Alloy Digest (1987) 36 (7): Be-5.
Published: 01 July 1987
... BRUSH WELLMAN SR-200E is a grade of beryllium strengthened by a dispersion of beryllium oxide (2.0%). It has relatively high strength and ductility (a minimum of 10% elongation). Its uses include missiles, space vehicles, structural parts on both commercial and military satellites and optical...
Journal Articles
Alloy Digest (1960) 9 (4): CI-28.
Published: 01 April 1960
... NI-RESIST DUCTILE IRONS are a group of austenitic nickel-alloyed cast irons having high strength and ductility combined with heat and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (1972) 21 (12): CI-37.
Published: 01 December 1972
... SORBO-MAT DUCTILE IRON is a high-carbon ferrous material. It is produced in five varieties providing various combinations of strength and toughness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (1956) 5 (9): CI-16.
Published: 01 September 1956
... DUCTILE IRON is a high carbon ferrous material having high strength, high ductility, toughness, good castability and ready machinability. It is a family of materials and is produced in six different commercial types providing various combinations of strength, ductility and toughness...
Journal Articles
Alloy Digest (1986) 35 (3): CI-53.
Published: 01 March 1986
... AUSTEMPERED DUCTILE IRON has high strength with excellent toughness and ductility. Its strength is twice that of conventional ductile irons, comparable to heat-treated wrought steels. Composition is balanced to provide foundry compatibility, minimal segregation and good response to austempering...
Journal Articles
Alloy Digest (1989) 38 (4): CI-58.
Published: 01 April 1989
... Ductile Iron grade 45-12 produced by continuous casting has consistent density and fine grain structure. It is the softest of the regular grades of ductile iron and it machines at high speeds with good surface finish. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1990) 39 (8): CI-62.
Published: 01 August 1990
... 55-06 and 70-02 Ductile Dura-Bar are continuously cast ductile irons with about 50 and 75% pearlitic microstructures, respectively. 55-06 has about the same tensile strength as SAE 1045 as-hot-rolled steel. Its maximum yield strength and elongation are equivalent to a eutectoid carbon steel. 70-02...
Journal Articles
Alloy Digest (2020) 69 (10): CI-74.
Published: 01 October 2020
... Dura-Bar 100-70-03 is a pearlitic ductile iron that is used for continuous cast products. It has the best wear resistance of the ascast ductile irons and is used in applications requiring high strength and high wear resistance. This grade is normally used as an alternative to quenched and tempered...
Journal Articles
Alloy Digest (2021) 70 (10): CI-86.
Published: 01 October 2021
... Dura-Bar 60-40-18 is a ductile iron that is used for the production of continuous cast products. Its microstructure consists of nodular graphite in a fully ferritic matrix. Dura-Bar 60-40-18 is typically used for applications requiring excellent ductility and impact strength. This datasheet...
Journal Articles
Alloy Digest (2021) 70 (12): CI-88.
Published: 01 December 2021
... Dura-Bar 65-45-12X is a ductile iron that is used for the production of continuous cast products. Its microstructure consists of nodular graphite and a matrix comprising ferrite and 10–50% pearlite. The predominantly ferritic matrix of Dura-Bar 65-45-12X allows it to be easily machined as opposed...
Journal Articles
Alloy Digest (2022) 71 (2): CI-90.
Published: 01 February 2022
... Meehanite SFF350 is a ferritic ductile iron with a minimum tensile strength of 350 MPa (51 ksi) and a minimum elongation of 24%, when measured on test pieces machined from separately cast samples. It is specifically designed to provide good impact properties at low temperature. This fully ferritic...
Journal Articles
Alloy Digest (2022) 71 (5): CI-93.
Published: 01 May 2022
... Meehanite SFF400 is a ferritic ductile iron with a minimum tensile strength of 400 MPa (58 ksi) and a minimum elongation of 20%, when measured on test pieces machined from separately cast samples. It is specifically designed to provide good impact properties at low temperature. This fully ferritic...
Journal Articles
Alloy Digest (2022) 71 (10): CI-98.
Published: 01 October 2022
... Meehanite SF400 is a ferritic ductile iron that has a minimum tensile strength of 400 MPa (58 ksi) and a minimum elongation of 17%, when measured on test pieces machined from separately cast samples. This fully ferritic Meehanite grade is produced by either strict control of the raw materials...
Journal Articles
Alloy Digest (2023) 72 (3): CI-103.
Published: 01 March 2023
... physical properties shear strength tensile properties thermal properties ISO1083/JS/350-22-RT (Ferritic Ductile Iron) Filing Code: CI-103 Cast Iron :: March 2023 Materials Park, Ohio 44073-0002, USA :: +1.440.338.5151 :: www.asminternational.org :: [email protected] Published by ASM...
Journal Articles
Alloy Digest (2023) 72 (4): CI-104.
Published: 01 April 2023
... castability chemical composition elasticity fatigue properties hardness heat treatability ISO1083/JS/400-18-LT physical properties shear strength tensile properties thermal properties ISO1083/JS/400-18-LT (Ferritic Ductile Iron) Filing Code: CI-104 Cast Iron :: April 2023 Materials Park, Ohio...
Journal Articles
Alloy Digest (2023) 72 (5): CI-105.
Published: 01 May 2023
... treatability ISO1083/JS/400-15 physical properties shear strength tensile properties thermal properties ISO1083/JS/400-15 (Ferritic Ductile Iron) Filing Code: CI-105 Cast Iron :: May 2023 Materials Park, Ohio 44073-0002, USA :: +1.440.338.5151 :: www.asminternational.org :: [email protected]...
Journal Articles
Alloy Digest (2023) 72 (9): CI-106.
Published: 01 September 2023
... Meehanite SF420.12 is a ductile iron that has a minimum tensile strength of 420 MPa (61 ksi) and a minimum elongation of 12%, when measured on test pieces machined from separately cast samples. This Meehanite grade possesses a predominantly ferritic matrix giving the material a good level...
Journal Articles
Alloy Digest (2023) 72 (10): CI-107.
Published: 01 October 2023
... Meehanite SF450.15 is a ductile iron that has a minimum tensile strength of 450 MPa (65 ksi) and a minimum elongation of 15%, when measured on test pieces machined from separately cast samples. This Meehanite grade possesses a predominantly ferritic matrix giving the material a good level...
Journal Articles
Alloy Digest (2023) 72 (11): CI-108.
Published: 01 November 2023
... Meehanite SFP500 is a ductile iron that has a minimum tensile strength of 500 MPa (73 ksi) and a minimum elongation of 8%, when measured on test pieces machined from separately cast samples. This Meehanite grade possesses a mixed matrix of ferrite and pearlite, with the ferrite predominating...
Journal Articles
Alloy Digest (1971) 20 (3): SA-261.
Published: 01 March 1971
... properties tensile properties weldability workability Youngstown YS-T Steel Filing Code: SA-261 YOUNGSTOWN YS-T ST EEL Stee - A oy MARCH 1971 kGESTd - DATA ON WORLD WIDE METALS AND ALLOYS Published by Engineering Alloys Digest, Inc. Upper Montclair. New Jersey YOUNGSTOWN YS-T STEEL (Ductile High...