Published: 01 May 2005
... Applications: Haynes 617 alloy is used in applications such as gas turbines for combustion cans, ducting, and transition lines. HAYNES® ALLOY NO. 617 Filing code: Ni-625 Nickel May 2005 HAYNES® ALLOY NO. 617 (Nickel-Base Superalloy) Haynes 617 is a solid-solution Ni-Cr-Co-Mo alloy with excellent high...
Abstract
View article
PDF
Haynes 617 is a solid-solution nickel-chromium-cobalt-molybdenum alloy with excellent high temperature strength and oxidation resistance. It has applications at high temperature for aerospace engines. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as heat treating. Filing Code: Ni-625. Producer or source: Haynes International Inc.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (4): Co-130.
Published: 01 April 2020
... sulfidation resis- tance, nonmagnetic. Product Forms Bar, coil, sheet Applications Afterburner liners, aircraft engine components, combustor cans, flame holders, gas turbines, transition ducts Supplier United Performance Metals 3475 Symmes Road Hamilton, Ohio 45015, USA Tel: +1 513 860 6500 Web: www.upmet.com...
Abstract
View article
PDF
UPM Nickel Alloy 188 (UNS R30188 / Werkstoff Number 2.4683) is a low-carbon, cobalt-nickel-chromium-tungsten alloy that combines excellent high-temperature strength with very good oxidation resistance up to 1095 °C (2000 °F). It is widely used in commercial and military aircraft gas turbine engines. This datasheet provides information on composition and physical properties. It also includes information on forming and joining. Filing Code: Co-130. Producer or source: United Performance Metals.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (7): Ni-761.
Published: 01 July 2020
... Components for industrial and aircraft gas turbines (e.g., casings, combustion chambers, and ducting), and structural components for industrial furnaces. Supplier ATI 1000 Six PPG Place Pittsburgh, Pennsylvania 15222, USA Tel: +1 800 289 7454 Web: www.atimetals.com ISSN 002-614X Ni-761B ...
Abstract
View article
PDF
ATI 75 (UNS N06075) is a nickel-chromium alloy with controlled additions of titanium and carbon; it derives its high temperature strength essentially from solid solution strengthening. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, and joining. Filing Code: Ni-761. Producer or source: ATI.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2002) 51 (9): Ni-590.
Published: 01 September 2002
... treatment, and furnace components; flare tips; ducting and gas turbine parts. Producer: Metrode Products, Ltd. Hanworth lane, Chertsey Surrey, KT16 9LL +44(0)1932 566721 +44(0)1932 566168 (Sales fax) +44(0)1932 569449 (Technical fax) +44(0)1932 566199 (Export fax) ISSN: 002-614X Ni-590B ...
Abstract
View article
PDF
Rima 617 is an Inconel-type consumable with a nominal composition of Ni, 24% Cr,12% Co, and 9% Mo and is used to join UNS N06617 and Nicrofer 6023 to themselves. The alloy is designed for high-temperature service and is often used as the weld metal in dissimilar cases to ensure the weld has as good strength as does the base metal. Tungsten inert gas (TIG) wire for this alloy is referred to as 61-70. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on joining. Filing Code: Ni-590. Producer or source: Metrode Products Ltd.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (2): Ni-756.
Published: 01 February 2020
... applications, up to about 760 °C (1400 °F), that require good elevated temperature strength, low thermal expansion, and good oxidation resistance. Typical applications in the aerospace industry include casings, containment rings, duct segments, fasteners, pumps, rocket nozzles, and sealing rings. Supplier ATI...
Abstract
View article
PDF
ATI 10242 is an age-hardenable nickel-molybdenum-chromium alloy that derives its strength from a long-range ordering reaction during aging. This ordering reaction not only provides the alloy’s strength, but also imparts excellent thermal stability. This datasheet provides information on composition, physical properties, and hardness. It also includes information on high temperature performance as well as forming, machining, and joining. Filing Code: Ni-756. Producer or source: ATI.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1956) 5 (10): Cu-43.
Published: 01 October 1956
...&- tmce to corrosion and may be used for screw machine pt-0. ducts which are reqtkd to withstand severely cortive cuoditiouS. IO tin and Itod c0oteom make it my useful for baring pmposa Forms Avail&k: Comosion Resistance: Rod.%rOkd~PrOdW%=dsaip. Highly &stint to corrosion, being unakted by, and free from...
Abstract
View article
PDF
CHASE 444 BRONZE is a special free-cutting Phosphor Bronze, Grade B-2. It is used primarily for automatic screw machine products, bearings and gears. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-43. Producer or source: Chase Brass & Copper Company Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1959) 8 (2): Mg-40.
Published: 01 February 1959
...- vented by suitable methods of insulation. General Characteristics: Magnesium W62A alloy has very high tensile strength, ductility and excellent fatigue properties. It shows a very low tendency towards miaoporosiy. The alloy has the best combination of strength, duct&y and pressure tighmess yet attained...
Abstract
View article
PDF
Magnesium ZH62A is a high strength casting alloy having acceptable castability and weldability. It has good fatigue properties and ductility. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Mg-40. Producer or source: Dow Chemical Company, Magnesium Products Department.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1959) 8 (3): Co-17.
Published: 01 March 1959
... by a lowering of duct&y. Machinability: Easily machined with carbide tooh ar speeds of 28 to 42 surface feet per minute. Suggested at&s for single- point tools are 4-6 degree front and side angles, O-8 degree back top rake, 5-8 degree side rake, 15-30 degree side cutting-edge angle, and 15 degree end cut- ting...
Abstract
View article
PDF
HAYNES Alloy No. 36 is a cobalt-base alloy having excellent strength at temperatures up to 1800 deg. F. It is the cast modification of wrought HAYNES Alloy No. 25 and has been used successfully in jet engine blading and nozzle vanes. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and joining. Filing Code: Co-17. Producer or source: Haynes Stellite Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (9): Be-8.
Published: 01 September 1996
... been con- ducted on several lots of material and are the basis for this data sheet. The test material was consolidated by extrusion of gas atomized Powder containing 62 wt.% Be and 38 wt.% Al. DOI: 10.31399/asm.ad.be0008 Table 1 AlBeMet AM 162 Properly Data Sheet Table 2 AlBeMet AM162 Typical...
Abstract
View article
PDF
AlBeMet AM 162 is a beryllium, 38% aluminum alloy produced in extruded bar, rolled sheet, and hot isostatic pressed (HIP) billets that combines the high-modulus and low-density characteristics of beryllium with the fabrication and mechanical behavior of aluminum. The alloy is weldable, can be formed, machined and brazed like conventional aluminum alloys. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on machining. Filing Code: BE-8. Producer or source: Brush Wellman Inc.